폴리머포머를 이용한 SiC 분말 함유 다공성 예비성형체의 제조방법
    31.
    发明公开
    폴리머포머를 이용한 SiC 분말 함유 다공성 예비성형체의 제조방법 失效
    使用聚合物成型制备含SIC的多孔预制件

    公开(公告)号:KR1020030070752A

    公开(公告)日:2003-09-02

    申请号:KR1020020010276

    申请日:2002-02-26

    Abstract: PURPOSE: Provided is a simple production method of porous SiC preforms satisfying initial volume fraction by ball-milling and pressing the mixture of SiC, polymer former and additives. CONSTITUTION: The porous SiC preforms used in metal matrix composite is produced by the following steps of: ball milling SiC powder, polymer former, ethyl cellulose(400-500micrometer), and additives such as an inorganic binder, flocculant (polyacryl amide) and water, wherein the volume fraction of SiC and ethyl cellulose is 1:0.9 - 1:1.6 and at least 30wt.% of polyacryl amide is added; pressing the prepared slurry to decrease the moisture content of the slurry; drying through at least two steps of natural and forced (oven at 100deg.C) drying; heating over 1100deg.C at a rate of 5deg.C/min, except for the range of 250-450deg.C at a rate of 2deg.C/min.

    Abstract translation: 目的:提供通过球磨和压制SiC,聚合物成型剂和添加剂的混合物来满足初始体积分数的多孔SiC预制件的简单制备方法。 构成:用于金属基体复合材料的多孔SiC预制件通过以下步骤制备:球磨SiC粉末,聚合物成型剂,乙基纤维素(400-500微米)和添加剂如无机粘合剂,絮凝剂(聚丙烯酰胺)和水 ,其中SiC和乙基纤维素的体积分数为1:0.9-1:1.6,并且加入至少30重量%的聚丙烯酰胺; 压制制备的浆料以降低浆料的含水量; 干燥至少两步,天然和强制(烘箱在100℃)干燥; 以5℃/分钟的速度加热1100℃以上,除了250-450℃的范围外,以2℃/分钟的速度加热。

Patent Agency Ranking