Abstract:
A propylene composition comprising (percent by weight): A) 70%-95%, of a propylene homopolymer having a Polydispersity Index (P.I.) value of from 4.6 to 10, a fraction insoluble in xylene at 25°C, higher than 90 %, and MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 100 to 250 g/10 min; B) 5%-30%, of a copolymer of propylene containing from 36% to 44% of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25°C comprised between 3 and 5 dl/g.
Abstract:
Polyolefin composition, comprising in percent by weight: 1) 75-85% of a copolymer of propylene, said copolymer containing up to 15% by weight, of ethylene and/or C 4 -C 10 α-olefin(s) and having a fraction soluble in Xilene at room temperature lower than 6% by weight, and 2) 15-25% of a copolymer of ethylene with one or more C 4 -C 10 α-olefin(s) containing from 10 to 25% by weight of said C 4 -C 10 α-olefin(s); said composition having the value of MFR, measured at 230 °C, 2.16 kg, of less than 2.5 g/10 min, the total content of ethylene of from 14 to 22 % by weight, the total content Of C 4 -C 10 α-olefin(s) of less than 4.5% by weight, the ratio of the total content of ethylene to the total content of C 4 -C 10 α-olefin(s) equal to or higher than 4, the value of the intrinsic viscosity of the total fraction soluble in xylene at room temperature equal to or less than 1.5 dl/g, and the ratio of the amount of component 2) and the amount Of C 4 -C 10 α-olefin(s) in component 2) equal to or higher than 0.80.
Abstract:
A polymer composition comprising (per cent by weight): a) 57%-74%, of a crystalline propylene polymer having an amount of isotactic pentads (mmmm), measured by 13 C-MNR on the fraction insoluble in xylene at 25° C, higher than 97.5 molar % and a polydispersity index ranging from 5 to 10; b) 8 to 15%, of an elastomeric copolymer of ethylene and propylene, the copolymer having an amount of recurring units deriving from ethylene ranging from 30 to 50%, and being partially soluble in xylene at ambient temperature; the polymer fraction soluble in xylene at ambient temperature having an intrinsic viscosity value ranging from 2.5 to 3.5 dl/g; and c) 18-28%, of ethylene homopolymer having an intrinsic viscosity value ranging from 1.5 to 4 dl/g; said composition having a value of melt flow rate ranging from 35 to 60 g/10 min, and the amount of hexane extractables lower than 4.0 wt%.
Abstract:
A polymer composition comprising (per cent by weight): a) 70-84% of a crystalline propylene polymer having an amount of isotactic pentads (mmmm), measured by 13C-MNR on the fraction insoluble in xylene at 25° C., higher than 97.5 molar %; b) 8-15% of an elastomeric copolymer of ethylene and propylene, the copolymer having an amount of recurring units deriving from ethylene ranging from 25 to 50 wt % and being partially soluble in xylene at ambient temperature; the polymer fraction soluble in xylene at ambient temperature having an intrinsic viscosity value ranging from 2.5 to 3.5 dl/g; and c) 8-15% of ethylene homopolymer having an intrinsic viscosity value ranging from 1.5 to 4 dl/g; said composition having a value of melt flow rate ranging from 55 to 90 g/10 min, and the amount of hexane extractables lower than 3.5 wt %.
Abstract:
A propylene composition comprising (percent by weight): A) 70%-95%, of a propylene homopolymer having a Polydispersity Index (P.I.) value of from 4.6 to 10, a fraction insoluble in xylene at 25° C., higher than 90%, and MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230° C. and 2.16 kg load) from 60 to 120 g/10 min; B) 5%-30%, of a copolymer of propylene containing from 34.5% to 30.0% extremes included of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25° C. comprised between 3 and 5 dl/g.
Abstract:
A case for valve-regulated lead-acid battery comprising an olefin polymer composition comprising: A) From 60 wt% to 95 wt%, of a propylene homopolymer, or a copoloymer of propylene containing 3% or less of ethylene, said homopolymer or copolymer having a Polydispersity Index (P.I.) value of from 4.6 to 10 and a fraction insoluble in xylene at 25 °C, higher than 98 molar %; and B) from 5 wt% to 40wt %, of a copolymer of propylene and ethylene containing from 30 wt% to 65 wt% of ethylene derived units; the sum A)+B being 100.
Abstract:
A propylene polymer composition comprising (percent by weight): A) 68%-80%, of a propylene homopolymer having a Polydispersity Index (P.I.) value of from 4.7 to 10 and MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 10 to 30 g/10 min; B) 20%-32%, of a copolymer of propylene containing from 40.1% to 42.5% extremes included of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 3 and 6 dl/g and a MFR L from 4 to 12 g/10 min. Said Propylene polymer composition being particularly suitable for injection moulded articles having high rigidity and high impact properties at room and at low temperatures.
Abstract:
A propylene composition comprising (percent by weight): A) 70%-95%, of a propylene homopolymer having a Polydispersity Index (P.I.) value of from 4.6 to 10, a fraction insoluble in xylene at 25° C., higher than 90%, and MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230° C. and 2.16 kg load) from 60 to 120 g/10 min; B) 5%-30%, of a copolymer of propylene containing from 34.5% to 30.0% extremes included of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25° C. comprised between 3 and 5 dl/g.