Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt% B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100; the composition being characterized by the following features: - molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; - the creep and recovery curve measured on the polymer fuse at 200°C measured accordingto the procedure reported in the characterizing section shows a maximum value between 600 and 200 seconds lower than 53x10-4 1/Pa.
Abstract:
A multilayer film is characterized by having at least a skin layer comprising a propylene -- ethylene copolymers characterized by the following features: ethylene derived units content of between 1.0 wt% and 15.0% wt%; molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; - the content of xylene soluble fraction (XS) and the ethylene derived units content (C2) fulfill the following relation: XS 0.435C2 where XS is the percentage by weight of the fraction soluble in xylene at 25°C and C2 is the percentage by weight of ethylene units in the said copolymers determined via NMR.
Abstract:
A propylene-1-hexene copolymer having: i) a content of 1-hexene derived units ranging from 0.6 wt% to 3.0 wt%; ii) melt flow rate (MFR) measured according to the method ISO 1133 (230° C, 5 kg) ranging from 0.5 g/10 min to 5.0 g/10 min iii) the polydispersity (PI) ranges from 4.5 to 10 and the distribution of molecular weight is of multimodal type; iv) the melting point ranges from 160°C to 145°C; v) the DSC curve (temperature/heat of fusion) shows at least two peaks.