Abstract:
Thermoset polyolefin elastomer obtained by static curing with water a silane-grafted thermoplastic heterophasic polyolefin composition (I) having a flexural modulus equal to or lower than 150 MPa, and comprising: (a) a crystalline propylene homopolymer or copolymer of propylene with up to 15% by weight of ethylene or other alpha-olefin comonomer(s), or their combinations, and (b) a copolymer or a composition of copolymers of ethylene with other alpha-olefins containing from 15% by weight to less then 40% by weight of ethylene; said thermoset polyolefin elastomer having a compression set value of from 30 to 65%, a ratio of elongation at break to compression set values of above 8, and hardness shore A values below 90.
Abstract:
Polypropylene compositions having a MFR value (2.16 kg, 230 °C) from 15 to 200 g/10 min., comprising: A) a propylene polymer or polymer composition selected from propylene homopolymers or copolymers of propylene containing up to 5% by moles of comonomer(s), said homopolymers and copolymers having values of MFR, obtained without degradation treatments, from 500 to 2500 g/10 min., or combinations of the said homopolymers or copolymers; B) a filler or pigment, or their combinations; and optionally C) from 0.5 to 5% by weight, with respect to the total weight of A), B) and C), of a compatibilizer.
Abstract:
Filled polyolefin compositions comprising: A) from 15% to 55% by weight of a polypropylene component; B) from 20% to 80% by weight of a filler; C) from 4% to 25% of an elastomeric polymer or polymer composition; wherein the percentages of A), B) and C) are referred to the sum of A) B) and C), and A) is selected from the following compositions: a) a polypropylene composition containing from 20% to 80% by weight of a polypropylene fraction AI) having a Melt Flow Rate L (MFRI) value of 500 g/ 10 min. or more, and from 20% to 80% by weight of a polypropylene fraction AII) having a Melt Flow Rate L (MFRII) value of from 0.1 to 30 g/10 min., the said percentages of AI) and AII) being referred to the sum of AI) and AII); or b) a polypropylene composition containing from 15% to 72% by weight of a polypropylene fraction AI) having a Melt Flow Rate L (MFRI) value of 500 g/10 min. or more, from 15% to 70% by weight of a polypropylene fraction AII) having a Melt Flow Rate L (MFRII) value of from 0.1 to 30 g/10 min. and from 0.5% to 15% by weight of a compatibilizer Q), the said percentages of AI), AII) and Q) being referred to the sum of AI), AII) and Q).
Abstract:
Filled polyolefin compositions comprising: A) from 20% to 80% by weight of a polypropylene component; B) from 20% to 80% by weight of a filler; wherein the percentages of A) and B) are referred to the sum of A) and B), and A) is selected from the following compositions: a) a polypropylene composition containing from 20% to 80% by weight of a polypropylene fraction AI) having a Melt Flow Rate value of 500 g/10 min. or more, and from 20% to 80% by weight of a polypropylene fraction AII) having a Melt Flow Rate value of from 0.1 to 30 g/10 min., the said percentages of AI) and AII) being referred to the sum of AI) and AII); or b) a polypropylene composition containing from 15% to 72% by weight of a polypropylene fraction AI) having a Melt Flow Rate value of 500 g/10 min. or more, from 15% to 70% by weight of a polypropylene fraction A11) having a Melt Flow Rate value of from 0.1 to 30 g/10 min. and from 0.5% to 15% by weight of a compatibilizer Q), the said percentages of AI), AII) and Q) being referred to the sum of AI), AII) and Q).