Abstract:
A propylene, ethylene, 1-butene terpolymer made from or containing a) from about 1.8 wt % to about 5.9 wt % of ethylene derived units; and b) from about 2.0 wt % to about 4.5 wt % of 1 butene derived units; and having i) a ratio of C2 wt %/C4 wt % in the range from about 0.9 to about 1.3; wherein C2 wt % is the weight percent of ethylene derived units and C4 wt % is the weight percent of 1-butene derived units; ii) a Melt flow rate (determined according to ISO 1133 230° C., 2.16 kg) in the range from about 1.0 to about 30.0 g/10 min; and iii) a xylene soluble fraction at 25° C. between about 10 wt % and about 30 wt %. The weight percentages are based upon the total weight of the terpolymer.
Abstract:
Films or sheets comprising a layer of a heterophasic propylene copolymer containing up to 7.0% by weight of ethylene-derived units and comprising: (a) from 80% to 92% by weight of a matrix phase being a propylene homopolymer or a propylene copolymer containing up to 5% by weight of units derived from ethylene and/or an alpha-olefin; and (b) from 8% to 20% by weight of a rubber phase that is an ethylene-propylene copolymer containing from 20% to 60% by weight of ethylene-derived units.
Abstract:
A strap comprising a propylene and 1-hexene copolymer containing from 0.3wt% to less than 5wt% of 1-hexene derived units said copolymer having a melt flow rate (MFR) determined according to ISO method 1133 (230° C, 2.16 kg ranging from 0.3 to less than 11g/10min.
Abstract:
A fiber comprising a terpolymer containing propylene, ethylene and an alpha olefin of formula CH2=CHZ wherein Z is an hydrocarbon group having from 2 to 10 carbon atoms, wherein: (i) the content of ethylene derived units ranges from 0.5 wt% to 5.0 wt%; (ii) the content of alpha olefin derived units ranges from 1.0 wt% to 5.0 wt%; (iii) the amount (Wt%) of alpha-olefin (C6), the amount (Wt%) of ethylene (C2) and the melting point (Tm) of the terpolymer fulfil the following relation: Tm>157-6*(C2+0.8C6) (iv) the melt flow rate (MFR) (ISO 1133 230°C, 2.16 kg) ranges from 10 to 100 g/10 min.
Abstract:
A propylene polymer composition comprising (weight percentages being referred to the sum of A+B): A propylene polymer composition comprising (weight percentages being referred to the sum of A+B): (A) 60-90% by weight of a copolymer of propylene with ethylene containing less than 2.5%wt of ethylene units; and (B) 10-40% by weight of a copolymer of propylene comprising from 15 to 35%wt of ethylene units, said polymer composition having a melt flow rate value according to ISO 1133 (230°C, 2.16 Kg) of less than 10 g/10min.
Abstract:
Pipe systems having at least one layer comprising a semi-crystalline random polymer of propylene and 0.2 to 5 wt% 1-hexen and optionally a recurring unit selected from ethylene and a C4-C10 α-olefin in an amount from more than 0 to 9 % by moles. The polymer exhibits broad molecular weight distribution, in terms of the ratio of weight average molecular weight to numeric average molecular weight formula (I), ranging from 5 to 11, molecular weight distribution of monomodal type and hexen-1 content in the fraction with an intrinsic viscosity of equal to or higher than 3.3 dl/g lower than the hexen-1 content in the fraction with an intrinsic viscosity of less than 3.3 dl/g.
Abstract:
A propylene polymer composition comprising: a) from 40 wt% to 80 wt% of a propylene 1-hexene copolymer containing from 5.5 to 9.0% by weight, of 1-hexene derived units having a Melt Flow Rate (MFR, measured according to ASTM D 1238, 230°C/2.16 kg, i.e. at 230°C, with a load of 2.16 kg) from 3.5 to 12.0 g/10 min; b) from 20 wt% to 60 wt% of a propylene ethylene copolymer containing from 1.5 wt% to 6.5 wt% of ethylene derived units, a having a Melt Flow Rate (MFR, measured according to ASTM D 1238, 230°C/2.16 kg, i.e. at 230°C, with a load of 2.16 kg) from 3.5 to 12.0 g/10 min.
Abstract:
A terpolymer containing propylene, ethylene and an alpha olefins of formula CH2═CHZ wherein Z is an hydrocarbon group having from 2 to 10 carbon atoms wherein: (i) the content of ethylene derived units ranges from 0.5 wt % to 5.0 wt %; (ii) the content of alpha olefin derived units ranges from 1.0 wt % to 5.0 wt %; (iii) the area of the DSC curve after the peak of the melting point (Tm) represents more than 22%; of the total area of the DSC curve; (iv) the polydispersity index (PI) ranges from 2.0 to 7.0.