公开(公告)号:AU2013226034A1
公开(公告)日:2014-10-02
申请号:AU2013226034
申请日:2013-02-28
Applicant: CORNING INC
Inventor: FADEEV ANDREI GENNADYEVICH , CHANG THERESA , BOOKBINDER DANA CRAIG , PAL SANTONA , SAHA CHANDAN KUMAR , DEMARTINO STEVEN EDWARD , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN
Abstract: Low-friction coatings and glass articles with low-friction coatings are disclosed. According to one embodiment, a coated glass article may include a glass body comprising a first surface and a low-friction coating positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated glass article may be thermally stable at a temperature of at least about 260°C for 30 minutes. A light transmission through the coated glass article may be greater than or equal to about 55% of a light transmission through an uncoated glass article for wavelengths from about 400 nm to about 700 nm. The low- friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150°C to 350°C at a ramp rate of about 10°C/minute.
-
公开(公告)号:SG11201405220WA
公开(公告)日:2014-09-26
申请号:SG11201405220W
申请日:2013-02-28
Applicant: CORNING INC
Inventor: FADEEV ANDREI GENNADYEVICH , CHANG THERESA , BOOKBINDER DANA CRAIG , PAL SANTONA , SAHA CHANDAN KUMAR , DEMARTINO STEVEN EDWARD , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN
Abstract: Low-friction coatings and glass articles with low-friction coatings are disclosed. According to one embodiment, a coated glass article may include a glass body comprising a first surface and a low-friction coating positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated glass article may be thermally stable at a temperature of at least about 260°C for 30 minutes. A light transmission through the coated glass article may be greater than or equal to about 55% of a light transmission through an uncoated glass article for wavelengths from about 400 nm to about 700 nm. The low-friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150°C to 350°C at a ramp rate of about 10°C/minute.
-
公开(公告)号:CA3061515A1
公开(公告)日:2014-06-05
申请号:CA3061515
申请日:2013-11-22
Applicant: CORNING INC
Inventor: CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHNOY , TIMMONS CHRISTOPHER LEE , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE , BOOKBINDER DANA CRAIG
Abstract: The glass containers described herein have at least two performance attributes selected from resistance to delamination, improved strength, and increased damage resistance. In one embodiment, a glass container may include a body having an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. At least the inner surface of the body may have a delamination factor less than or equal to 10. A tenacious inorganic coating may be positioned around at least a portion of the outer surface of the body. The outer surface of the body with the tenacious inorganic coating may have a coefficient of friction less than or equal to 0.7.
-
公开(公告)号:MX386260B
公开(公告)日:2025-03-18
申请号:MX2017001906
申请日:2017-02-10
Applicant: CORNING INC
Abstract: De conformidad con una modalidad, un aparato para soportar puede incluir una pluralidad de elementos de sujeción de mercancía para recibir artículos de vidrio; cada elemento de sujeción de mercancía puede incluir un cuerpo de retención que comprende una bobina de alambre limitando un volumen de recepción de artículos de vidrio; un bobinado más inferior de la bobina de alambre forma un tope de mercancía en el cuerpo de retención; el cuerpo de retención puede incluir una bobina separadora que se extiende desde el cuerpo de retención por debajo del tope de mercancía; una estructura de base puede incluir una pluralidad de aperturas que se extienden a través de la estructura de base; cada uno de la pluralidad de elementos de sujeción de mercancía puede estar colocado en una apertura correspondiente en la estructura de base de tal manera que el cuerpo de retención de cada elemento de sujeción de mercancía está sobre una superficie superior de la estructura de base y la bobina separadora de cada elemento de sujeción de mercancía está debajo de una superficie inferior de la estructura de base.
-
35.
公开(公告)号:MX378948B
公开(公告)日:2025-03-10
申请号:MX2015006897
申请日:2015-05-29
Applicant: CORNING INC
Inventor: CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , TIMMONS CHRISTOPHER LEE , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE
IPC: B32B17/06 , B65D1/40 , B65D23/08 , B65D25/14 , C03C17/00 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/00 , C09D179/08
Abstract: Los contenedores de vidrio descritos en la presente tienen por lo menos dos atributos de rendimiento seleccionados de resistencia a la deslaminación, resistencia mejorada y mayor resistencia al daño; en una modalidad, un contenedor de vidrio puede incluir un cuerpo que tiene una superficie interna, una superficie externa y un grosor de pared que se extiende entre la superficie externa y la superficie interna; por lo menos la superficie interna del cuerpo puede tener un factor de deslaminación menor o igual que 10; se puede colocar un revestimiento inorgánico tenaz alrededor de por lo menos una porción de la superficie externa del cuerpo; la superficie externa del cuerpo con el revestimiento inorgánico tenaz puede tener un coeficiente de fricción menor o igual que 0.7.
-
公开(公告)号:CA3061515C
公开(公告)日:2022-03-29
申请号:CA3061515
申请日:2013-11-22
Applicant: CORNING INC
Inventor: CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHNOY , TIMMONS CHRISTOPHER LEE , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE , BOOKBINDER DANA CRAIG
Abstract: The glass containers described herein have at least two performance attributes selected from resistance to delamination, improved strength, and increased damage resistance. In one embodiment, a glass container may include a body having an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. At least the inner surface of the body may have a delamination factor less than or equal to 10. A tenacious inorganic coating may be positioned around at least a portion of the outer surface of the body. The outer surface of the body with the tenacious inorganic coating may have a coefficient of friction less than or equal to 0.7.
-
公开(公告)号:CA2888831C
公开(公告)日:2019-05-28
申请号:CA2888831
申请日:2013-10-23
Applicant: CORNING INC
Inventor: CHANG THERESA , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , TIMMONS CHRISTOPHER LEE , BOOKBINDER DANA CRAIG
Abstract: According to one embodiment, a glass container may include a body formed from a Type I, Class B glass composition according to ASTM Standard E438-92. The body may have an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. The body may also include a compressively stressed layer extending into the wall thickness from at least one of the outer surface and the inner surface. A lubricous coating may be positioned on at least a portion of the outer surface of the body, wherein the outer surface of the body with the lubricous coating has a coefficient of friction less than or equal to 0.7.
-
公开(公告)号:AU2018200466A1
公开(公告)日:2018-02-08
申请号:AU2018200466
申请日:2018-01-19
Applicant: CORNING INC
Inventor: FADEEV ANDREI GENNADYEVICH , CHANG THERESA , BOOKBINDER DANA CRAIG , PAL SANTONA , SAHA CHANDAN KUMAR , DEMARTINO STEVEN EDWARD , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN
Abstract: A coated pharmaceutical package comprising: a glass body comprising a first surface and a second surface opposite the first surface, wherein the glass body is a glass container formed from a borosilicate glass composition and the first surface is an exterior surface of the glass container; and a low-friction coating positioned on at least a portion of the first surface of the glass body, the low-friction coating comprising: a polymer selected from the group consisting of polyimides, fluoropolymers, silsesquioxane-based polymers, and silicone resins; and a coupling agent layer disposed between the polymer and the first surface of the glass body, wherein the coefficient of friction of the portion of the coated pharmaceutical package with the low-friction coating is at least 20% less than a coefficient of friction of a surface of an uncoated pharmaceutical package formed from the same glass composition.
-
公开(公告)号:AU2016206304B2
公开(公告)日:2018-02-08
申请号:AU2016206304
申请日:2016-07-20
Applicant: CORNING INC
Inventor: FADEEV ANDREI GENNADYEVICH , CHANG THERESA , BOOKBINDER DANA CRAIG , PAL SANTONA , SAHA CHANDAN KUMAR , DEMARTINO STEVEN EDWARD , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN
Abstract: A coated pharmaceutical package comprising: a glass body comprising a first surface and a second surface opposite the first surface, wherein the glass body is a glass container and the first surface is an exterior surface of the glass container; and a low-friction coating positioned on at least a portion of the first surface of the glass body, the low-friction coating comprising a polymer chemical composition, wherein: the coated pharmaceutical package is thermally stable at a temperature of at least about 260'C for 30 minutes; the low-friction coating has a mass loss of less than about 5% of its mass when heated from a temperature of 1 50 C to 350 C at a ramp rate of about 10 C/minute; and the coefficient of friction of the portion of the coated pharmaceutical package with the low-friction coating is at least 20% less than a coefficient of friction of a surface of an uncoated pharmaceutical package formed from a same glass composition.
-
公开(公告)号:AU2013352514B2
公开(公告)日:2017-03-16
申请号:AU2013352514
申请日:2013-11-22
Applicant: CORNING INC
Inventor: CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , TIMMONS CHRISTOPHER LEE , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE
IPC: B32B17/06 , B65D1/40 , B65D23/08 , B65D25/14 , C03C17/00 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/00 , C09D179/08
Abstract: The glass containers described herein have at least two performance attributes selected from resistance to delamination, improved strength, and increased damage resistance. In one embodiment, a glass container may include a body having an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. At least the inner surface of the body may have a delamination factor less than or equal to 10. A tenacious inorganic coating may be positioned around at least a portion of the outer surface of the body. The outer surface of the body with the tenacious inorganic coating may have a coefficient of friction less than or equal to 0.7.
-
-
-
-
-
-
-
-
-