Abstract:
A resin composition includes 1 to 20% by mass of (A) a copolymer containing a conjugated diene unit and a vinyl aromatic compound unit, 1 to 20% by mass of (B) a softening agent for rubber, and 70 to 95% by mass of (C) metal hydroxide, in which (A) the copolymer containing the conjugated diene unit and the vinyl aromatic compound unit includes a plurality of polymer blocks of the vinyl aromatic compound unit.
Abstract:
The present invention relates to an epoxy resin composition which comprises a phosphorus-containing modified epoxy resin (A) consisting of a compound (a) represented by Formula (a); a novolak epoxy resin (B); a hardener (C) for epoxy resins; and a metal hydroxide (D), wherein the content in mass % of the phosphorus-containing modified epoxy resin (A), CA, and the content in mass % of the metal hydroxide (D), CD, relative to the total amount of the epoxy resin composition, satisfy the following Formulas (1), (2), and (3): (1) 2.5CA+CD≧5; (2) 6≦CA≦40; and (3) 3≦CD≦30. This epoxy resin composition can give a composite material which has excellent flame retardancy even when neither a halogenated flame retardant, nor red phosphorus, nor a phosphoric acid ester is contained therein. According to the invention, it is also possible to provide a prepreg and a fiber-reinforced composite material obtained using the prepreg.
Abstract:
A flame retardant resin composition including: a thermoplastic resin; and a flame retardant, wherein the flame retardant includes a phosphorylated lignin derivative, and wherein the phosphorylated lignin derivative is produced by adding phosphoric acid to a lignin derivative obtained by subjecting a naturally occurring lignin to a predetermined treatment.
Abstract:
Commercial thermoplastic clean flame retardant materials in wire and cable insulation are mechanically unstable due to high filler loading. In the present invention, thermoplastic, black color, clean flame retardant composition using carbon nano tubes (CNT) is made. The resultant compositions possess very low smoke and toxicity. CNT with outer diameter of 40-60 nm and length of under 20 μm are used to increase mechanical properties and flame retardancy. Thermo plastically extruded composition consists of each component by parts by weight as follows: 100 of resin (polyolefin or 100 of polyolefin/ethylene propylene diene monomer (EPDM)), 90-150 of non-halogen containing flame retardants, 1-20 of auxiliary secondary flame retardant agents, 2-4 of CNT (outer diameter of 40-60 nm) and length under 20 μm and 0.2-1.0 of antioxidants. A reliable method for producing thermoplastic black color clean flame retardant insulation material for wire and cable without deterioration of mechanical properties is discussed.
Abstract:
The present invention relates to a flame-retardant polyolefin resin containing a blend which comprises 0.1-80 wt % of piperazine metal salts or polymers thereof, 10-80.0 wt % of nitrogen-containing synergists or phosphorus/nitrogen retardants, and 1-50 wt % of inorganic compounds, wherein the sum of the components of the blend is 100 wt %.
Abstract:
A low-gloss thermoplastic resin composition that can have excellent heat resistance and weather resistance of the present invention includes (A) a thermoplastic resin forming a first dispersed phase; and (B) an acrylic resin forming a second dispersed phase, wherein the first dispersed phase has a network configuration.
Abstract:
A flame and drip resistant halogen-free insulating composition which is extrudible and suitable for a insulating coating or a sheath of electrical conductors, which has a mixture of low density polyethylene, at least one polyolefin grafted with maleic anhydride, at least one flame retardant, and at least one filler, and have a burning time of less than 8 minutes after the exposure to a flame for 40 minutes with a damage extent of less than 70 centimeters.
Abstract:
Provided are a resin blend for melt processing, a pellet and a method of preparing a resin article using the same. The resin blend may include a first resin, and a second resin having a difference in melt viscosity from the first resin of 0.1 to 3000 pa*s at a shear rate of 100 to 1000 s−1 and a processing temperature of the resin blend. The resin blend can improve mechanical and surface characteristics of a resin article. Further, since coating or plating is not required for manufacturing a resin article, a manufacturing time and/or cost can be reduced, and productivity can be increased.
Abstract:
Provided are a resin blend for melt processing, a pellet and a method of preparing a resin article using the same. The resin blend may include a first resin, and a second resin having a difference in solubility parameter from the first resin at 25° C. of 0.001 to 10 (J/cm3)1/2. The resin blend can improve mechanical and surface characteristics of a resin article. Further, since coating or plating is not required for manufacturing a resin article, a manufacturing time and/or cost can be reduced, and productivity can be increased.
Abstract translation:提供了用于熔融加工的树脂共混物,颗粒和使用其制备树脂制品的方法。 树脂共混物可以包括第一树脂和在25℃下与第一树脂的溶解度参数差为0.001至10(J / cm 3)1/2的第二树脂。 树脂共混物可以改善树脂制品的机械和表面特性。 此外,由于制造树脂制品不需要涂覆或电镀,因此可以降低制造时间和/或成本,并且可以提高生产率。
Abstract:
The invention relates to a polymer composition comprising high impact polystyrene (HIPS) and a combination of flame retardants which are brominated epoxy oligomers and polymers. A process for preparing the HIPS composition through a masterbatch route and a masterbatch composition which contains the flame retardants are also disclosed.