公开(公告)号:KR1019940011693B1
公开(公告)日:1994-12-23
申请号:KR1019920017340
申请日:1992-09-23
Applicant: 한국과학기술연구원
IPC: H01F1/00
Abstract: The method is to manufacture a high frequency inductant core material which can be sintered at a low temperture. The core material includes Fe2O3 47.5-51.5 mole%, CuO 5-15 mole%, NiO 15-35 mole%, ZnO 5.5-25.5 mole% with Co2O3 0.01-3 wt.% or WO3 0.01-1 wt.% addition. The core material is manufactured by sintering the powders at 900-950 deg.C.
Abstract translation: 该方法是制造可在低温下烧结的高频感应芯材料。 核心材料包括Fe2O3 47.5-51.5摩尔%,CuO 5-15摩尔%,NiO 15-35摩尔%,ZnO 5.5-25.5摩尔%,Co 2 O 3 0.01-3重量%或WO 3 0.01-1重量%添加。 核心材料通过在900-950℃下烧结粉末制造。
-
-
-
公开(公告)号:KR100118814B1
公开(公告)日:1997-07-24
申请号:KR1019940015749
申请日:1994-07-01
Applicant: 한국과학기술연구원
IPC: C04B35/462
-
公开(公告)号:KR1019970000061B1
公开(公告)日:1997-01-04
申请号:KR1019940008605
申请日:1994-04-22
Applicant: 한국과학기술연구원
IPC: H01P11/00
Abstract: The dielectric material comprises (Zr, Sn)TiO4 system, more particularly including 0.3-1.0 wt.% B2O3 as curing agent, and 0.75-3.0 wt.% NiO and 0.1-1.0 wt.% Nd2O3. La2O3 or Ta2O5 can also use as a curing agent, wherein the (Zr, Sn)TiO4 system has the mole ratio formula of 0.72 ZrO4 + 0.3 SnO2 + 1.0 TiO2.
Abstract translation: 电介质材料包括(Zr,Sn)TiO4体系,更具体地包括0.3-1.0重量%的B 2 O 3作为固化剂,以及0.75-3.0重量%的NiO和0.1-1.0重量%的Nd 2 O 3。 La2O3或Ta2O5也可用作固化剂,其中(Zr,Sn)TiO4体系的摩尔比为0.72 ZrO4 + 0.3SnO2 + 1.0TiO3。
-
公开(公告)号:KR1019960011351B1
公开(公告)日:1996-08-22
申请号:KR1019930030637
申请日:1993-12-29
Applicant: 한국과학기술연구원
IPC: C04B35/26
Abstract: The sintered ferrite at a low temperature is prepared by mixing and heat-treating Bi2O3 and other oxides to calcined ferrite powder; and adding a liquid forming agent to form a stable phase. Bi2O3 of the liquid forming aid agent and other oxides are mixed to give a composition such that the liquid phase temperature in the phase diagram is in the range of 750 to 850 deg.C. The ferrite can be used for a noise filter and inductor.
Abstract translation: 通过将Bi 2 O 3等氧化物与煅烧铁氧体粉末混合并热处理,制备低温烧结铁氧体; 并加入液体形成剂以形成稳定的相。 将液体形成助剂和其它氧化物的Bi 2 O 3混合,得到相图中的液相温度在750〜850℃的范围内的组成。 铁氧体可用于噪声滤波器和电感器。
-
-
-
公开(公告)号:KR1019960006242B1
公开(公告)日:1996-05-11
申请号:KR1019930020437
申请日:1993-10-04
Applicant: 한국과학기술연구원
IPC: C04B35/46
CPC classification number: H01B3/12 , C04B35/465 , H01P7/10
Abstract: The dielectric ceramic composition for high frequency is prepared in such a manner that CaTiO3 having (+) temperature coefficient and (Li1/2Nd1/2)TiO3 having (-) temperature coefficient are mixed with mole ratio of 0.1-0.3 of CaTiO3 and 0.9-0.7 of (Li1/2Nd1/2)TiO3.
Abstract translation: 具有(+)温度系数的CaTiO 3和具有( - )温度系数的(Li1 / 2Nd1 / 2)TiO3与CaTiO3的摩尔比为0.1-0.3和0.9〜 (Li1 / 2Nd1 / 2)TiO3的0.7。
-
公开(公告)号:KR1019960004279A
公开(公告)日:1996-02-23
申请号:KR1019940015749
申请日:1994-07-01
Applicant: 한국과학기술연구원
IPC: C04B35/462
-
-
-
-
-
-
-
-
-