Abstract:
A propylene composition comprising (percent by weight): A) 70%-95%, of a propylene homopolymer having a Polydispersity Index (P.I.) value of from 4.6 to 10, a fraction insoluble in xylene at 25°C, higher than 90 %, and MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 100 to 250 g/10 min; B) 5%-30%, of a copolymer of propylene containing from 36% to 44% of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25°C comprised between 3 and 5 dl/g.
Abstract:
A terpolymer containing propylene, ethylene and an alpha olefins of formula CH2═CHZ wherein Z is an hydrocarbon group having from 2 to 10 carbon atoms wherein: (i) the content of ethylene derived units ranges from 0.5 wt % to 5.0 wt %; (ii) the content of alpha olefin derived units ranges from 1.0 wt % to 5.0 wt %; (iii) the area of the DSC curve after the peak of the melting point (Tm) represents more than 22%; of the total area of the DSC curve; (iv) the polydispersity index (PI) ranges from 2.0 to 7.0.
Abstract:
A container comprising a propylene, ethylene, 1-hexene terpolymer wherein in the terpolymer: (i) the content of ethylene derived units ranges from 0.6 wt% to 1.1 wt%; (ii) the content of 1-hexene derived units ranges from 1.1 wt% to 2.8 wt%; (iii) the ratio between the ethylene derived units content and the 1-hexene derived units content C2/C6 fulfills the following equation (I); C2/C6
Abstract:
A heterophasic polypropylene composition comprising (percent by weight referred to the sum of components A) and B)): A) from 80 % to 97 % of a random copolymer of propylene containing from 0.1 to 4 % of 1-hexene derived units; B) from 3-20 % of a copolymer of propylene and ethylene having a content of ethylene derived units ranging from 50 % to 55 % extremes excluded; wherein the heterophasic polypropylene composition is endowed with a Melt Flow Rate: measured according to ISO 1133 (230 °C, 5 Kg) ranging from 0.5 to 5 g/10min; and an intrinsic viscosity (IV) of the fraction soluble in xylene at room temperature ranging from 2.5 to 5.5;
Abstract:
A propylene composition comprising (percent by weight): A) 70%-95%, of a propylene homopolymer having a Polydispersity Index (P.I.) value of from 4.6 to 10, a fraction insoluble in xylene at 25°C, higher than 90 %, and MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 100 to 250 g/10 min; B) 5%-30%, of a copolymer of propylene containing from 36% to 44% of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25°C comprised between 3 and 5 dl/g.