Abstract:
The present disclosure relates to highly filled polyolefin compositions with improved balance of properties particularly for applications where puncture and tear resistance is requested comprising a flexible heterophasic polyolefin composition (I), consisting of a crystalline polymer fraction (A) consisting of a copolymer of propylene with ethylene having a fraction insoluble in xylene at 25° C. of at least 90% by weight, and an elastomeric fraction (B) consisting of a copolymer or blend of copolymers of ethylene with propylene; the copolymer or blend containing units derived from ethylene in a quantity lower than 40% by weight. The fraction soluble in xylene at 25° C. of the polyolefin composition having an IVgpc lower than 2.5 dl/g, a broad molecular weight distribution Mw/Mn (GPC) equal to or higher than 4, and a Mz/Mw (GPC) equal to or higher than 2.5.
Abstract:
Polyolefin compositions suitable for injection molded items e.g. for impact bumpers and car interiors comprising from 30% to 90% by weight of an heterophasic propylene polymer composition (A) ; and from 10% to 70% by weight of a multimodal ethylene/butene-1 copolymer (B); having density from 0.850 to 0.935 g/cm 3 , total comonomer content from 6% to 30% by weight, Mw/Mn from 4 to 20; intrinsic viscosity in decalin at 135°C from 1.0 to 4.0 dL/g, and comprising an HDPE fraction (HDPE %wt) up to 30%wt; further comprising from 0 to 50 % by weight of a filler (C) and optionally, in amount up to 10% by weight with respect to the overall composition, an impact modifier masterbatch component D consisting of an ultra-soft heterophasic copolymer component.
Abstract:
Polyolefin composition with improved sealability comprising from 70 to 95% of one or more copolymers of propylene with one or more comonomers selected from ethylene, a C4-C8 α-olefin and combinations thereof, where the comonomer, or comonomers, content in (A) is from 5 to 25%, and from 5 to 30% by weight of butene-1 (co)polymer (B) having a flexural modulus of 60 MPa or less.
Abstract:
Polyolefin compositions comprising, all percentages being by weight: A) from 70 to 95%, of a compositions comprising (by weight): A I ) 15-80% of one or more copolymers of propylene; A II ) 20-85% of one or more copolymers with different comonomer(s) content than in A) B) from 5 to 30% of an elastomeric or plastomeric polyolefin or polyolefin composition.
Abstract:
A multilayer film in which at least one layer (A) comprises a copolymer (A1) of propylene with hexene-1 containing from 4 to 10% by weight of hexene-1 and having Melt Flow Rate from 1 to 10 g/10 min.; and at least one layer (B) comprises a copolymer (B1) of ethylene containing up to 20 mol % of CH 2 =CHR α-olefins and having a density from 0.88 to 0.945 g/cm 3 .
Abstract:
A propylene 1-hexene copolymer containing from 5.5 to 9.0% by weight, of 1-hexene derived units having: a) two peaks in the DSC plot having a difference in height ranging from 0 to 5 mW; b) the higher melting temperature, measured by DSC, ranging from 141.0 °C to 151.0 °C; c) Melt Flow Rate (MFR, measured according to ASTM D 1238, 230°C/2.16 kg, from 3.5 to 8.0 g/10 min.