公开(公告)号:DE4014261A1
公开(公告)日:1991-11-07
申请号:DE4014261
申请日:1990-05-04
Applicant: BASF AG
Inventor: WITTENBERG DIETMAR DR , HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , O'CALLAGHAN MICHAEL P DR , RIETHUES MICHAEL DR
IPC: C08F2/44 , C08F2/18 , C08J9/00 , C08J9/16 , C08K5/00 , C08K5/01 , C08K5/05 , C08K5/06 , C08K5/36 , C08K5/41 , C08L25/04 , C08L33/00
Abstract: Expandable styrene polymers containing …… a) a styrene polymer, … b) from 0.05 to 3 % by weight, based on a), of water, … c) from 0.001 to 1 % by weight, based on a), of a finely divided organic polymer having a water-absorption capacity of at least 10 g/g, … d) from 0.5 to 8 % by weight, based on a), of a C3- to C6-hydrocarbon, and optionally … e) conventional additives in effective amounts, … are distinguished by good flow properties and a low degree of clumping during prefoaming.
-
公开(公告)号:DE4005164A1
公开(公告)日:1991-08-22
申请号:DE4005164
申请日:1990-02-17
Applicant: BASF AG
Inventor: WEBER REINHOLD , ALICKE GERHARD , WEILBACHER MANFRED DR , GUHR UWE DR , HAHN KLAUS DR
IPC: B29C47/00 , B29C44/00 , B29K25/00 , B29K105/04 , B29L7/00 , C08J9/00 , C08J9/12 , C08L25/06 , C08L73/00
Abstract: Foam boards (sheets) of high heat distortion resistance contain a) from 80 to 99% by weight of a styrene polymer and b) from 1 to 20% by weight of poly-1,4-phenylenesulphide and optionally conventional additives. They are produced by extrusion using a low-boiling blowing agent.
-
公开(公告)号:DE4000542A1
公开(公告)日:1991-07-11
申请号:DE4000542
申请日:1990-01-10
Applicant: BASF AG
Inventor: WEBER REINHOLD , ALICKE GERHARD , WEILBACHER MANFRED DR , GUHR UWE DR , HAHN KLAUS DR
IPC: B29C48/305 , B29K25/00 , B29K73/00 , B29K105/04 , B29L7/00 , C08J9/00 , C08J9/12 , C08L25/06
Abstract: Foam boards (sheets) of high heat distortion resistance contain a) from 80 to 99 % by weight of a styrene polymer and b) from 1 to 20 % by weight of poly(2,6-dimethyl-1,4-phenylene oxide) and optionally conventional additives. They are produced by extrusion using a low-boiling blowing agent.
-
公开(公告)号:DE3904370A1
公开(公告)日:1990-08-16
申请号:DE3904370
申请日:1989-02-14
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , GELLERT ROLAND DR
Abstract: Bead-form expandable moulding compositions of high heat resistance contain from 80 to 99 % by weight of a styrene polymer, from 1 to 20 % by weight of poly(2,6-dimethyl)-1,4-diphenyl ether, from 3 to 10 % by weight of a C3-C6-hydrocarbon as blowing agent and optionally conventional additives. They are obtained by suspension polymerisation of a solution of the polyphenylene ether in styrene.
-
公开(公告)号:ES2083412T3
公开(公告)日:1996-04-16
申请号:ES90120264
申请日:1990-10-23
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , HOENL HANS DR
Abstract: Expandable styrene polymers which contain from 10 to 90% by weight of a crosslinked styrene-diene copolymer containing from 2 to 45% by weight of the diene, and from 1 to 10% by weight of a C3- to C6-hydrocarbon as blowing agent can be processed to give foams which have high resistance to aromatics.
-
公开(公告)号:DE59010161D1
公开(公告)日:1996-04-04
申请号:DE59010161
申请日:1990-10-23
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , HOENL HANS DR
Abstract: Expandable styrene polymers which contain from 10 to 90% by weight of a crosslinked styrene-diene copolymer containing from 2 to 45% by weight of the diene, and from 1 to 10% by weight of a C3- to C6-hydrocarbon as blowing agent can be processed to give foams which have high resistance to aromatics.
-
公开(公告)号:AT134675T
公开(公告)日:1996-03-15
申请号:AT90120264
申请日:1990-10-23
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , HOENL HANS DR
Abstract: Expandable styrene polymers which contain from 10 to 90% by weight of a crosslinked styrene-diene copolymer containing from 2 to 45% by weight of the diene, and from 1 to 10% by weight of a C3- to C6-hydrocarbon as blowing agent can be processed to give foams which have high resistance to aromatics.
-
公开(公告)号:DE59007037D1
公开(公告)日:1994-10-13
申请号:DE59007037
申请日:1990-06-21
Applicant: BASF AG
Inventor: HINTZ HANS DR , GUHR UWE DR , HAHN KLAUS DR , KEPPLER HANS GEORG DR
Abstract: Bead-form expandable styrene polymers are obtained by suspension polymerization of styrene with addition of from 1 to 10% by weight of C3- to C6-hydrocarbons as blowing agents and, if desired, customary additives, where (a) the polymerization is initiated by rapidly heating the polymerization batch to form 80 DEG to 90 DEG C. within a maximum of 2 hours, (b) subsequently allowing the reaction temperature to increase to from 120 DEG C. to 130 DEG C. by from 8 DEG to 17 DEG C. per hour, and (c) the conversion is formed 30 to 60% when 100 DEG C. is reached, and (d) the conversion is 80% or more when the maximum temperature is reached, and (e) the batch is subsequently kept at from 100 DEG to 130 DEG C. until the residual monomer content in the polymer has dropped to less than 0.1%.
-
公开(公告)号:AT111130T
公开(公告)日:1994-09-15
申请号:AT90111719
申请日:1990-06-21
Applicant: BASF AG
Inventor: HINTZ HANS DR , GUHR UWE DR , HAHN KLAUS DR , KEPPLER HANS GEORG DR
Abstract: Bead-form expandable styrene polymers are obtained by suspension polymerization of styrene with addition of from 1 to 10% by weight of C3- to C6-hydrocarbons as blowing agents and, if desired, customary additives, where (a) the polymerization is initiated by rapidly heating the polymerization batch to form 80 DEG to 90 DEG C. within a maximum of 2 hours, (b) subsequently allowing the reaction temperature to increase to from 120 DEG C. to 130 DEG C. by from 8 DEG to 17 DEG C. per hour, and (c) the conversion is formed 30 to 60% when 100 DEG C. is reached, and (d) the conversion is 80% or more when the maximum temperature is reached, and (e) the batch is subsequently kept at from 100 DEG to 130 DEG C. until the residual monomer content in the polymer has dropped to less than 0.1%.
-
公开(公告)号:AT93533T
公开(公告)日:1993-09-15
申请号:AT90108204
申请日:1990-04-30
Applicant: BASF AG
Inventor: WITTENBERG DIETMAR DR , HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR
IPC: C08F2/18 , C08F283/00 , C08F291/02 , C08J9/16 , C08J9/18 , C08J9/20 , C08L51/04
-
-
-
-
-
-
-
-
-