公开(公告)号:DE59010161D1
公开(公告)日:1996-04-04
申请号:DE59010161
申请日:1990-10-23
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , HOENL HANS DR
Abstract: Expandable styrene polymers which contain from 10 to 90% by weight of a crosslinked styrene-diene copolymer containing from 2 to 45% by weight of the diene, and from 1 to 10% by weight of a C3- to C6-hydrocarbon as blowing agent can be processed to give foams which have high resistance to aromatics.
-
公开(公告)号:AT134675T
公开(公告)日:1996-03-15
申请号:AT90120264
申请日:1990-10-23
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , HOENL HANS DR
Abstract: Expandable styrene polymers which contain from 10 to 90% by weight of a crosslinked styrene-diene copolymer containing from 2 to 45% by weight of the diene, and from 1 to 10% by weight of a C3- to C6-hydrocarbon as blowing agent can be processed to give foams which have high resistance to aromatics.
-
公开(公告)号:DE59007037D1
公开(公告)日:1994-10-13
申请号:DE59007037
申请日:1990-06-21
Applicant: BASF AG
Inventor: HINTZ HANS DR , GUHR UWE DR , HAHN KLAUS DR , KEPPLER HANS GEORG DR
Abstract: Bead-form expandable styrene polymers are obtained by suspension polymerization of styrene with addition of from 1 to 10% by weight of C3- to C6-hydrocarbons as blowing agents and, if desired, customary additives, where (a) the polymerization is initiated by rapidly heating the polymerization batch to form 80 DEG to 90 DEG C. within a maximum of 2 hours, (b) subsequently allowing the reaction temperature to increase to from 120 DEG C. to 130 DEG C. by from 8 DEG to 17 DEG C. per hour, and (c) the conversion is formed 30 to 60% when 100 DEG C. is reached, and (d) the conversion is 80% or more when the maximum temperature is reached, and (e) the batch is subsequently kept at from 100 DEG to 130 DEG C. until the residual monomer content in the polymer has dropped to less than 0.1%.
-
公开(公告)号:AT111130T
公开(公告)日:1994-09-15
申请号:AT90111719
申请日:1990-06-21
Applicant: BASF AG
Inventor: HINTZ HANS DR , GUHR UWE DR , HAHN KLAUS DR , KEPPLER HANS GEORG DR
Abstract: Bead-form expandable styrene polymers are obtained by suspension polymerization of styrene with addition of from 1 to 10% by weight of C3- to C6-hydrocarbons as blowing agents and, if desired, customary additives, where (a) the polymerization is initiated by rapidly heating the polymerization batch to form 80 DEG to 90 DEG C. within a maximum of 2 hours, (b) subsequently allowing the reaction temperature to increase to from 120 DEG C. to 130 DEG C. by from 8 DEG to 17 DEG C. per hour, and (c) the conversion is formed 30 to 60% when 100 DEG C. is reached, and (d) the conversion is 80% or more when the maximum temperature is reached, and (e) the batch is subsequently kept at from 100 DEG to 130 DEG C. until the residual monomer content in the polymer has dropped to less than 0.1%.
-
公开(公告)号:AT93533T
公开(公告)日:1993-09-15
申请号:AT90108204
申请日:1990-04-30
Applicant: BASF AG
Inventor: WITTENBERG DIETMAR DR , HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR
IPC: C08F2/18 , C08F283/00 , C08F291/02 , C08J9/16 , C08J9/18 , C08J9/20 , C08L51/04
-
公开(公告)号:DE59000920D1
公开(公告)日:1993-04-01
申请号:DE59000920
申请日:1990-07-19
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , WITTENBERG DIETMAR DR
IPC: C08F283/00 , C08J9/00 , C08J9/20 , C08J9/14 , C08L25/06
Abstract: Expandable molding compositions having high heat distortion resistance and containing from 80 to 99% by weight of a styrene polymer, 1 to 20% by weight of poly-1,4-phenylene sulfide, from 1 to 10% by weight of a C3-C6-hydrocarbon as blowing agent and, if desired, customary additives, are obtained by suspension polymerization of a solution of the polyphenylene sulfide in styrene.
-
公开(公告)号:DE59000743D1
公开(公告)日:1993-02-25
申请号:DE59000743
申请日:1990-04-24
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , ROEHRIG KARL HEINZ
IPC: C08J9/14 , C08J9/20 , C08K3/26 , C08K3/30 , C08K5/02 , C08K5/17 , C08K5/3492 , C08K13/02 , C08L25/02 , C08L25/04
Abstract: Expandable styrene polymers which contain a C3-C6-hydrocarbon as a blowing agent, an organic bromine compound as a flameproofing agent and small amounts of ammonium salt and of an organic amine give, on expansion, foams which have a particularly homogenous foam structure and a good heat insulation effect.
-
公开(公告)号:DE4038042A1
公开(公告)日:1992-06-04
申请号:DE4038042
申请日:1990-11-29
Applicant: BASF AG
Inventor: HINTZ HANS DR , HAHN KLAUS DR , GUHR UWE DR , RIETHUES MICHAEL DR
IPC: C08J9/14 , C08F2/18 , C08F2/44 , C08J9/00 , C08J9/16 , C08L25/00 , C08L25/04 , C08L25/08 , C08L25/10
Abstract: Oil-resistant expandable styrene polymers containing …… a) from 10 to 90% by weight of uncrosslinked polystyrene and/or an uncrosslinked styrene copolymer containing at least 50% by weight of copolymerised styrene, … b) from 10 to 90% by weight of a crosslinked styrene polymer which contains at least 0.1% by weight, but less than 2% by weight, of a copolymerised monomer containing at least two olefinic double bonds, … c) from 1 to 10% by weight, based on the sum of a) and b), of a C3- to C6-hydrocarbon as blowing agent, and optionally … d) conventional additives in effective amounts, … where the mixture of a) and b) has a melt flow index MFI (200 DEG C, 5.0 kp) in accordance with DIN 53 735 of between 1 and 20 [g/10 min].
-
公开(公告)号:DE3936596A1
公开(公告)日:1991-05-08
申请号:DE3936596
申请日:1989-11-03
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , HOENL HANS DR
Abstract: Expandable styrene polymers which contain from 10 to 90% by weight of a crosslinked styrene-diene copolymer containing from 2 to 45% by weight of the diene, and from 1 to 10% by weight of a C3- to C6-hydrocarbon as blowing agent can be processed to give foams which have high resistance to aromatics.
-
公开(公告)号:DE3931862A1
公开(公告)日:1991-04-04
申请号:DE3931862
申请日:1989-09-23
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , WITTENBERG DIETMAR DR
Abstract: Expandable styrene polymers containing a) 80 to 99% by weight of polystyrene, b) 1 to 20% by weight of a styrene-soluble polymer having a softening temperature above 140 DEG C, c) 3 to 10% by weight, based on the sum of a) and b), of a C3- to C6-hydrocarbon as a blowing agent, and optionally d) conventional additives, in which the mixture of components a) and b) has a melt flow index MFI 200/5 of between 15 and 30, are distinguished by high heat distortion resistance and good expandability.
-
-
-
-
-
-
-
-
-