公开(公告)号:AU2002366630A1
公开(公告)日:2003-06-23
申请号:AU2002366630
申请日:2002-11-21
Applicant: CABOT CORP
Inventor: WANG TING , WANG MENG-JIAO , MCCONNELL GLENDON A , REZNEK STEVEN R
IPC: C08L101/00 , C08K3/04 , C08L21/00 , C08K3/00
Abstract: Elastomer composites and elastomer blends comprising particulate fillers having selected and surface area values are disclosed as well as elastomer composites and elastomer blends having improved properties. Methods of making and using elastomer composites and elastomer blends are also disclosed.
-
公开(公告)号:CA2305702A1
公开(公告)日:1999-04-08
申请号:CA2305702
申请日:1998-09-28
Applicant: CABOT CORP
Inventor: MORGAN ALLAN CLARK , CHUNG BIN , SHELL JAMES A , TOKITA NOBORU , MABRY MELINDA ANN , PODOBNIK IVAN ZLATKO , WANG TING
IPC: B01F5/02 , B29B7/76 , B29B15/04 , B60C1/00 , C08C1/14 , C08C1/15 , C08J3/215 , C08J3/22 , C08K3/04 , C08K3/36 , C08L21/00
Abstract: Elastomer composite blends are produced by novel wet/dry mixing methods and apparatus. In the wet mixing step or stage, fluid streams of particulate filler and elastomer latex are fed to the mixing zone of a coagulum reactor to form a mixture in semi-confined flow continuously from the mixing zone through a coagulum zone to a discharge end of the reactor. The particulate filler fluid is fed under high pressure to the mixing zone, such as to form a jet stream to entrain elastomer latex fluid sufficiently energetically to substantially completely coagulate the elastomer with the particulate filler prior to the discharge end. Highly efficient and effective elastomer coagulation is achieved without the need for a coagulation step involving exposure to acid or salt solution or the like. Elastomer composites are produced. Such elastomer composites may be cured or uncured, and combine material properties, such as choice of filler, elastomer, level of filler loading, and macro-dispersion, not previously achieved. The coagulum produced by such wet mixing step, with or without intermediate processing steps, is then mixed with additional elastomer in a dry mixing step or stage to form elastomer composite blends. The additional elastomer to the coagulum may be the same as or different from the elastomer(s) used in the wet mixing step.
-
公开(公告)号:MX337856B
公开(公告)日:2016-03-16
申请号:MX2010008684
申请日:2009-02-05
Applicant: CABOT CORP
Inventor: GREEN MARTIN C , ZHANG XUAN , MORRIS MICHAEL D , WANG MENG-JIAO , WANG TING , TIRU-MALA VIJAY R
IPC: C08J3/22
Abstract: Se describe un método para producir un material mixto de elastómero. El método incluye A) combinar un primer fluido que comprende látex de elastómero con un segundo fluido que comprende material de relleno particulado; B) hacer que el látex de elastómero coagule, con lo cual se forma el grumo de mezcla madre; C) llevar el grumo de mezcla madre hasta un contenido de agua de aproximadamente 1 por ciento en peso hasta aproximadamente 20 por ciento en peso, con lo cual se forma un coágulo deshidratado; D) eliminar el agua a partir del coágulo deshidratado sometiendo el coágulo deshidratado a energía mecánica, con lo cual se ocasiona que el coágulo deshidratado se caliente como resultado de la fricción, al tiempo que se permite que el coágulo deshidratado logre una temperatura de aproximadamente 130°C hasta aproximadamente 190°C, en el cual el contenido de agua se reduce aproximadamente a 0.5% hasta aproximadamente 3% y en el cual sustancialmente todo el decremento en contenido de agua se logra mediante evaporación, con lo cual se produce una mezcla madre plastificada; y E) someter la mezcla madre plastificada a por lo menos 0.3 MJ/kg adicionales de energía mecánica al tiempo que se reduce adicionalmente el contenido de agua.
-
公开(公告)号:CA2773595C
公开(公告)日:2014-02-04
申请号:CA2773595
申请日:2010-09-16
Applicant: CABOT CORP
Inventor: ZHANG XUAN , WANG TING , MORRIS MICHAEL D
Abstract: A wet mix elastomer composite comprising carbon black dispersed in an elastomer including a blend of a natural rubber and styrene-butadiene rubber. When the wet mix elastomer composite is processed with CTV Method 1, the vulcanized wet mix elastomer composite exhibits a resistivity that A) has a natural logarithm satisfying the equation In(resistivity) >= -0.1(loading) + x, where x is 14, or B) is at least 2.9 times greater than the resistivity of a vulcanized dry mix elastomer composite having the same composition and prepared using Comparative CTV Method 1.
-
公开(公告)号:AU2010296002B2
公开(公告)日:2013-07-18
申请号:AU2010296002
申请日:2010-09-16
Applicant: CABOT CORP
Inventor: WANG TING , WANG MENG-JIAO , MARIADASS BERNARD , GOVINDAN THIRUNAVUC KARASU , DAS THIRUHELVANATHAN ANTHONY , LEE BOON KWANG , ZHANG XUAN
Abstract: A method of producing a coagulated latex composite. A coagulating mixture of a first elastomer latex and a particulate filler slurry is flowed along a conduit, and a second elastomer latex is introduced into the flow of the coagulating mixture.
-
公开(公告)号:ES2400790T3
公开(公告)日:2013-04-12
申请号:ES10182699
申请日:2002-11-21
Applicant: CABOT CORP
Inventor: WANG TING , WANG MENG-JIAO , MCCONNELL GLENDON A , REZNEK STEVEN R
IPC: C08L21/00 , C08L101/00 , C08K3/00 , C08K3/04
Abstract: Una composición de elastómero que comprende un caucho para propósito general y relleno en partículasdisperso en el caucho para propósito general, en donde el relleno en partículas comprende una cantidad de por lomenos un negro de humo que tiene valores de estructura y área superficial que satisfacen la ecuación CDBP, elnúmero de adsorción de dibultilftalato después que la muestra se ha triturado, medido de acuerdo con el método deprueba ASTM D-3493,
-
公开(公告)号:PT2292689E
公开(公告)日:2013-02-07
申请号:PT10182699
申请日:2002-11-21
Applicant: CABOT CORP
Inventor: WANG TING , WANG MENG-JIAO , MCCONNELL GLENDON A , REZNEK STEVEN R
IPC: C08L21/00 , C08L101/00 , C08K3/00 , C08K3/04
-
公开(公告)号:AU2009210723B2
公开(公告)日:2012-08-16
申请号:AU2009210723
申请日:2009-02-05
Applicant: CABOT CORP
Inventor: MORRIS MICHAEL D , GREEN MARTIN C , WANG TING , ZHANG XUAN , TIRUMALA VIJAY R , WANG MENG-JIAO
IPC: C08J3/22
Abstract: A method of producing an elastomer composite. The method includes A) combining a first fluid comprising elastomer latex with a second fluid comprising particulate filler; B) causing the elastomer latex to coagulate, thereby forming masterbatch crumb; C) bringing the masterbatch crumb to a water content of about 1 weight percent to about 20 weight percent, thereby forming a dewatered coagulum; D) removing water from the dewatered coagulum by subjecting the dewatered coagulum to mechanical energy, thereby causing the dewatered coagulum to heat as a result of friction, while allowing the dewatered coagulum to achieve a temperature of about 130°C to about 19O°C, wherein water content is reduced to about 0.5 % to about 3 % and wherein substantially all of the decrease in water content is accomplished by evaporation, thereby producing a masticated masterbatch; and E) subjecting the masticated masterbatch to at least an additional 0.3 MJ/kg of mechanical energy while further reducing the water content.
-
公开(公告)号:AT552044T
公开(公告)日:2012-04-15
申请号:AT04028180
申请日:1998-09-28
Applicant: CABOT CORP
Inventor: MABRY MELINDA ANN , PODOBNIK IVAN ZLATKO , MORGAN ALLAN CLARK , TOKITA NOBORU , WANG TING , SHELL JAMES A , CHUNG BIN
IPC: B01F5/02 , B29B7/76 , B29B15/04 , B60C1/00 , C08C1/14 , C08C1/15 , C08J3/215 , C08J3/22 , C08K3/04 , C08K3/36 , C08L21/00
Abstract: Elastomer composite blends are produced by novel wet/dry mixing methods and apparatus. In the wet mixing step or stage, fluid streams of particulate filler and elastomer latex are fed to the mixing zone of a coagulum reactor to form a mixture in semi-confined flow continuously from the mixing zone through a coagulum zone to a discharge end of the reactor. The particulate filler fluid is fed under high pressure to the mixing zone, such as to form a jet stream to entrain elastomer latex fluid sufficiently energetically to substantially completely coagulate the elastomer with the particulate filler prior to the discharge end. Highly efficient and effective elastomer coagulation is achieved without the need for a coagulation step involving exposure to acid or salt solution or the like. Elastomer composites are produced. Such elastomer composites may be cured or uncured, and combine material properties, such as choice of filler, elastomer, level of filler loading, and macro-dispersion, nor previously achieved. The coagulum produced by such wet mixing step, with or without intermediate processing steps, is then mixed with additional elastomer in a dry mixing step or stage to form elastomer composite blends. The additional elastomer to the coagulum may be the same as or different from the elastomer(s) used in the wet mixing step.
-
公开(公告)号:AU2010296002A1
公开(公告)日:2012-03-29
申请号:AU2010296002
申请日:2010-09-16
Applicant: CABOT CORP
Inventor: WANG TING , WANG MENG-JIAO , MARIADASS BERNARD , GOVINDAN THIRUNAVUC KARASU , DAS THIRUHELVANATHAN ANTHONY , LEE BOON KWANG , ZHANG XUAN
Abstract: A method of producing a coagulated latex composite. A coagulating mixture of a first elastomer latex and a particulate filler slurry is flowed along a conduit, and a second elastomer latex is introduced into the flow of the coagulating mixture.
-
-
-
-
-
-
-
-
-