公开(公告)号:CA2636302A1
公开(公告)日:2007-08-23
申请号:CA2636302
申请日:2007-02-14
Applicant: TORAY INDUSTRIES
Inventor: MATSUMOTO TAISEI , NAKAMURA HIROKADO , KIMURA MASAHIRO
Abstract: The present invention provides a polyether-polylactic acid composition which is excellent in storage stability, melt stability and hue. The polyether-polylactic acid composition of the present invention is a compound comprising a polyether and polylactic acid component and characterized in that a residual lactide content is 0.3 wt% or less, and an acid value is 50 equivalent/t or less.
-
公开(公告)号:MY124348A
公开(公告)日:2006-06-30
申请号:MYPI9905026
申请日:1999-11-18
Applicant: TORAY INDUSTRIES
Inventor: MATSUI RYOUSUKE , KIMURA MASAHIRO , TAKAHASHI KOHZO
Abstract: A FORMABLE BIAXIALLY-ORIENTED POLYESTER FILM HAS A DIFFERENCE OF NOT MORE THAN ABOUT 0.007 BETWEEN THE MAXIMUM AND MINIMUM VALUES OF FACE ORIENTATION COEFFICIENT AS DETERMINED IN A 20 SQUARE CM REGION OF THE FILM, AND AN AVERAGE FACE ORIENTATION COEFFICIENT OF ABOUT 0.11 TO 0.15 AS DETERMINED IN SUCH FILM REGION.
-
公开(公告)号:DE69628522D1
公开(公告)日:2003-07-10
申请号:DE69628522
申请日:1996-10-02
Applicant: TORAY INDUSTRIES
Inventor: KIMURA MASAHIRO , TAKAHASHI KOHZO , ABE KOICHI
Abstract: A biaxially oriented polyester film for use in producing containers comprises (1) a polyester containing 93 mol% or more of ethylene terephthalate units as a component, having a breaking elongation in the machine direction (S MD) and a breaking elongation in the transverse direction (S TD) satisfying ÄFormula 1Ü and ÄFormula 2Ü, or (2) a polyester containing 93 mol% or more of ethylene terephthalate units as a component and having a face orientation coefficient of from 0.01 to less than 0.13, or (3) a polyester containing 95 mol% or more of ethylene terephthalate units as a component and having an amorphous Young's modulus of from 120 to 220 kg/mm . Since the film has excellent formability, impact resistance and taste property, it is especially suitable as a film on both the inner and outer faces of metallic cans. S MD: Breaking elongation in the machine direction S TD: Breaking elongation in the transverse direction
-
公开(公告)号:DE69719143D1
公开(公告)日:2003-03-27
申请号:DE69719143
申请日:1997-05-15
Applicant: TORAY INDUSTRIES
Inventor: KIMURA MASAHIRO , TAKAHASHI KOHZO , KOJIMA HIROJI , ABE KOICHI
Abstract: A biaxially stretched polyester film for forming a container, characterized by being formed of a polyester substantially consisting of an ethylene terephthalate unit and an ethylene naphthalate unit, the refractive index in the direction of thickness of the film being 1.5 or greater. This film is not only excellent in the formability during formation into cans or the like, but has excellent properties in taste property, particularly, the taste property after the retorting, and may be suitably used for containers produced by forming process and, particularly, for metallic cans.
-
公开(公告)号:DE69621858D1
公开(公告)日:2002-07-25
申请号:DE69621858
申请日:1996-03-08
Applicant: TORAY INDUSTRIES
Inventor: TAKAHASHI KOHZO , KIMURA MASAHIRO , MIMURA TAKASHI
IPC: C08J7/04 , C09D167/00
Abstract: A film having a good adhesive property comprises a base film and a coated layer formed on at least one surface of the base film. The coated layer has carboxylic acid and primary groups such that, at a surface thereof, the concentration of the carboxylic acid groups is not less than 0.005 and the concentration of the primary amine groups is not less than 0.0015.
-
公开(公告)号:CA2290049A1
公开(公告)日:2000-05-20
申请号:CA2290049
申请日:1999-11-18
Applicant: TORAY INDUSTRIES
Inventor: MATSUI RYOUSUKE , KIMURA MASAHIRO , TAKAHASHI KOHZO
Abstract: A formable biaxially-oriented polyester film has a difference of not more than about 0.007 between the maximum and minimum values of face orientation coefficient as determined in a 20 square cm region of the film, and an average face orientation coefficient of about 0.11 to 0.15 as determined in such film region.
-
公开(公告)号:HK1010704A1
公开(公告)日:1999-06-25
申请号:HK98111431
申请日:1998-10-21
Applicant: TORAY INDUSTRIES
Inventor: KIMURA MASAHIRO , TAKAHASHI KOHZO , KASHIWAKURA NAOTAKE , TSUNASIMA KENJI , KUROME HIROKAZU
Abstract: A biaxially oriented, laminated polyester film having a Young's modulus of 10-250 kg/mm and comprising a layer of polyester A having a glass transition point of 50 DEG C or below and sandwiched between layers of polyester B. This film not only has characteristics that the conventional polyester films do not possess, such as impact resistance, resistance to pinhole generation and low-temperature performance, but also is excellent in flexibility.
-
公开(公告)号:DE69320565T2
公开(公告)日:1999-04-08
申请号:DE69320565
申请日:1993-02-24
Applicant: TORAY INDUSTRIES
Inventor: KIMURA MASAHIRO , TAKAHASHI KOHZO TORAY HOKUENRY , KASHIWAKURA NAOTAKE - , TSUNASIMA KENJI , KUROME HIROKAZU TORAY SONOYAMA
Abstract: A biaxially oriented, laminated polyester film having a Young's modulus of 10-250 kg/mm and comprising a layer of polyester A having a glass transition point of 50 DEG C or below and sandwiched between layers of polyester B. This film not only has characteristics that the conventional polyester films do not possess, such as impact resistance, resistance to pinhole generation and low-temperature performance, but also is excellent in flexibility.
-
公开(公告)号:DE69502135D1
公开(公告)日:1998-05-28
申请号:DE69502135
申请日:1995-06-23
Applicant: TORAY INDUSTRIES
Inventor: KIMURA MASAHIRO , IMAI SHIRO
Abstract: A polyester film for thermal lamination comprises at least a layer A, which layer A comprises a polyester A having a melting point of 140 to 245 DEG C and comprising at least 70 mol%, of the polyester A, of ethylene terephthalate and/or ethylene isophthalate units, and a thermoplastic elastomer mixed at a ratio by weight of, polyester A : thermoplastic elastomer, of 81 : 19 to 98 : 2.
-
公开(公告)号:CA2199334A1
公开(公告)日:1998-03-09
申请号:CA2199334
申请日:1997-03-06
Applicant: TORAY INDUSTRIES
Inventor: TAKAHASHI KOHZO , KIMURA MASAHIRO , ABE KOICHI , SHIMIZU YUZO , SUZUKI MASARU
Abstract: A biaxially oriented polyester film is suitable for laminating onto a metallic sheet so as to provide a laminate capable of being formed into a can. The polyester film comprises at least one of: (1) a polyester having a melting point of 246 to 280.degree.C and being such that when the laminate is formed into a can, then at a neck of the can the film provides an inner 1 to 3 .mu.m portion (a) close to the metallic sheet and an outer 1- 3 .mu.m portion (b) remote from the metallic sheet, which said portions (a) and (b) have respective average orientation intensity ratios, as measured by Raman spectrometry, of 6 or less and 8 or more; and (2) a polyester layer (A) of a polyester having at least 93 mol% thereof of units derived from ethylene terephthalate and/or ethylene naphthalate and a polyester layer (B) of a polyester containing an ionomer and which film has a face orientation factor of 0.10 to 0.15.
-
-
-
-
-
-
-
-
-