IPC: C23C22/07 , C23C22/40 , C10M173/00
CPC classification number: B21C43/02 , B21C9/005 , B21C9/02 , C10M169/04 , C10M173/02 , C10M2201/041 , C10M2201/0413 , C10M2201/066 , C10M2201/0663 , C10M2201/08 , C10M2201/0803 , C10M2201/084 , C10M2201/085 , C10M2201/0853 , C10M2201/087 , C10M2201/0873 , C10M2201/102 , C10M2201/1023 , C10M2205/00 , C10M2205/003 , C10M2207/125 , C10M2207/1253 , C10M2213/062 , C10M2213/0623 , C10N2240/402 , C10N2240/50 , C10N2250/08 , C10N2250/121 , C10N2280/00 , C23C22/06 , C23C22/60 , C23C22/68
Abstract: 本发明提供一种方法,其中,采用选自喷丸处理、喷砂清理、弯曲、阳极酸洗涤和阴极酸洗涤的至少1种清洁化处理方法,对钢、不锈钢、铝等金属线材的表面施行20秒以下清洁化处理后,接触含有选自磷酸盐、硫酸盐、硼酸盐、硅酸盐、钼酸盐和钨酸盐的至少1种无机盐、和选自金属皂、蜡、聚四氟乙烯、二硫化钼和石墨的至少1种润滑剂的水系润滑被膜形成处理液5秒钟以下,立即干燥,以连续直列方式在上述线材表面形成附着量0.5-20g/m2的润滑被膜。采用上述方法能够在短时间内制造具有优良润滑性的塑性加工用金属材料。
-
公开(公告)号:CN1543489A
公开(公告)日:2004-11-03
申请号:CN02816023.1
申请日:2002-07-22
Applicant: 日本帕卡濑精株式会社
IPC: C09D1/02 , B05D7/14 , C10M169/04
CPC classification number: C09D5/08 , B05D2202/00 , C04B28/26 , C04B2111/00215 , C04B2111/00525 , C09D1/02 , C09D1/04 , C10M173/00 , C10M173/02 , C10M2201/102 , C10M2201/1023 , C10M2201/1026 , C10M2201/1036 , C10M2201/18 , C10M2203/1006 , C10M2205/143 , C10M2205/163 , C10M2205/183 , C10M2207/126 , C10M2207/401 , C10M2213/0623 , C10M2215/02 , C10M2215/04 , C10N2210/01 , C10N2210/02 , C10N2210/03 , C10N2230/12 , C10N2240/40 , C10N2250/10 , C10N2250/121 , C10N2250/14 , C04B24/08 , C04B2103/44 , C04B24/005 , C04B24/26 , C04B24/383 , C04B14/062 , C04B14/10 , C04B24/36 , C04B24/00
Abstract: 一种在水中配合了式M2O·nSiO2(式中,n表示2~9的数,M为Na、K、Li和NR4(式中各R独立地表示氢原子或烷基)中的至少1种)表示的硅酸碱的保护涂膜处理剂。通过在该保护涂膜处理剂中配合润滑成分,可赋予涂膜优异的自润滑性能。本发明的保护涂膜处理剂附着在金属材料表面上后,用干燥的简便方法便可形成具有与化学转化法一样或更佳的优异耐烧结性、优异防锈性的涂膜。本发明进一步涉及具有用该保护涂膜处理剂形成的保护涂膜的金属材料,和采用该保护涂膜处理剂的保护涂膜形成方法。
-
公开(公告)号:CN1406164A
公开(公告)日:2003-03-26
申请号:CN01805881.7
申请日:2001-03-05
Applicant: 耶达研究与开发有限公司 , 霍隆科技学院
IPC: B22F3/11 , C22C32/00 , C10M171/06 , C10M103/06 , C10N20/06
CPC classification number: C10M103/06 , B22F3/114 , C10M103/00 , C10M103/04 , C10M171/06 , C10M2201/003 , C10M2201/0403 , C10M2201/0433 , C10M2201/05 , C10M2201/053 , C10M2201/0603 , C10M2201/0613 , C10M2201/0623 , C10M2201/065 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/10 , C10M2201/1006 , C10M2201/1023 , C10M2201/1033 , C10M2201/1053 , C10M2201/123 , C10M2203/10 , C10N2210/06 , C22C32/0089 , Y10S977/734 , Y10T428/12028 , Y10T428/12528
Abstract: 本发明提供一种新型复合材料,该复合材料包含由金属、金属合金或者半导体材料制成的多孔基体以及一种金属硫族化合物或者这类化合物的混合物的空心类富勒烯纳米粒子。所述复合材料的特征在于其孔隙率为约10-40%。所述复合材料中空心纳米粒子的量为1-20重量%。
-
公开(公告)号:CN1063479C
公开(公告)日:2001-03-21
申请号:CN96106237.1
申请日:1996-05-16
Applicant: 梯姆考而有限公司
IPC: C10M103/06
CPC classification number: C10M169/044 , C10M103/00 , C10M103/02 , C10M103/06 , C10M125/24 , C10M125/26 , C10M145/14 , C10M145/40 , C10M2201/003 , C10M2201/02 , C10M2201/0403 , C10M2201/041 , C10M2201/0413 , C10M2201/042 , C10M2201/0423 , C10M2201/0433 , C10M2201/0603 , C10M2201/0613 , C10M2201/0623 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/085 , C10M2201/0853 , C10M2201/0863 , C10M2201/087 , C10M2201/0873 , C10M2201/10 , C10M2201/1006 , C10M2201/102 , C10M2201/1023 , C10M2201/1033 , C10M2201/105 , C10M2201/1053 , C10M2201/12 , C10M2201/123 , C10M2209/084 , C10M2209/12 , C10N2240/402 , C10N2240/403 , C10N2240/404 , C10N2240/405 , C10N2240/406 , C10N2240/407 , C10N2240/408 , C10N2240/409
Abstract: 本发明提供了一种适用于表面温度为800-1300℃的工件的润滑剂组合物。
-
公开(公告)号:CN87106375A
公开(公告)日:1988-04-06
申请号:CN87106375
申请日:1987-09-14
Applicant: 隆察股份公司
Inventor: 汉斯·鲁道夫·施陶布 , 雅奎斯·佩列安特
IPC: C10M145/02 , C10N40/22
CPC classification number: C10M111/04 , C10M103/04 , C10M103/06 , C10M107/12 , C10M107/14 , C10M125/02 , C10M125/18 , C10M125/22 , C10M143/10 , C10M143/12 , C10M173/02 , C10M2201/00 , C10M2201/02 , C10M2201/041 , C10M2201/042 , C10M2201/053 , C10M2201/0603 , C10M2201/061 , C10M2201/0613 , C10M2201/0623 , C10M2201/065 , C10M2201/0653 , C10M2201/066 , C10M2201/0663 , C10M2201/08 , C10M2201/0803 , C10M2201/081 , C10M2201/082 , C10M2201/084 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/1006 , C10M2201/102 , C10M2201/1023 , C10M2201/103 , C10M2201/1033 , C10M2201/1053 , C10M2201/123 , C10M2201/14 , C10M2201/16 , C10M2201/18 , C10M2203/10 , C10M2205/04 , C10M2205/043 , C10M2205/06 , C10M2205/063 , C10M2209/04 , C10M2209/06 , C10M2209/062 , C10M2209/084 , C10M2209/104 , C10M2209/12 , C10N2240/402 , C10N2240/403 , C10N2240/404 , C10N2240/405 , C10N2240/406 , C10N2240/407 , C10N2240/408 , C10N2240/409 , C10N2250/02 , C10N2250/121
Abstract: 一种高温下钢无切屑成型时用的,特别是在所谓多管轧机中生产无缝管时所用的润滑剂,此时润滑剂必须附着在工具上防水。这可由除了固体润滑剂和增稠剂之外还含有由一系列羧酸化的苯乙烯-二丁烯乳胶组成的粘结剂的润油剂来达到。
-
公开(公告)号:CN85103499A
公开(公告)日:1986-10-29
申请号:CN85103499
申请日:1985-04-29
Applicant: 隆察股份公司
Inventor: 雅奎斯·佩列安特 , 海斯·鲁道夫·斯道布 , 阿伦·克隆
IPC: C10M145/00 , C10M161/00 , C10M173/02 , C10N40/20
CPC classification number: C10M103/00 , C10M103/02 , C10M103/06 , C10M2201/003 , C10M2201/02 , C10M2201/0403 , C10M2201/041 , C10M2201/0413 , C10M2201/042 , C10M2201/0423 , C10M2201/0433 , C10M2201/0603 , C10M2201/0613 , C10M2201/0623 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/1006 , C10M2201/102 , C10M2201/1023 , C10M2201/103 , C10M2201/1033 , C10M2201/105 , C10M2201/1053 , C10M2201/123 , C10M2205/00 , C10M2205/022 , C10M2205/024 , C10M2205/026 , C10M2205/04 , C10M2205/06 , C10M2205/14 , C10M2209/04 , C10M2209/06 , C10M2209/062 , C10M2209/08 , C10M2209/084 , C10M2209/086 , C10M2209/12 , C10M2217/028 , C10M2217/06 , C10N2240/402 , C10N2240/403 , C10N2240/404 , C10N2240/405 , C10N2240/406 , C10N2240/407 , C10N2240/408 , C10N2240/409 , C10N2250/121
Abstract: 金属无切屑热加工用的高温润滑剂,优先采用的是水悬浮液状的,为了避免固体物质在水悬浮液中凝聚和保持能经受温度变化的均匀的润滑膜,高温润滑剂中除了含有固体润滑剂外,还含有可完全分解的有机物。由聚磷酸盐、硼化物和碱金属硅酸盐组成的无机添加剂以及有机稳定剂。
-
公开(公告)号:KR1020080033386A
公开(公告)日:2008-04-16
申请号:KR1020087003327
申请日:2006-07-11
Applicant: 어드밴스드 루브리케이션 테크놀로지, 아이엔씨.
Inventor: 올리제스,윌리엄,이. , 로버츠,플로이드 , 아르넬,제리
IPC: C10M107/02 , C10M139/00
CPC classification number: C10M169/04 , C09D5/086 , C10M2201/087 , C10M2201/1023 , C10M2205/043 , C10M2207/046 , C10M2207/289 , C10M2209/0845 , C10M2215/042 , C10M2215/1006 , C10M2217/0453 , C10M2229/025 , C10N2230/06 , C10N2230/12 , C10N2250/121 , C10N2270/00 , C10M2205/063
Abstract: This invention relates to a structural coating comprising a polymeric resin, a borate-based additive, and a dynamic stabilization material. The borate-based additive provides corrosion protection through electrochemical binding of active surface corrosive sites, lubrication enhancement through the creation and re-supply to a surface where friction contact occasionally occurs of a weak slip lane crystalline material which may be a locally formed product utilizing local atmospheric humidity, and a material for reaction with an initiator to provide for freezing point depression during coating application. The dynamic stabilization material creates a balance of stabilized material for supply of corrosion protection product, lubrication reduction product, and freezing point depression product.
Abstract translation: 本发明涉及包含聚合物树脂,硼酸盐基添加剂和动态稳定材料的结构涂层。 硼酸盐添加剂通过电化学结合活性表面腐蚀性位点提供腐蚀保护,通过产生和再供给到偶尔发生摩擦接触的表面的润滑增强,弱滑道结晶材料可能是局部形成的产品,其利用局部 大气湿度,以及用于与引发剂反应的材料,以在涂布施用期间提供凝固点抑制。 动态稳定材料产生稳定材料的平衡,供应防腐蚀产品,润滑减少产品和凝固点抑制产品。
-
公开(公告)号:KR1019930011934B1
公开(公告)日:1993-12-22
申请号:KR1019910005008
申请日:1991-03-29
Applicant: 하나노쇼지가부시키가이샤
Inventor: 하나노다까시
IPC: C10M113/16
CPC classification number: B22D17/2038 , C10M101/02 , C10M101/025 , C10M101/04 , C10M103/00 , C10M103/02 , C10M103/06 , C10M105/24 , C10M105/32 , C10M107/04 , C10M107/06 , C10M107/12 , C10M107/28 , C10M107/30 , C10M107/32 , C10M107/34 , C10M107/36 , C10M107/44 , C10M107/50 , C10M111/00 , C10M111/02 , C10M111/04 , C10M2201/041 , C10M2201/0613 , C10M2201/0623 , C10M2201/066 , C10M2201/1023 , C10M2201/1033 , C10M2203/10 , C10M2205/022 , C10M2205/04 , C10M2205/16 , C10M2205/18 , C10M2207/28 , C10M2207/40 , C10M2209/084 , C10M2209/10 , C10M2209/102 , C10M2209/103 , C10M2209/12 , C10M2217/045 , C10M2229/02 , C10N2220/082 , C10N2220/084 , C10N2240/402 , C10N2250/08 , C10M2205/024
Abstract: The powder lubricant for plunger device of this invention is a mixture of a powdered or granulated lubricant base material used for a lubricant in a solid form, with an organic compound giving an adhesion ability to the lubricant base material. The most outstanding feature of this invention is that the lubricant base material has the powdered or granulated form. Effect of this invention are that occurrence of defects inside products can be positively avoided, dangers such as fire etc. and environmental pollution can be prevented, and sliding of plunger can be made smooth to improve the workability.
-
公开(公告)号:JP6244384B2
公开(公告)日:2017-12-06
申请号:JP2015563081
申请日:2014-05-26
Inventor: ジーモン ミラー=ユップ , ギュンター シューベルト
IPC: C10M169/04 , C09D123/04 , C09D123/10 , C09D125/04 , C09D123/22 , C09D133/12 , C09D7/12 , B32B27/18 , B32B15/20 , B05D7/14 , B05D7/24 , C10N10/12 , C10N30/00 , C10N40/24 , B32B15/08
CPC classification number: C09D123/12 , B05D3/007 , B05D7/16 , B21D31/00 , C09D5/008 , C09D7/61 , C09D7/65 , C10M111/04 , C10M169/04 , C08K2003/2224 , C08K2003/385 , C08K3/04 , C08K3/22 , C08K3/34 , C08K3/346 , C08K3/38 , C10M2201/041 , C10M2201/0413 , C10M2201/061 , C10M2201/0613 , C10M2201/066 , C10M2201/0663 , C10M2201/087 , C10M2201/0873 , C10M2201/102 , C10M2201/1023 , C10M2201/103 , C10M2201/1033 , C10M2205/0225 , C10M2205/0245 , C10M2205/0265 , C10M2205/043 , C10M2209/084 , C10M2209/1033 , C10M2213/062 , C10N2230/06 , C10N2250/121 , C10N2250/14
-
公开(公告)号:JP2012180524A
公开(公告)日:2012-09-20
申请号:JP2012097945
申请日:2012-04-23
Applicant: Rolls-Royce Corp , ロールス−ロイス・コーポレーション
Inventor: NAIK SUBHASH K , KLOTZ JAMES M , BARBER MICHAEL J
IPC: C10M173/02 , C08K3/16 , C09D183/04 , C10M103/06 , C10M111/04 , C10M129/08 , C10M155/02 , C10M173/00 , C10N10/04 , C10N30/08 , C10N40/00 , C10N40/02
CPC classification number: C10M111/04 , C08K3/16 , C09D183/04 , C10M103/06 , C10M107/50 , C10M125/18 , C10M127/06 , C10M129/50 , C10M155/02 , C10M173/00 , C10M173/02 , C10M2201/02 , C10M2201/0603 , C10M2201/0613 , C10M2201/0623 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/081 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/1006 , C10M2201/1023 , C10M2201/1033 , C10M2201/1053 , C10M2201/123 , C10M2203/06 , C10M2207/022 , C10M2207/027 , C10M2207/141 , C10M2209/023 , C10M2229/02 , C10M2229/025 , C10M2229/04 , C10M2229/0405 , C10M2229/041 , C10M2229/0415 , C10M2229/042 , C10M2229/0425 , C10M2229/043 , C10M2229/0435 , C10M2229/044 , C10M2229/0445 , C10M2229/045 , C10M2229/0455 , C10M2229/046 , C10M2229/0465 , C10M2229/047 , C10M2229/0475 , C10M2229/048 , C10M2229/0485 , C10M2229/05 , C10M2229/0505 , C10M2229/051 , C10M2229/0515 , C10M2229/052 , C10M2229/0525 , C10M2229/053 , C10M2229/0535 , C10M2229/054 , C10M2229/0545 , C10N2210/02 , C10N2210/03 , C10N2230/08 , C10N2250/04 , C10N2250/14 , C10N2250/141 , Y10T428/31663
Abstract: PROBLEM TO BE SOLVED: To provide dry film lubricant coatings by using a silicone resin binder, either as an aqueous emulsion or in a solvent-based system, to fix an alkaline earth metal fluoride to a substrate.SOLUTION: The compositions used to apply the coatings may also include relatively minor amounts of xylene, ammonium benzoate, a wetting agent, and/or a porosity-inducing agent, although none of those additives remains in the cured coating. Multi-layer dry film lubricant coatings are also disclosed, with the multi-layer coating having a basecoat layer as described above, and a topcoat layer made of a layer-lattice solid such as graphite or molybdenum disulfide, and a silicone resin, aluminum phosphate or an alkali metal silicate binder.