방수성, 투습성 및 항균성을 가지는 피혁 및 그 제조방법.
    51.
    发明授权
    방수성, 투습성 및 항균성을 가지는 피혁 및 그 제조방법. 失效
    방성성,투습성및항균성을가지는피혁및및그제조방법。

    公开(公告)号:KR100389515B1

    公开(公告)日:2003-06-25

    申请号:KR1020000061790

    申请日:2000-10-20

    Abstract: PURPOSE: Provided are a waterproof, water-permeative and antibacterial leather with functionality and a method for producing the leather. CONSTITUTION: The method comprises (i) immersing hide subjected to soaking, liming, deliming, and bating processes in formic acid so as the pH of the hide to be 2.0-3.5, and treating the hide with 450-1,800 ppm(based on weight of raw leather) of antimicrobial of CMK type for 1 hour; (ii) treating the material resulting from the step(i) with chromium to mineralize an animal origin material on the fiber, and treating the resulting material with 450-1,800 ppm(based on weight of raw leather) of antimicrobial of TCMTB type for 1 hour; and (iii) neutralizing the material resulting from the step (ii) to increase a pH of the material to 5.0-6.5, and treating the material with 450-1,800 ppm(based on weight of active ingredients) of antimicrobial of OITZ type for 1 hour to impart an antibiosis to the material.

    Abstract translation: 用途:提供一种具有功能性的防水,透水和抗菌皮革和一种生产该皮革的方法。 构成:该方法包括(ⅰ)将经过浸泡,浸灰,脱灰和软化过程的皮浸泡在甲酸中,使生皮的pH值为2.0-3.5,并用450-1,800ppm(按重量计) 的生皮革)CMK型抗菌剂1小时; (ii)用铬处理步骤(i)产生的材料以使纤维上的动物源材料矿化,并且用450-1,800ppm(基于生皮重量)生产的TCMTB型抗菌剂1 小时; 和(iii)中和步骤(ii)产生的物质,使物质的pH值升高到5.0-6.5,并用450-1,800ppm(基于活性成分的重量计)OITZ型抗微生物剂1 小时以赋予材料抗菌作用。

    경량성 피혁의 제조 방법.
    52.
    发明授权
    경량성 피혁의 제조 방법. 失效
    轻量皮革制造方法

    公开(公告)号:KR100318020B1

    公开(公告)日:2001-12-22

    申请号:KR1019990018346

    申请日:1999-05-17

    Abstract: 본발명은피혁제조업체에서일반적으로통용되고있는천연피혁의단점인무거움을 30∼50% 정도로감소시켜신발및 의류그리고가방용피혁소재인스프릿레더를제조하는제혁공정에응용한다용도경량성피혁의제조방법에관한것이다. 즉, 기존의광물성피혁유제및 재유제약품, 그리고천연유지를원료로하여합성된가지제등 피혁제조공정상무거운느낌을소유하고있는제혁약품들을지양하고또한기본적인피혁물성은뒤떨어지지않으면서기존복잡한제혁공정을간편하고단순한처방으로개선연구하여합성피혁과유사하게밀도가적으면서착용감, 활동성및 기능성이탁월한경량성피혁의제조방법에관한것이다.

    천연 피혁 유사 소재의 제조 방법 및 그 소재.
    53.
    发明公开
    천연 피혁 유사 소재의 제조 방법 및 그 소재. 有权
    生产皮革材料及其材料

    公开(公告)号:KR1020010081315A

    公开(公告)日:2001-08-29

    申请号:KR1020000007172

    申请日:2000-02-11

    Abstract: PURPOSE: A process for preparing leather like material by using shaving scrap as waste leather generated in the process for the manufacture of leather as raw material without changing basic physical properties and feeling of leather is provided, which reduces environmental pollution and treatment expenses and recycles the resources of waste. CONSTITUTION: The titled leather like material is prepared by the process consisting of: beating waste leather and other industrial wastes for 1 to 120deg.C and neutralizing with 0.1 to 10.0% HCOONa and 0.1 to 10.0% NaHCO3 for 10 to 360 min; treating with 0.1 to 10.0% retanning agent for 10 to 360 min; and treating with 0.1 to 20.0% oil or fat liquor to give lubricity.

    Abstract translation: 目的:提供在不改变皮革基本物理性能和皮革感觉的前提下,以皮革为原料生产过程中产生的刮屑作为废皮,制备皮革样物料的方法,减少环境污染和处理费用,并回收利用 浪费资源 规定:标签皮革样材料通过以下工艺制备:将废皮革和其他工业废料打碎1至120℃,并用0.1至10.0%HCOONa和0.1至10.0%NaHCO 3中和10至360分钟; 用0.1至10.0%的复鞣剂处理10至360分钟; 并用0.1至20.0%的油或脂肪液处理以提供润滑性。

    무공해성스플릿레더의제조방법

    公开(公告)号:KR1019980080537A

    公开(公告)日:1998-11-25

    申请号:KR1019980009880

    申请日:1998-03-16

    Abstract: 본 발명은 비크롬 유제방법을 통하여 크롬을 전혀 사용하지 않고 100℃ 근처의 열적 수축율을 지닌 무공해성 스플릿 레더를 제조하는 방법을 제공하기 위한 것이다. 상기 스플릿 레더는 탈모 처리된 하부층의 나피를 탈회 및 효해공정을 거쳐 무기산으로 드럼내 침산 pH를 약 1.0∼6.0 정도로 조정하는 과정과, 비크롬 유제물질를 선택적으로 단독 또는 혼합 유제처리하기 위하여 약 1∼20% 정도로 한번 또는 여러번 나누어 침산처리된 드럼내에 투입하는 과정과, 소정인 pH에서 유제물질과 침산처리된 나피간에 결합 및 침투력을 효율적으로 수행하기 위하여 분당 6∼16회 속도로 드럼내 연속적인 유제작업을 수행하는 과정과, 상기 유제작업에 의해 유제 처리된 가죽을 통과시켜 적정의 두께로 조절하여 비크롬 유제 처리된 스플릿 레더를 제조하는 과정과, 상기 비크롬처리된 스플릿 레더를 염색 드럼에 재차 투입하여 약 1∼16% 정도의 염료 및 피혁관련 약품을 사용하여 각 품목별 처방에 따른 제혁과정을 거쳐 제조된다.