Abstract:
The present invention relates to a Ce-La complex oxide desulfurizing agent and a manufacturing method thereof, and specifically, to a Ce-La complex oxide desulfurizing agent and a manufacturing method characterized by mixing La (lanthanum) that is an oxidation promoting substance into a Ce (cerium) based desulfurizing agent using a coprecipitation and a sintering process. By using the Ce-La complex oxide desulfurizing agent of the present invention, a desulfurizing process having high durability at high temperatures and high efficiency in the oxidizing atmosphere can be realized.
Abstract:
본 발명은 산화탈황공정에서 생성된 황산화물 함유 고비점 유분으로부터 황산화물을 분리 제거하는 방법으로서, (S1) 황산화물 함유 고비점 유분에 추출 용매를 공급하여 미반응 산화제 및 산화반응 부산물을 제거하는 추출 단계로서, 상기 추출 용매가 메탄올 또는 아세토나이트릴인 것을 특징으로 하는 추출 단계; (S2) 상기 추출 용매를 증류에 의해 제거하는 추출 용매 제거 단계; 및 (S3) 흡착제를 사용하여 황산화물 함유 고비점 유분 내 황산화물을 흡착 분리하는 흡착 단계를 포함하는 황산화물 함유 고비점 유분으로부터 황산화물을 분리 제거하는 방법에 관한 것이다. 본 발명에 따라, 고비점 유분에 특화된 황산화물 분리 공정에서 메탄올 또는 아세토나이트릴을 추출 용매로 사용한 추출 단계 및 추출 용매 제거 단계를 흡착 단계 이전에 수행하면 경제적인 방식으로 황 농도 10 ppm 이하의 고비점 유분을 제조할 수 있다.
Abstract:
본 발명은 본 발명은 원유정제공정에서 발생하는 상압잔사유와 같은 중질유를 유동층접촉분해하여 가솔린, 프로필렌 등을 생산하는 설비의 배가스로부터 에틸렌을 농축하여 회수하기 위한 방법과 장치에 관한 것이다. 본 발명은 유동층접촉분해 배가스(FCC) 중의 에틸렌 순도를 높이고 약흡착성분들의 농도를 낮추어 줌으로써 후단의 에틸렌 치환탈착 공정에서 에틸렌 세정양을 줄이고, 약흡착성분과 탈착제의 증류 분리 조작 시 손실되는 탈착제의 양을 줄일 수 있는 압력변동흡착공정을 이용한 유동층접촉분해 배가스로부터의 에틸렌 회수방법 및 장치를 제공함으로써 중질유의 유동층접촉분해 배가스로부터 에틸렌은 높은 순도 및 저비용으로 회수할 수 있다.
Abstract:
PURPOSE: A desorption material for a continuous sulfur oxide adsorption removal process and a method consecutively removing a sulfur oxide from a hydrocarbon stream using the same are provided to efficiently remove a sulfide from a hydrocarbon stream by maintaining the sulfur oxide adsorption quantity of an adsorption material highly in a continuous process repeating the adsorption and desorption of the sulfur oxide. CONSTITUTION: A desorption material for a continuous sulfur oxide adsorption removal process includes any one selected from a DME (dimethyl ether), a DMC (dimethyl carbonate), and a MTBE (methyl tertiary butyl ether), and a mixture thereof. The desorption material additionally includes hexane or benzene. The desorption is performed at 40~90>=, 1~20barg. The vaporization latent heat of the desorption material is below 500 kJ/kg. The boiling point is 120>= or less which is a sulfide oxidation temperature. A method consecutively removing a sulfur oxide from a hydrocarbon stream includes following steps. A step for absorbing the sulfur oxide from a hydrocarbon stream by using an adsorption material selectively adsorbing the sulfur oxide; a step for reproducing the adsorption material by detaching the adsorbed sulfur oxide with the desorption material; and a step for reusing by separating a desorption material from the detached sulfur oxide and the mixture of the desorption material.
Abstract:
PURPOSE: A manufacturing method of an anisotropy element and a method thereof are provided to implement fine pitch connection by forming a nanostructure or a microstructure with the anisotropy element. CONSTITUTION: After a plate-shaped substrate is annealed, an electro polishing process of the plate-shaped substrate is executed(a-1). The pre-processed substrate is firstly anodized(a-2). An oxide layer of the substrate which is firstly anodized is eliminated in an etching process(a-3). The plate-shaped substrate is secondly anodized(a-4). A plurality of minute through holes is extended by acid treatment(a-5). [Reference numerals] (AA) Surface; (BB) Lateral cross section; (CC) Start; (DD) Pre-treatment; (EE) Firstly anodizing; (FF) Oxide etching; (GG) Secondly anodizing; (HH) Through hole extension; (II) End; (JJ) Step a-1; (KK) Step a-2; (LL) Step a-3; (MM) Step a-4; (NN) Step a-5;