Abstract:
b) an oligomeric or polymeric organic compound having one or more terminal hydroxyl groups and a viscosity at 40° C. of at least about 20 mm2/sec (DIN 51562).
Abstract:
A terpolymer containing propylene, ethylene and 1-hexene obtainable by the step of copolymerizing propylene, ethylene and 1-hexene in the presence of a catalyst system comprising the product obtained by contacting the following components: (a) a solid catalyst component comprising a magnesium halide, a titanium compound having at least a Ti-halogen bond and at least two electron donor compounds one of which being present in an amount from 40 to 90% by mol with respect to the total amount of donors and selected from succinates and the other being selected from 1,3 diethers, (b) an aluminum hydrocarbyl compound, and (c) optionally an external electron donor compound. wherein in the terpolymer (i) the content of 1-hexene derived units ranges from 0.5 to 5.0 wt%; (ii) the content of ethylene derived units is higher than 1.4 t% and fulfils the following relation (1): C �¢ 2
Abstract:
A propylene polymer composition comprising: A) 70-94% wt of a propylene-ethylene copolymer comprising from 2.5 to 5% wt of ethylene derived units; and B) 6-30% wt of a second propylene-ethylene copolymer comprising from 35 to 60% wt of ethylene derived units. Said propylene polymer composition having a MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230° C. and 2.16 kg load) from 0.1 to 5 g/10 min, and an Intrinsic Viscosity of the fraction soluble in xylene [XSIV] at room temperature: from 1 to 4.5 dl/g. Such propylene polymer composition being particularly suitable for the production of injection moulded articles and in particular of films.
Abstract:
A container comprising a propylene, ethylene, 1-butene terpolymer wherein in the terpolymer: i) the content of ethylene derived units ranges from 0.5 wt% to 1.8 wt%; ii) the content of 1-butene derived units ranges from 3.5 wt% to 6.5 wt%; iii) the ratio C2wt%/C4wt% ranges from 0.12 to 0.22; wherein C2wt% is the weight per cent of ethylene derived units and C4wt% is the weight per cent of 1-butene derived units; iv) the total content of ethylene and 1-butene derived units is comprised between 4.2 wt% and 7.5 wt%; v) the melt flow rate,MFR measured according to ISO 1133,230° C, 2.16 kg ranges from 20 to 80 g/10 min; vi) the xylene soluble fraction at 25°C is lower than 7.0 wt%; vii) the melting point is higher than 140°C.
Abstract:
Propylene terpolymers are prepared by polymerizing propylene, ethylene and an alpha-olefin selected from the group of C4-C8 alpha-olefins in the presence of a catalyst system obtained by contacting a solid catalyst component comprising a magnesium halide, a titanium compound having at least a Ti-halogen bond and at least two electron donor compounds one of which being present in an amount from 40 to 90% by mol with respect to the total amount of donors and selected from succinates and the other selected from 1,3 diethers, an aluminum hydrocarbyl compound, and optionally an external electron donor compound.