Abstract:
A cross-linked composition, obtained by cross-linking polyolefin composition comprising, all percentages being by weight: A) from 5 to 38% of a polypropylene component; B) from 35 to 85% of a copolymer of ethylene with propylene, containing from 42 to 70% of ethylene and having solubility in xylene at room temperature greater than 50%; C) from 5 to 45% of a polymer composition comprising a blend of: i) from 20 to 80% of an ethylene copolymer having a Shore A hardness value equal to or lower than 90 points and containing up to 45% of at least one alpha-olefin comonomer, provided that, when propylene is present as comonomer, such copolymer i) has a composition which is different from B); ii) from 20 to 80% of a propylene copolymer having a Shore A hardness value equal to or lower than 90 points and containing up to 40% of at least one alpha-olefin comonomer; wherein the amounts of A), B) and C) are referred to the total weight of A)+B)+C) and the amounts of i) and ii) are referred to the weight of C).
Abstract:
Polyolefin composition with improved sealability comprising from 70 to 95% of one or more copolymers of propylene with one or more comonomers selected from ethylene, a C4-C8 α-olefin and combinations thereof, where the comonomer, or comonomers, content in (A) is from 5 to 25%, and from 5 to 30% by weight of butene-1 (co)polymer (B) having a flexural modulus of 60 MPa or less.
Abstract:
A multilayer film in which at least one layer (A) comprises a copolymer (A1) of propylene with hexene-1 containing from 4 to 10% by weight of hexene-1 and having Melt Flow Rate from 1 to 10 g/10 min.; and at least one layer (B) comprises a copolymer (B1) of ethylene containing up to 20 mol % of CH 2 =CHR α-olefins and having a density from 0.88 to 0.945 g/cm 3 .
Abstract:
A 1-butene propylene ethylene terpolymer having a content of propylene derived units ranging from 0.1-10 % by weight and an ethylene derived units content ranging from 0.1 to 3 % by weight having the following properties: a) distribution of molecular weight Mw/Mn measured by GPC lower than 3.5; b) melting point (DSC) comprised between 60°C and 120°C; c) Content of 1-butene units in the form of isotactic pentads (mmmm) higher than 95%.
Abstract:
Elastoplastic polyolefin composition comprising, in percent by weight: A) 10-50 % of a copolymer of propylene with one or more comonomer(s) selected from ethylene and CH2=CHR alpha-olefins where R is a 2-8 carbon alkyl, which copolymer contains from 1 to 8% of comonomer(s); B) 50-90 % of a copolymer of ethylene and (i) propylene or (ii) CH2=CHR alpha-olefins, where R is a 2-8 carbon alkyl radical,or (iii) a combination thereof, optionally with minor amounts o f a diene, containing from 57 to 80 % of ethylene; wherein the weight ratio B/XS of the content B of copolymer component (B) to the fraction XS soluble in xylene at room temperature, both referred to the total weight of (A) + (B), is of 1.5 or less, and the intrinsic [η] viscosity of the said XS fraction is of 3 dl/g or more.
Abstract:
Propylene-ethylene copolymers are flexible and show a very good balance between softness and mechanical properties in their crude state are obtained by solution polymerization in the presence of Ziegler-Natta catalysts. The said copolymers comprise from 10 to 50%wt of ethylene and are characterized by: product of the comonomer reactivity ratio r1•r2 ≤1.5; absence of 2,1 propylene insertions and tensile strength at break higher than 4 Mpa.
Abstract:
Filled olefin polymer concentrates having improved mechanical properties and scratch resistance comprising: A. about 1.0 to about 40.0 wt% of an oxidized olefin polymer material; B. about 0.5 to about 40.0 of a maleated polypropylene; and C. about 7.0 to about 80.0 wt% of a filler chosen from fiberglass, carbon fibers, graphite fibers, whiskers, metal fibers, aramides, talc, wollastonite, calcium carbonate, mica, glass microspheres, ceramic microspheres, glass wool, rock wool, stainless steel wool, steel wool, gypsum, alumina, alumina-silica, silica, and mixtures thereof; wherein the sum of components A + B+ C is equal to 100 wt%.
Abstract:
A propylene 1-hexene copolymer containing from 5.5 to 9.0% by weight, of 1-hexene derived units having: a) two peaks in the DSC plot having a difference in height ranging from 0 to 5 mW; b) the higher melting temperature, measured by DSC, ranging from 141.0 °C to 151.0 °C; c) Melt Flow Rate (MFR, measured according to ASTM D 1238, 230°C/2.16 kg, from 3.5 to 8.0 g/10 min.
Abstract:
A polyolefin composition made from or containing (A) from 90.0 to 99.0 wt % of a first propylene ethylene copolymer wherein (i) the ethylene derived units is between 1.0 and 8.0 wt %; (ii) the melting temperature ranges from 135 to 155° C.; (iii) the melt flow rate (230° C./5 kg ISO 1133) ranges from 0.2 to 3.5 g/10 min; (iv) the xylene solubles at 25° C. ranges from 10.0 to 4.0 wt %; (v) the polydispersity index ranges from 3.0 to 7.0; and (B) from 1.0 to 10.0 wt % of a second propylene ethylene copolymer (i) containing from 8.0 to 20.0 wt % of ethylene derived units; and having a MFR (measured at 190° C. 2.16 kg of load) between 0.5 and 5.0 g/10 min, wherein (a) the resulting polyolefin composition has a melt flow rate (230° C./5 kg ISO 1133) ranging from 0.2 to 4.0 g/10 min and (b) the sum A+B being 100.