公开(公告)号:DE59000920D1
公开(公告)日:1993-04-01
申请号:DE59000920
申请日:1990-07-19
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , WITTENBERG DIETMAR DR
IPC: C08F283/00 , C08J9/00 , C08J9/20 , C08J9/14 , C08L25/06
Abstract: Expandable molding compositions having high heat distortion resistance and containing from 80 to 99% by weight of a styrene polymer, 1 to 20% by weight of poly-1,4-phenylene sulfide, from 1 to 10% by weight of a C3-C6-hydrocarbon as blowing agent and, if desired, customary additives, are obtained by suspension polymerization of a solution of the polyphenylene sulfide in styrene.
-
公开(公告)号:DE59000743D1
公开(公告)日:1993-02-25
申请号:DE59000743
申请日:1990-04-24
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , ROEHRIG KARL HEINZ
IPC: C08J9/14 , C08J9/20 , C08K3/26 , C08K3/30 , C08K5/02 , C08K5/17 , C08K5/3492 , C08K13/02 , C08L25/02 , C08L25/04
Abstract: Expandable styrene polymers which contain a C3-C6-hydrocarbon as a blowing agent, an organic bromine compound as a flameproofing agent and small amounts of ammonium salt and of an organic amine give, on expansion, foams which have a particularly homogenous foam structure and a good heat insulation effect.
-
公开(公告)号:DE4038042A1
公开(公告)日:1992-06-04
申请号:DE4038042
申请日:1990-11-29
Applicant: BASF AG
Inventor: HINTZ HANS DR , HAHN KLAUS DR , GUHR UWE DR , RIETHUES MICHAEL DR
IPC: C08J9/14 , C08F2/18 , C08F2/44 , C08J9/00 , C08J9/16 , C08L25/00 , C08L25/04 , C08L25/08 , C08L25/10
Abstract: Oil-resistant expandable styrene polymers containing …… a) from 10 to 90% by weight of uncrosslinked polystyrene and/or an uncrosslinked styrene copolymer containing at least 50% by weight of copolymerised styrene, … b) from 10 to 90% by weight of a crosslinked styrene polymer which contains at least 0.1% by weight, but less than 2% by weight, of a copolymerised monomer containing at least two olefinic double bonds, … c) from 1 to 10% by weight, based on the sum of a) and b), of a C3- to C6-hydrocarbon as blowing agent, and optionally … d) conventional additives in effective amounts, … where the mixture of a) and b) has a melt flow index MFI (200 DEG C, 5.0 kp) in accordance with DIN 53 735 of between 1 and 20 [g/10 min].
-
公开(公告)号:DE3936596A1
公开(公告)日:1991-05-08
申请号:DE3936596
申请日:1989-11-03
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , HOENL HANS DR
Abstract: Expandable styrene polymers which contain from 10 to 90% by weight of a crosslinked styrene-diene copolymer containing from 2 to 45% by weight of the diene, and from 1 to 10% by weight of a C3- to C6-hydrocarbon as blowing agent can be processed to give foams which have high resistance to aromatics.
-
公开(公告)号:DE3931862A1
公开(公告)日:1991-04-04
申请号:DE3931862
申请日:1989-09-23
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , WITTENBERG DIETMAR DR
Abstract: Expandable styrene polymers containing a) 80 to 99% by weight of polystyrene, b) 1 to 20% by weight of a styrene-soluble polymer having a softening temperature above 140 DEG C, c) 3 to 10% by weight, based on the sum of a) and b), of a C3- to C6-hydrocarbon as a blowing agent, and optionally d) conventional additives, in which the mixture of components a) and b) has a melt flow index MFI 200/5 of between 15 and 30, are distinguished by high heat distortion resistance and good expandability.
-
公开(公告)号:DE3924868A1
公开(公告)日:1991-01-31
申请号:DE3924868
申请日:1989-07-27
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , WITTENBERG DIETMAR DR
IPC: C08F283/00 , C08J9/00 , C08J9/20 , C08L25/06 , C08J9/14
Abstract: Expandable molding compositions having high heat distortion resistance and containing from 80 to 99% by weight of a styrene polymer, 1 to 20% by weight of poly-1,4-phenylene sulfide, from 1 to 10% by weight of a C3-C6-hydrocarbon as blowing agent and, if desired, customary additives, are obtained by suspension polymerization of a solution of the polyphenylene sulfide in styrene.
-
公开(公告)号:DE3914292A1
公开(公告)日:1990-10-31
申请号:DE3914292
申请日:1989-04-29
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , ROEHRIG KARL HEINZ
IPC: C08J9/14 , C08J9/20 , C08K3/26 , C08K3/30 , C08K5/02 , C08K5/17 , C08K5/3492 , C08K13/02 , C08L25/02 , C08L25/04
Abstract: Expandable styrene polymers which contain a C3-C6-hydrocarbon as a blowing agent, an organic bromine compound as a flameproofing agent and small amounts of ammonium salt and of an organic amine give, on expansion, foams which have a particularly homogenous foam structure and a good heat insulation effect.
-
公开(公告)号:DE3901329A1
公开(公告)日:1990-07-19
申请号:DE3901329
申请日:1989-01-18
Applicant: BASF AG
Inventor: HAHN KLAUS DR , GUHR UWE DR , HINTZ HANS DR , GELLERT ROLAND DR
-
公开(公告)号:DE2860059D1
公开(公告)日:1980-11-13
申请号:DE2860059
申请日:1978-07-12
Applicant: BASF AG
Inventor: KNIESE WILHELM DR , KEPPLER HANS GEORG DR , MOELLER ROLF DR , GUHR UWE DR
-
-
-
-
-
-
-
-