Brazed or soldered joints
    51.
    发明授权
    Brazed or soldered joints 失效
    钎焊或焊接接头

    公开(公告)号:US4333669A

    公开(公告)日:1982-06-08

    申请号:US142919

    申请日:1980-04-23

    Applicant: Roland Eckert

    Inventor: Roland Eckert

    CPC classification number: B23K1/20 B23K37/06 G01K1/00 G01K5/326 B23K2201/04

    Abstract: The brazed or soldered joint is for the connection of a capillary tube, namely of a very thin, flexible metal tube, with a test point or with an expansion chamber of a temperature regulator operating with an expanding fluid. The brazing or soldering location between the connecting socket of the test point and the capillary tube is surrounded with a sheet-metal sleeve being folded from a sheet-metal strip and embraces the connecting socket, but leaves a slot open. The soldering material in the form of a brazing or soldering paste is placed into a window or into a triangular pocket, is firmly held in this position, thus the brazing or soldering may be carried out in a continuous-heating furnace. The sleeve extends far beyond the free end of the connecting socket and is at a distance from the capillary tube, thus it serves meanwhile as a support against the excessive bending of the capillary tube.

    Abstract translation: 钎焊或焊接的接头用于将毛细管即非常薄的柔性金属管与测试点或与膨胀流体一起工作的温度调节器的膨胀室连接。 测试点的连接插座和毛细管之间的钎焊或焊接位置由金属板套管围绕,该金属套筒从金属板条折叠并且包围连接插座,但是留下槽。 将钎焊或焊膏形式的焊接材料放置在窗口或三角形凹槽中,牢固地保持在该位置,因此钎焊或焊接可以在连续加热炉中进行。 套筒延伸远远超过连接插座的自由端,并且与毛细管有一段距离,因此它同时用作抵抗毛细管过度弯曲的支撑。

    Method for the manufacture of axial sealing rings
    52.
    发明授权
    Method for the manufacture of axial sealing rings 失效
    制造轴向密封圈的方法

    公开(公告)号:US4314660A

    公开(公告)日:1982-02-09

    申请号:US105529

    申请日:1979-12-20

    Applicant: Teunis Visser

    Inventor: Teunis Visser

    CPC classification number: B23K1/0008 B23K2201/04 Y10S277/922

    Abstract: The invention relates to a method of manufacturing large diameter axial sealing rings from hard-metal blocks which are placed in an annular groove said blocks being secured within said groove by filling said groove with liquid solder and circumferentially pressing the radial end faces of the blocks within said liquid solder filled groove against each other by means of radially acting clamp bolts.

    Abstract translation: 本发明涉及一种从硬金属块制造大​​直径轴向密封环的方法,它们放置在环形凹槽中,所述块通过用液体焊料填充所述凹槽并周向地将块的径向端面周向地按压而固定在所述凹槽内 所述液体焊料填充槽通过径向作用的夹紧螺栓相互抵靠。

    接合方法
    58.
    发明专利

    公开(公告)号:TW200927345A

    公开(公告)日:2009-07-01

    申请号:TW097149333

    申请日:2008-12-18

    IPC: B23K

    CPC classification number: B23K20/126 B23K20/124 B23K2201/04 B23K2203/10

    Abstract: 提供一種接合方法,使一對金屬構件彼此的平接部容易接合之同時,可提高接合部分的氣密性及水密性。本發明的接合方法在成為金屬構件的平板14與角構件R4平接而形成的構造體(被接合金屬構件N)中,使上述金屬構件彼此平接的平接部J8的接合方法中,進行對平接部J8從構造體的外面A側進行摩擦攪拌的摩擦攪拌工程之後,對平接部J8從內面B側進行熔接的熔接工程。

    Abstract in simplified Chinese: 提供一种接合方法,使一对金属构件彼此的平接部容易接合之同时,可提高接合部分的气密性及水密性。本发明的接合方法在成为金属构件的平板14与角构件R4平接而形成的构造体(被接合金属构件N)中,使上述金属构件彼此平接的平接部J8的接合方法中,进行对平接部J8从构造体的外面A侧进行摩擦搅拌的摩擦搅拌工程之后,对平接部J8从内面B侧进行熔接的熔接工程。

    可調式筒夾、與螺柱焊接裝置組合之可調式筒夾
    60.
    发明专利
    可調式筒夾、與螺柱焊接裝置組合之可調式筒夾 失效
    可调式筒夹、与螺柱焊接设备组合之可调式筒夹

    公开(公告)号:TW360577B

    公开(公告)日:1999-06-11

    申请号:TW086111128

    申请日:1997-08-04

    IPC: B23K

    CPC classification number: B23K11/0053 B23K9/201 B23K2201/04

    Abstract: 一種用於螺柱焊接之新穎可調式筒夾,其採用複數個充有電流之夾顎以穩固地夾持具有不同形狀、尺寸及方向之螺柱,且同時將其焊接至一工作表面上。此可調式筒夾亦將確保與螺柱可有較佳之接觸,並因而降低了產生電弧之可能性及不良之焊接,亦可藉由降低在筒夾與螺柱之間的滑動接觸而避免筒夾過早磨損。

    Abstract in simplified Chinese: 一种用于螺柱焊接之新颖可调式筒夹,其采用复数个充有电流之夹颚以稳固地夹持具有不同形状、尺寸及方向之螺柱,且同时将其焊接至一工作表面上。此可调式筒夹亦将确保与螺柱可有较佳之接触,并因而降低了产生电弧之可能性及不良之焊接,亦可借由降低在筒夹与螺柱之间的滑动接触而避免筒夹过早磨损。