Abstract:
PURPOSE: A high functional piezoelectric ceramic composition manufacturing method and piezoelectric ceramic composition manufactured using the same are provided to manufacture piezoelectric components with high reliability by increasing a mechanical quality factor. CONSTITUTION: Specimens of PbO, ZrO2, TiO2, MnO2, NiO, and Nb2O5 are mixed and pulverized. The mixed and pulverized specimen is dried in a temperature range of 75 to 100°C. The dried specimen is calcined in a temperature range of 800 to 900°C. The calcined specimen is mixed and pulverized for a second time after adding CeO2 and a dispersion medium. The mixed and pulverized calcined specimen is dried in the temperature range of 75 to 100°C. The dried calcined specimen is molded for being sintered.
Abstract:
PURPOSE: Functional shoes are provided to improve energy conversion efficiency and to endure external force repeated during walking. CONSTITUTION: Functional shoes comprise: a shoes body(110); an elastic airbag(120) which repeats contraction and expansion by an external force applied during walking; an air channel tube(130) which inhales air from an inlet and discharges air to an outlet; a check valve(140) preventing the suction of the air from the outlet during inflation of the elastic airbag and the exhaustion of the air to the inlet during contraction of the elastic airbag; a turbine(150) which is formed within the air channel tube and revolves; a generator(160) generating electromotive force by the rotation of the turbine; and an output terminal(170) which outputs electrical energy to the outside of the shoes body.
Abstract:
본 발명은 납이 함유되지 않은 비납계 압전 세라믹 조성물과 그의 제조방법에 관한 것으로서, 보다 상세하게는 센서 및 액추에이터에 적용될 수 있는 우수한 전기기계결합계수 및 압전특성을 지닌 납이 함유되지 않은 압전 세라믹 조성물 및 그 제조방법에 관한 것이다. 본 발명의 압전 센서 및 액추에이터용 비납계 압전 세라믹 조성물은 x Na(Nb 0.8 Ta 0.2 )O 3 - y K(Nb 0.8 Ta 0.2 )O 3 - z Li(Nb 0.8 Ta 0.2 )O 3 의 분말 1mol 대비 a mol의 비율로 Li 2 CO 3 가 첨가된 조성을 갖되, 상기 x는 0.47 이상 0.53 이하이고, y는 0.98-x이고, z는 0.02이며, a는 0.01이다. 보다 바람직하게는 상기 x는 0.51이다. 비납계, 압전, 세라믹조성물, 하소, 재하소, 소결,
Abstract:
본 발명은 압전 자기 조성물에 관한 것으로서, 압전변위제어용으로 적층형 압전 액츄에이터에 사용될 수 있는 높은 전기기계결합계수(k p )와 압전상수(d 33 )를 갖는 압전 자기 조성물에 관한 것이다. 본 발명의 조성물은 안정한 ABO 3 구조를 갖는 0.4Pb(Mg 1/3 Nb 2/3 )O 3 -0.25PbZrO 3 -0.35PbTiO 3 의 100중량부 대비, 0.05 중량부의 Li 2 CO 3 , 0.01 중량부의 Bi 2 O 3 , 1 중량부의 PbO 및 d중량부의 CuO가 첨가된 압전 자기 조성물로서, 상기 d는 0 초과 0.5이하의 범위이며, 보다 바람직하게는 상기 d는 0.3이다. CuO를 첨가함에 따라 전기기계결합계수(k p ) 및 압전상수(d 33 )가 증가하는 한편 소결온도는 950 ℃로 낮출수 있었으며, 따라서 보다 값싼 은 전극을 사용할 수 있는 적층형 압전액츄에이터에 응용될 수 있는 압전 자기 조성물 및 그 제조방법을 제공한다. 압전세라믹스, 액츄에이터, 압전변위소자, 적층세라믹스, 저온소성
Abstract:
본 발명은 전기영동증착을 이용한 적층형 세라믹 소자의 공극 밀봉 방법에 관한 것으로 동시 소성이 요구되는 적층형 세라믹 소자의 제조 시 부 전극과 세라믹 테이프로 구성되는 적층체들 사이에 발생되는 세라믹테이프와 전극 사이의 단차를 줄일 수 있으며 고 적층체를 제조하기 위해서 적층형 세라믹 소자의 상층부와 하층부에 포함된 내부 전극의 변형이 없이 간편하게 일체화된 고적층형 세라믹 소자를 제조할 수 있는 공정에 관한 것이다. 세라믹 적층 소자 공극 밀봉 전기영동증착
Abstract:
PURPOSE: A piezoelectric composition is provided to use in a multilayer piezoelectric actuator for controlling piezoelelctric strain and to lower sintering temperature by 950 °C. CONSTITUTION: A piezoelectric composition is a composition in which Li2CO3, Bi2O3, PbO and CuO are added to xPb(Mg_1/3 Nb_2/3)O3-yPbZrO_3-zPbTiO_3. X is 0.35-0.45, and y is 0.2-0.3, z is 1-x-y. The addition amount of Li_2CO_3, Bi_2O_3 and PbO is a weight parts, b weight parts, and c weight parts.
Abstract translation:目的:提供一种压电组合物,用于多层压电致动器,用于控制压电应变和将烧结温度降低950℃。 构成:压电组合物是其中将Li 2 CO 3,Bi 2 O 3,PbO和CuO加入到xPb(Mg_1 / 3Nb_2 / 3)O3-yPbZrO_3-zPbTiO_3中的组合物。 X为0.35-0.45,y为0.2-0.3,z为1-x-y。 Li_2CO_3,Bi_2O_3和PbO的添加量是重量份,b重量份和c重量份。
Abstract:
PURPOSE: A stacked bending type piezoelectric device and an energy generation device using the same are provided to successively generate energy by overlapping the attenuation section of voltage signal. CONSTITUTION: A metal plate(120) is stacked on one side of a piezoelectric device(110) which is based on a ceramic. The ceramic-based piezoelectric device and one end of the metal plate are bent. A bending part(b) is formed. The piezoelectric device and the metal plate are adhered by a resin adhesion layer(130). The resin adhesion layer fixes the metal plate and the piezoelectric device.
Abstract:
A composition and a manufacturing method of lead-free piezoelectric ceramics are provided to improve the piezoelectricity characteristic by adding Li2CO3 and Na2CO3 to the ceramic composition. The manufacturing method of the lead-free piezoelectric ceramic composition comprises the following steps: the step that mixes and pulverizes the sample of the Na2CO3, K2CO3, Li2CO3, Nb2O5, and Ta2O5 and dries and burns; the step that re-burns the burned sample; the step for remixing, re-pulverizing the sample; the step for sintering and molding the dried sample. Li2CO3 and Na2CO3 are added to the ceramic composition of (NaxK0.95-xLi0.05)(Nb0.95Ta0.05)O3.
Abstract translation:提供无铅压电陶瓷的组成和制造方法,以通过向陶瓷组合物中加入Li 2 CO 3和Na 2 CO 3来改善压电特性。 无铅压电陶瓷组合物的制备方法包括以下步骤:将Na 2 CO 3,K 2 CO 3,Li 2 CO 3,Nb 2 O 5和Ta 2 O 5的样品混合并粉碎并干燥和灼烧; 重烧烧伤样本的步骤; 重新混合,重新粉碎样品的步骤; 烧结和模制干燥样品的步骤。 (Na x K 0.95-x Li 0.05)(Nb 0.95 Ta 0.05)O 3的陶瓷组合物中添加Li 2 CO 3和Na 2 CO 3。