公开(公告)号:KR1019960012944B1
公开(公告)日:1996-09-25
申请号:KR1019930020905
申请日:1993-10-08
IPC: H01P1/20
Abstract: a cubic dielectric block(1) of which five surfaces excluding an upper side are plated with conductor; and a plurality of plated resonators(2,3). The coupling structure consists of: a coupler(4) placed between resonators(2,3), having a hole determined according to the coupling between resonators, and plated with conductor, so that it can adjust the amount of coupling between resonators(2,3); an error correction groove(5) of a depth at the upper side of the coupler(4) inside of which is plated with conductor; and an electrode pattern(6) connecting a side of dielectric block and the error correction groove(5) so that it can be used for grounding.
Abstract translation: 其中除了上侧之外的五个表面镀有导体的立方体介质块(1) 和多个电镀谐振器(2,3)。 耦合结构包括:放置在谐振器(2,3)之间的耦合器(4),具有根据谐振器之间的耦合确定的孔并且镀有导体,从而可以调节谐振器(2, 3); 位于其内部的耦合器(4)的上侧的深度的纠错槽(5)镀有导体; 以及连接介质块的一侧和误差校正槽(5)的电极图案(6),使得其可以用于接地。
-
-
-
公开(公告)号:KR1019950014717B1
公开(公告)日:1995-12-13
申请号:KR1019930004196
申请日:1993-03-18
IPC: C04B35/46
Abstract: The magnetic composition of dielectric ceramics comprises 70 mol% titania(TiO2), 20mol% barium carbonate(BaCO3), 5-9 mol% neodymium oxide(Nd2O3), 1-5 mol% dysprsium oxide(Dy2O3) and less than 1 mol% copper titanate(CuTiO3). And the compound is sintered at 1,220-1,260 deg.C. The CuTiO3 is prepared by calcinating a mixture of copper oxide and titania having a mole ratio of 1:1. The obtained dielectric ceramics, used for temperature compensation, has a low temperature coefficient, a high permittivity and a low dielectric loss at high frequencies.
Abstract translation: 电介质陶瓷的磁性组成包括70mol%二氧化钛(TiO 2),20mol%碳酸钡(BaCO 3),5-9mol%氧化钕(Nd 2 O 3),1-5mol%氧化镝(Dy 2 O 3)和小于1mol% 钛酸铜(CuTiO3)。 该化合物在1,220-1,260℃烧结。 通过煅烧氧化铜和摩尔比为1:1的二氧化钛的混合物制备CuTiO 3。 用于温度补偿的所获得的电介质陶瓷在高频下具有低温度系数,高介电常数和低介电损耗。
-
-
公开(公告)号:KR1019940011690B1
公开(公告)日:1994-12-23
申请号:KR1019920011795
申请日:1992-07-02
IPC: H01C7/00
Abstract: The dielectric magnetic compound has the high dielectric constant, low temperature coefficient, and the high sintering density on the range of 5.21-5.64. The dielectric magnetic compound consists of 54 mol% ZrO2, 50-46 mol% TiO2, and 0-5 mol% Ta2O5 sintered at the temperature of 1350-1450 deg.C.
Abstract translation: 介电磁性复合材料介电常数高,温度系数低,烧结密度高,为5.21-5.64。 介电磁性化合物由1350-1450℃温度下烧结的54mol%ZrO 2,50-46mol%TiO 2和0-5mol%Ta 2 O 5组成。
-
-
-
公开(公告)号:KR1019940002871A
公开(公告)日:1994-02-19
申请号:KR1019920011794
申请日:1992-07-02
IPC: H01C7/00
Abstract: 본 발명은 온도보상용 유전체 자기 조성물에 관한 것으로, 상온에서 유전율 80 이상, 그리고 1000 이상의 높은 품질계수 Q와 양호한 온도특성을 갖도록 하여 캐패시터 및 노이즈 제거용 EMI(전자파장해)필터 제작에 이용하는 한편, 전극재료로는 고가의 Pd이나 Pt재료 대신에 저가의 은합금을 이용할 수 있는 온도보상용 유전체 자기 조성물에 관한 것이다.
이에 따른 본 발명은 희토류가 포함된 온도보상용 유전체 자기 조성물에 있어서, 70mol% 이산화티탄(Ti0
2 ), 16mon%의 탄산바륨(BaCO
3 ), 5~9mol%의 산화네오디뮴(Nd
2 O
3 ), 1~5mol%의 산화세륨(CeO
2 )으로 이루어 지는 것을 특징으로 하는 온도보상용 유전체 자기조성물에 관한 것이다.
-
-
-
-
-
-
-
-
-