酸・塩基混合物および該混合物からなるイオン伝導体
    1.
    发明申请
    酸・塩基混合物および該混合物からなるイオン伝導体 审中-公开
    这种混合物组成的酸碱混合物和离子导体

    公开(公告)号:WO2005006352A1

    公开(公告)日:2005-01-20

    申请号:PCT/JP2004/009801

    申请日:2004-07-09

    Abstract: An acid-base mixture composed of a base component and an acid component wherein at least either the base component or the acid component is composed of at least two different compounds is characterized in that at least one base in the base component is represented by the formula (1) below. An ion conductor is characterized by being composed of an acid-base mixture which is composed of a base component composed of a base represented by the formula (2) below and an acid component. (In the formula (1), R , R and R represent a hydrocarbon group having 1-20 carbon atoms or a hydrogen atom, and at least one of them is a hydrocarbon group.) (In the formula (2), R , R and R represent a hydrocarbon group having 1-20 carbon atoms or a hydrogen atom, and R and R are not the same.)

    Abstract translation: 由碱组分和酸组分组成的酸碱混合物,其中至少一种碱组分或酸组分由至少两种不同的化合物组成,其特征在于,基组分中的至少一个碱由式 (1)。 离子导体的特征在于由酸基混合物组成,该酸碱混合物由以下由式(2)表示的碱组成的碱组分和酸组分组成。 (式(1)中,R 1,R 2,R 3表示碳原子数为1〜20的烃基或氢原子,至少1个为烃基)( 在式(2)中,R 1,R 2和R 3表示具有1-20个碳原子或氢原子的烃基,R 1和R 3不同 。)

    高分子電解質膜およびその製造法
    3.
    发明申请
    高分子電解質膜およびその製造法 审中-公开
    聚电解质膜及其制备方法

    公开(公告)号:WO2004001771A1

    公开(公告)日:2003-12-31

    申请号:PCT/JP2003/007740

    申请日:2003-06-18

    Abstract: 両面に貫通した細孔を有する高分子微多孔質膜に、重量比l/99~99/1の範囲の高分子と溶融塩との混合物および/または溶融塩を含有させてなる高分子電解質膜。該高分子電解質膜は、安価で耐久性があり、機械的強度に優れ、高温でも構造保持性に優れ、高分子微多孔質膜に溶融塩を安定に保持でき、耐熱性に優れ、水あるいは溶媒がなくても高いイオン伝導性を示し、燃料電池、二次電池、電気二重層キャパシタ、電解コンデンサなどに利用することができる。

    Abstract translation: 一种聚电解质膜,其包含聚合物和熔融盐的重量比为1 / 99-99 / 1的混合物和/或熔融盐,所述熔融盐包含在具有穿透相对表面的薄孔的聚合物微孔膜中 它们。 聚电解质膜廉价耐用,机械强度优异,即使在高温下也具有优异的结构保持性,能够不断地将熔融盐保持在聚合物微孔膜中,耐热性优异,即使在 无水或溶剂,适用于燃料电池,二次电池,双电层电容器,电解电容器等。

    高分子電解組成物
    6.
    发明申请
    高分子電解組成物 审中-公开
    聚电解质组合物

    公开(公告)号:WO2003046080A1

    公开(公告)日:2003-06-05

    申请号:PCT/JP2002/012510

    申请日:2002-11-29

    Abstract: An inexpensive and durable polyelectrolyte composition which is characterized by consisting of both an aromatic polymer containing carbonyl linkages and/or sulfonyl linkages in the backbone chain and bearing cation-exchange groups and a fused salt and which exhibits a high ionic conductivity even in the absence of water or a solvent. The aromatic polymer is preferably an aromatic polyether sulfone comprising specific structural units and bearing cation-exchange groups, an aromatic polyether ketone comprising specific structural units and bearing cation-exchange groups, an aromatic polyether sulfone block copolymer consisting of at least one hydrophilic segment bearing cation-exchange groups and at least one hydrophobic segment free from cation-exchange groups, and/or an aromatic polyether ketone block copolymer consisting of at least one hydrophilic segment bearing cation-exchange groups and at least one hydrophobic segment free from cation-exchange groups. The use of such a block copolymer as the aromatic polymer gives polyelectrolyte compositions which are excellent in maintenance of structure even at high temperature.

    Abstract translation: 其特征在于廉价且耐用的聚电解质组合物,其特征在于在主链中含有羰基键和/或磺酰基键并带有阳离子交换基团的芳族聚合物和熔融盐,并且即使在不存在 水或溶剂。 芳族聚合物优选为包含特定结构单元和带有阳离子交换基团的芳族聚醚砜,包含特定结构单元并带有阳离子交换基团的芳族聚醚酮,由至少一个亲水链段承载阳离子组成的芳族聚醚砜嵌段共聚物 - 交换基团和至少一个不含阳离子交换基团的疏水链段,和/或由至少一个带有阳离子交换基团的亲水链段和至少一个不含阳离子交换基团的疏水部分组成的芳族聚醚酮嵌段共聚物。 使用这样的嵌段共聚物作为芳香族聚合物,即使在高温下也具有优异的维持结构的聚电解质组合物。

    ポリイミドフィルム
    8.
    发明专利

    公开(公告)号:JPWO2018221607A1

    公开(公告)日:2020-04-02

    申请号:JP2018020805

    申请日:2018-05-30

    Abstract: フィルム厚みが10μmで、400℃で4時間保持した時の重量保持率が99.0%以上であり、YI(黄色度)が10以下であり、且つ、100〜350℃の間の線熱膨張係数が55ppm/K以下であるポリイミドフィルムが開示される。このポリイミドフィルムは、透明性、耐熱性に優れ、線熱膨張係数も低く、例えばディスプレイ用、タッチパネル用、または太陽電池用の基板に好適に用いることができる。

    ポリイミドフィルム
    10.
    发明专利

    公开(公告)号:JP2018204034A

    公开(公告)日:2018-12-27

    申请号:JP2018184592

    申请日:2018-09-28

    Abstract: 【課題】 透明性、耐熱性に優れ、線熱膨張係数も低く、例えばディスプレイ用、タッチパネル用、または太陽電池用の基板に好適に用いることができるポリイミドフィルムを提供する。 【解決手段】 本発明のポリイミドフィルムは、フィルム厚みが10μmで、400℃で4時間保持した時の重量保持率が99.0%以上であり、YI(黄色度)が10以下であり、且つ、100〜350℃の間の線熱膨張係数が55ppm/K以下であることを特徴とする。 【選択図】 なし

Patent Agency Ranking