公开(公告)号:JPH0370768A
公开(公告)日:1991-03-26
申请号:JP20729789
申请日:1989-08-09
Applicant: TORAY INDUSTRIES
Inventor: SAKAMOTO JUN , YOSHIDA MINORU , UEDA TOMOAKI
Abstract: PURPOSE:To obtain a polyester composition giving a molded article having excellent slipperiness, abrasion resistance, etc., and suitable for fiber, film, etc., by using composite inert particles having a specific shape as a component. CONSTITUTION:The objective polyester composition is produced by compounding a polyester with 0.005-10wt.% (preferably 0.01-3wt.%) of composite inert particles having an average particle diameter of 0.05-5mum (preferably 0.1-2mum) and produced e.g. by coating a core particle charged with positive or negative charge (e.g. silica, titanium oxide or calcium carbonate) with fine particles (e.g. silica or alumina) charged with opposite charge and having an average particle diameter corresponding to 1/(1,000-10) [preferably 1/(500-20)] of the diameter of the core particle. The ratio of the coating thickness to the diameter of the core particle is 1/1000-10, preferably 1/500-1.
-
42.
公开(公告)号:JPH0280455A
公开(公告)日:1990-03-20
申请号:JP23433188
申请日:1988-09-19
Applicant: TORAY INDUSTRIES
Inventor: YOSHIDA MINORU , SAKAMOTO JUN , UEDA TOMOAKI
Abstract: PURPOSE:To obtain the title composition useful for obtaining a film or a fiber excellent in lubricity, abrasion resistance and transparency by homogeneously dispersing spherical kaolinite particles in a thermoplastic polyester. CONSTITUTION:Desirably, 0.005-10wt.%, based on the polyester, porous synthetic spherical kaolinite particles having a mean particle diameter of, desirably, 0.01-5.0mum and a volume shape factor as defined by the equation (wherein V is the volume of a single particle; and D is the sphere equivalent diameter of a particle)
-
公开(公告)号:JPH0238444A
公开(公告)日:1990-02-07
申请号:JP18938988
申请日:1988-07-28
Applicant: TORAY INDUSTRIES
Inventor: YOSHIDA MINORU , SAKAMOTO JUN , UEDA TOMOAKI
Abstract: PURPOSE:To obtain the title composition which can give a film or a fiber improved in lubricity and abrasion resistance by adding alumina particles to a thermoplastic polyester. CONSTITUTION:The title composition is obtained by adding 0.005-10wt.% alumina particles (A) which is desirably slurried in a glycol (a), has a mean particle diameter of 0.01-5.0mum and a volume shape factor phi of the formula (wherein v is the volume of a single particle, and D is the equivalent diameter of an equal volume particle)
-
公开(公告)号:JPH01247450A
公开(公告)日:1989-10-03
申请号:JP7421088
申请日:1988-03-28
Applicant: TORAY INDUSTRIES
Inventor: SAKAMOTO JUN , YOSHIDA MINORU , UEDA TOMOAKI
Abstract: PURPOSE:To obtain a composition which can give a film or a fiber excellent in lubricity and abrasion resistance, by dispersing cerium oxide particles in a thermoplastic polyester. CONSTITUTION:A thermoplastic polyester composition is formed by homogeneously and finely dispersing cerium oxide particles in a thermoplastic polyester. Although the cerium oxide particles used may be particles of cerium (III) oxide (Ce2O3) or cerium (IV) oxide (CeO2), CeO2 particles are more desirable. The mean particle diameter of the cerium oxide particles used is desirably 0.1-3.0Xm when it is used in a film or a fiber. When this diameter is below 0.01mum, the lubricity of a molding is not sufficient, while a diameter above 5mum is undesirable because large protrusions are formed on the molding. The content of the cerium oxide is desirably 0.01-5wt.% based on the polyester.
-
公开(公告)号:JPH01223156A
公开(公告)日:1989-09-06
申请号:JP4787588
申请日:1988-03-01
Applicant: TORAY INDUSTRIES
Inventor: YOSHIDA MINORU , SAKAMOTO JUN , UEDA TOMOAKI
IPC: B29C55/12 , B29K67/00 , B29L7/00 , C08J5/18 , C08K3/04 , C08K3/22 , C08K3/26 , C08K3/34 , C08K7/18 , C08L67/00 , C08L67/02
Abstract: PURPOSE:To obtain the title composition capable of giving formed products of excellent slipperiness and wear resistance including biaxially oriented films suitable for e.g., magnetic tapes, by incorporating a polyester with each specified amount of each specific silicone resin particles and inert inorganic particles. CONSTITUTION:The objective composition can be obtained by incorporating a polyester with an intrinsic viscosity of 0.4-1.0 with (A) 0.005-10wt.% (pref. 0.01-5wt.%) of silicone resin particles with a mean size of 0.01-5mum (pref. 0.1-2mum) of which a structural unit of the formula [R1 is CnH2n-1 (n is 1-10) or phenyl] accounts for >=10mol.% (pref. >=50mol.%) and (B) 0.005-10wt.% (pref. 0.01-5wt.%) of an inert inorganic particles (e.g., talc, caolin, calcium carbonate) with a mean size of 0.01-5mum (pref. 0.1-2mum).
-
公开(公告)号:JPS62218123A
公开(公告)日:1987-09-25
申请号:JP6078186
申请日:1986-03-20
Applicant: TORAY INDUSTRIES
Inventor: MORITA TORU , YOSHIDA MINORU , OKASAKA HIDESADA
Abstract: PURPOSE:To realize favorable film-making productivity and at the same time high rigidity and excellent heat resisting property by a method wherein both calcium compound and phosphorous compound the number of molecules of which is specified are added during the synthesis stage of polyester. CONSTITUTION:In order to make polyester obtained by adding calcium compound and phosphorous compound, which satisfy formulae: 2
-
公开(公告)号:JPS62148453A
公开(公告)日:1987-07-02
申请号:JP28947685
申请日:1985-12-24
Applicant: TORAY INDUSTRIES
Inventor: YOSHIDA MINORU , MORITA TORU , OKASAKA HIDESADA
Abstract: PURPOSE:To enable ester interchange reaction of a dicarboxylic acid dialkyl ester with an alkylene glycol in short time and high stability, by performing he reaction in a reaction system under a pressure higher than atmospheric pressure and discharging the alkylene glycol out of the system. CONSTITUTION:Dialkyl ester of 1,2-bis(chlorophenoxy)ethane-4,4'-dicarboxylic acid is subjected to ester interchange reaction with an alkylene glycol under a pressure higher than atmospheric pressure, preferably under 0.1-3kg/cm G pressure. After the completion of the reaction, the pressure of the reaction system is lowered preferably to G and remaining alkylene glycol is discharged from the system to obtain bis(beta-hydroxyalkyl)-1,2-bis (chlorophenoxy)ethane-4,4'-dica-rboxyl ate or its oligomer.
-
公开(公告)号:JPS62109823A
公开(公告)日:1987-05-21
申请号:JP24892885
申请日:1985-11-08
Applicant: TORAY INDUSTRIES
Inventor: YOSHIDA MINORU , MORITA TORU , OKASAKA HIDESADA
Abstract: PURPOSE:To obtain the titled polymer having high rigidity, improved heat resistance, smooth film surface and good running property without trouble in yarn breakage as fibers, by adding inert inorganic particles to a specific dicarboxylic acid and glycol and poplycondensing the mixture. CONSTITUTION:(A) A dicarboxylic acid expressed by the formula (R1 and R2 are 1-4C alkyl), e.g. dimethyl 1,2-bis(2-chlorophenoxy)ethane-4,4'-dicarboxylate, and (B) a glycol, e.g. ethylene glycol, are charged into, e.g. a reactor, and ester interchange reaction is carried out. Before completing the reaction, (C) inert inorganic particles, e.g. mica, having
-
公开(公告)号:JP2003231229A
公开(公告)日:2003-08-19
申请号:JP2002029361
申请日:2002-02-06
Applicant: TORAY INDUSTRIES
Inventor: KOJIMA HIROJI , SAKAMOTO JUN , YOSHIDA MINORU
IPC: B32B27/36
Abstract: PROBLEM TO BE SOLVED: To provide a laminated polyester film excellent in strength and transparency and especially suitable for an optical use. SOLUTION: The laminated polyester film has at least one particle-containing layer and is characterized in that relational expressions of 0.5 COPYRIGHT: (C)2003,JPO
-
公开(公告)号:JP2003221491A
公开(公告)日:2003-08-05
申请号:JP2002021193
申请日:2002-01-30
Applicant: TORAY INDUSTRIES
Inventor: HONMA YOSHIHIRO , SAKAMOTO JUN , YOSHIDA MINORU
Abstract: PROBLEM TO BE SOLVED: To provide a polyester resin composition having various performances such as a productivity, an electric insulation, a thermal resistance, and to provide a film. SOLUTION: The polyester is composed of particles containing at least two kinds of elements selected from typical elements belonging to the IV or V period in the periodic table of elements. When the particles are added to the polyester to form the polyester resin composition, R and R0 satisfy the relation: R/R0≥1.1 (wherein R0 is a relative dielectric constant of the polyester before the particles are added and R is the relative dielectric constant of the polyester after the particles are added). COPYRIGHT: (C)2003,JPO
-
-
-
-
-
-
-
-
-