Abstract:
The instant invention concerns a composition comprising a base polymer, at least one compound of the formula E-(L-E)x wherein: E is formula (I) or formula (II) and L is a linking group; and at least one transition metal in a positive oxidation state. The invention also concerns packages containing walls comprising such compositions, methods of forming such packages, and methods of packaging an oxygen-sensitive item within such a package.
Abstract:
The present invention relates to methods for making cross-linked, oxidatively stable, and highly crystalline polymeric materials. The invention also provides methods of treating irradiation-cross-linked antioxidant-containing polymers and materials used therewith.
Abstract:
The object of the invention is to provide a polyester composition that actively scavenges oxygen, with or without a transition metal catalyst. This was achieved by using a monomer selected from the group consisting of linear difunctional monomers having the general formula: X—(CH2)n—CH═CH—(CH2)m—X′ wherein X and X′ are each independently selected from the group consisting of OR and COOR, wherein R is selected from the group consisting of H and alkyl groups with one or more carbon atoms; and n and m are each independently 1 or more. The preferred monomer is 2-butene-1,4-diol (BEDO), and the preferred polyester is the reaction product of this diol with terephthalic acid to form poly(oxy-2-butene-1,4-diyloxycarbonyl-1,4-phenylenecarbonyl)—PBET. Copolymers of PBET are also within the scope of this invention. The polyester oxygen scavenging composition is then blended with conventional container resin such as polyesters, polyamides or polyolefins to make a container.
Abstract:
Oxygen-scavenging polymers and packaging for holding oxygen-sensitive products. A heat treatment process has been found to significantly increase the oxygen-scavenging performance of the polymer. The enhanced scavenging polymer can be effectively incorporated into various packaging, including transparent multilayer containers for beer and juice. In one embodiment, a multilayer package made from the scavenger provides an actual reduction in oxygen content of a contents of the package, over a long period of time (e.g., 24 weeks). The package can be stored unfilled for an extended period (without significant loss of scavenging capability) and will scavenge substantially immediately upon filling with a liquid product. The package may incorporate a relatively low weight percentage of the scavenger, thus providing enhanced scavenging in a cost-effective manner.
Abstract:
An oxygen scavenger film includes a layer including an oxygen scavenger, and a layer including a cyclic olefin copolymer. An oxygen scavenger film includes a layer including a blend of an oxygen scavenger, and a cyclic olefin copolymer. A method of triggering an oxygen scavenger film includes providing an oxygen scavenger film including a layer including an oxygen scavenger, and a layer including a cyclic olefin copolymer; and subjecting the oxygen scavenger film to a dosage of actinic radiation effective to trigger the oxygen scavenger. A method of triggering an oxygen scavenger film includes providing an oxygen scavenger film including a layer including a blend of an oxygen scavenger and a cyclic olefin copolymer; and subjecting the oxygen scavenger film to a dosage of actinic radiation effective to trigger the oxygen scavenger.
Abstract:
The present invention provides conjugates having a degradable linkage and polymeric reagents useful in preparing such conjugates. The conjugates as well as the polymeric reagents used to form the conjugates include at least one of each the following: an aromatic moiety comprising an ionizable hydrogen atom, a spacer moiety, and a water-soluble polymer. Methods of making polymeric reagents and conjugates, as well as methods for administering conjugates and compositions, are also provided.
Abstract:
The present invention is directed to an oxygen scavenger composition comprising a mixture of (i) a polyester polymer composed of polymer segments containing cycloalkenyl group or functionality; and (ii) an ester type polymer selected from (a)a polyester having a high content of alkylene groups; (b) a polylactone; and (c) a polyvinylacetate having at least about 50 weight percent vinyl acetate mer units therein. The present polymer composition has been found to act as an oxygen scavenger agent under both ambient and refrigerated conditions, to be compatible with conventional film forming packaging materials, to provide compositions exhibiting low tack, and to be capable of being readily processed using conventional film forming equipment.
Abstract:
Disclosed herein are oxygen scavenging compositions and packaging articles that comprise (a) a metal catalyzed oxidizable compound and (b) at least one of a transition metal carboxylate, wherein the transition metal carboxylate comprises at least one carboxylate group and wherein each carboxylate group comprises between 20 and 30 carbon atoms, inclusive, such as cobalt behenate or cobalt arachidate.
Abstract:
A polymer composition capable of depleting oxygen from adjacent spaces is disclosed. One or more botanical extracts, either naturally occurring or synthetic, that contain proanthocyanidin or its derivatives are added to a base polymer or polymer blend prior to processing to provide the polymer with oxygen-scavenging benefits without adverse effect to the characteristics of the base polymer or polymer blend.
Abstract:
Oxygen-scavenging polymers and packaging for holding oxygen-sensitive products. A heat treatment process has been found to significantly increase the oxygen-scavenging performance of the polymer. The enhanced scavenging polymer can be effectively incorporated into various packaging, including transparent multilayer containers for beer and juice. In one embodiment, a multilayer package made from the scavenger provides an actual reduction in oxygen content of a contents of the package, over a long period of time (e.g., 24 weeks). The package can be stored unfilled for an extended period (without significant loss of scavenging capability) and will scavenge substantially immediately upon filling with a liquid product. The package may incorporate a relatively low weight percentage of the scavenger, thus providing enhanced scavenging in a cost-effective manner.