Abstract:
Cermets are provided in which the ceramic phase is selected from the group consisting of Cr23C6, Cr7C3, Cr3C2 and mixtures thereof. The binder phase is selected from certain specified Ni/Cr alloys and certain Fe/Ni/Cr alloys. These cermets are particularly useful in protecting surfaces from erosion at high temperatures.
Abstract translation:提供了金属陶瓷,其中陶瓷相选自Cr 23 C 6 C 6 C 6 C 7 C 6, SUB 3,Cr 3 3 C 2和它们的混合物。 粘结相选自某些特定的Ni / Cr合金和某些Fe / Ni / Cr合金。 这些金属陶瓷特别适用于在高温下保护表面免受侵蚀。
Abstract:
A method for welding and repairing cracks in metal parts is provided by subjecting the metal parts to be welded to friction stir welding and the cracks to be repaired to friction stir processing under conditions sufficient to provide a weld joint or crack repair having a preselected property or set of properties based upon the intended use of the weldment. The FSW and FSP methods are advantageous in joining and repairing metal structures and components in applications for natural gas transportation and storage, oil and gas well completion and production, and oil and gas refinery and chemical plants.
Abstract:
The invention includes a cermet composition represented by the formula (PQ) (RS) comprising: a ceramic phase (PQ) and a binder phase (RS) wherein, P is a metal selected from the group consisting of Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W, Fe, Mn and mixtures thereof, Q is carbonitride, R is a metal selected from the group consisting of Fe, Ni, Co, Mn and mixtures thereof, S comprises at least one element selected from Cr, Al, Si and Y.
Abstract:
The invention includes a cermet composition represented by the formula (PQ)(RS) comprising: a ceramic phase (PQ) and a binder phase (RS) wherein, P is a metal selected from the group consisting of Si, Mn, Fe, Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W and mixtures thereof, Q is nitride, R is a metal selected from the group consisting of Fe, Ni, Co, Mn and mixtures thereof, S consists essentially of at least one element selected from Cr, Al, Si, and Y, and at least one reactive wetting aliovalent element selected from the group consisting of Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W and mixtures thereof.
Abstract:
A cermet composition represented by the formula (PQ)(RS) comprising: a ceramic phase (PQ) and binder phase (RS) wherein, P is at least one metal selected from the group consisting of Group IV, Group V, Group VI elements, Q is boride, R is selected from the group consisting of Fe, Ni, Co, Mn and mixtures thereof, S comprises at least one element selected from Cr, Al, Si and Y.
Abstract:
A cermet composition represented by the formula (PQ)(RS) comprising: a ceramic phase (PQ) and binder phase (RS) wherein, P is at least one metal selected from the group consisting of Group IV, Group V, Group VI elements, Q is boride, R is selected from the group consisting of Fe, Ni, Co, Mn and mixtures thereof, S comprises at least one element selected from Cr, Al, Si and Y.
Abstract:
A method for processing a hot formed, high-tensile-strength steel having an ultimate tensile strength (UTS) of at least about 730 MPa (105 ksi) and excellent toughness to retain essentially all the strength and toughness is provided. This processing is needed for the fabrication of high strength fittings that are used in the construction of linepipe for transport of natural gas, crude oil, as well as other applications. Furthermore, the hot formed high strength steel may be weldable with a Pcm of less than or equal to 0.35.
Abstract:
An ultra-high strength, weldable, low alloy, dual phase steel with excellent cryogenic temperature toughness in the base plate and in the heat affected zone (HAZ) when welded, having a tensile strength greater than 830 MPa (120 ksi) and a microstructure comprising a ferrite phase and a second phase of predominantly lath martensite and lower bainite, is prepared by heating a steel slab comprising iron and specified weight percentages of some or all of the additives carbon, manganese, nickel, nitrogen, copper, chromium, molybdenum, silicon, niobium, vanadium, titanium, aluminum, and boron; reducing the slab to form plate in one or more passes in a temperature range in which austenite recrystallizes; further reducing the plate in one or more passes in a temperature range below the austenite recrystallization temperature and above the Ar.sub.3 transformation temperature; finish rolling the plate between the Ar.sub.3 transformation temperature and the Ar.sub.1 transformation temperature; quenching the finish rolled plate to a suitable Quench Stop Temperature (QST); and stopping the quenching.
Abstract:
A high strength steel composition comprising ferrite and martensite/bainite phases, the ferrite phase having primarily vanadium and niobium carbide or carbonitride precipitates, is prepared by a first rolling above the austenite recrystallization temperature, a second rolling below the austenite recrystallization temperature; cooling between the Ar.sub.3 transformation point and 500.degree. C.; and water cooling to below about 400.degree. C.
Abstract:
A steel composition and method from making a dual phase steel therefrom. The dual phase steel may have carbon of about 0.05% by weight to about 0.12 wt %; niobium of about 0.005 wt % to about 0.03 wt %; titanium of about 0.005 wt % to about 0.02 wt %; nitrogen of about 0.001 wt % to about 0.01 wt %; silicon of about 0.01 wt % to about 0.5 wt %; manganese of about 0.5 wt % to about 2.0 wt %; and a total of molybdenum, chromium, vanadium and copper less than about 0.15 wt %. The steel may have a first phase consisting of ferrite and a second phase having one or more of carbide, pearlite, martensite, lower bainite, granular bainite, upper bainite, and degenerate upper bainite. A solute carbon content in the first phase may be about 0.01 wt % or less.