Abstract:
This application describes a method of preparation of a natural graphene cellulose blended fiber, which comprises using a graphite powder as a raw material for preparing a graphene solution, adding the graphene solution to a slurry formed by mixing and dissolving a wood pulp with N-methylmorpholine N-oxide (NMMO), removing the water content thereof to form a spinning dope, and then spinning the spinning dope by a Dry-Jet Wet method to manufacture a natural graphene cellulose blended fiber. The present method does not require a highly toxic hydrazine hydrate solution. Further, by increasing the adding ratio of the graphene solution in the manufacturing process, control of the antistatic properties and thermal transferring functions can be achieved, and thereby various requirements of different consumers can be satisfied. Besides, the fibers can decompose naturally after being used, and thus the product is harmless, natural, and environmentally friendly.
Abstract:
This application describes a method of preparation of a natural graphene cellulose blended spunbond nonwoven fabric, which comprises using a graphite powder as a raw material for preparing a graphene solution, adding the graphene solution to a slurry formed by mixing and dissolving a wood pulp with N-methylmorpholine N-oxide (NMMO), removing the water content thereof to form a spinning dope, and then directly preparing the natural graphene cellulose blended spunbond nonwoven fabric by a spunbond process. The present method does not require a highly toxic hydrazine hydrate solution. Further, by increasing the adding ratio of the graphene solution in the manufacturing process, control of the antistatic properties and thermal transferring function can be achieved, and thereby various requirements of different consumers can be satisfied. Besides, the fabric can decompose naturally after being used, and thus the product is harmless, natural, and environmentally friendly.
Abstract:
The present invention provides a fabricating method for meltblown nonwoven from natural cellulose fiber blended with nano silver, which comprises following steps.Firstly, prepare nano silver colloidal sol by reduction titration for mixture of polyvinyl alcohol (PVA), silver nitrate (AgNO3) and sodium borohydride (NaBH4).Secondly, prepare mixing cellulose serum by blending agitation for mixture of wood pulp, N-methylmorpholine N-oxide (NMMO) and stabilizer.Thirdly, prepare blending mucilage from mixing cellulose serum via blending process.Fourthly, produce spinning dope by blending and dehydrating the nano silver colloidal sol and mixing cellulose serum.Fifthly, produce molten filament tow by meltblown spinning method in association with coagulation, regeneration in coagulation bath, and water rinse.Finally, by post treatments of hydro-entangled needle punching, drying, winding-up processes in proper order, obtain final product of meltblown nonwoven from natural cellulose fiber blended with nano silver, which is biodegradable with features of antibacterial and antistatic capabilities.
Abstract:
The present invention provides a fabricating method for spunbond nonwoven from natural cellulose fiber blended with nano silver, which comprises following steps.Firstly, prepare nano silver colloidal sol by reduction titration for mixture of polyvinyl alcohol (PVA), silver nitrate (AgNO3) and sodium borohydride (NaBH4).Secondly, prepare mixing cellulose serum by blending agitation for mixture of wood pulp, N-methylmorpholine N-oxide (NMMO) and stabilizer.Thirdly, prepare blending mucilage from mixing cellulose serum via blending process.Fourthly, produce spinning dope by blending and dehydrating the nano silver colloidal sol and mixing cellulose serum.Fifthly, produce molten filament tow by spunbond spinning method in association with coagulation, regeneration, water rinse and high-speed stretching process.Finally, by post treatments of hydro-entangled needle punching, drying, winding-up processes in proper order, obtain final product of spunbond nonwoven from natural cellulose fiber blended with nano silver, which is biodegradable with features of antibacterial and antistatic capabilities.
Abstract:
A spunbond method for producing non-woven fabric with deodorant feature from bamboo cellulose comprises following process steps. Prepare bamboo pulp mixture by blending bamboo pulp and coffee residue in proper mixing ratio. Put N-methylmorpholine N-oxide (NMMO) as solvent and 1, 3-phenylene-bis 2-oxazoline (BOX) as stabilizer into prepared bamboo pulp mixture to form dope. Via spunbond method, orderly perform extruding, spinning, quenching and pre-drawing process to convert the dope into bamboo filaments of fibrous strand. Orderly process coagulation, regeneration and post-draw to the bamboo filaments of fibrous strand to transform them into uniform fine bamboo cellulose filaments. Bond and lay these bamboo filaments of fibrous strand on a belt collector to form a webbed nonwoven. After post treatments of water rinsing, hydro-entangled needle punching and drying have been orderly applied, then a resultant nonwoven fabric in continuous filament of bamboo cellulose with deodorant feature is produced from the webbed nonwoven.
Abstract:
A stapled melt spinning method for producing nonwoven fabrics with hygroscopic metastatic feature. Firstly, fuse bio-polyamide 6,10 into melt, extrude and spin it out spin heads of extruder into filaments, cool, draw and collect filaments into tow, then extend, cut and card the filaments into the staples, and spread the staples on a conveyer to form fibrous web. Next, blend and dissolve pulp by N-methylmorpholine N-oxide (NMMO) dissolving solvent, dehydrate it to form dope, and extrude and spin it out spin heads of extruder into filaments, then cool, draw and collect filaments into tow, and extend, cut and card filaments into staples, then overlay the staples over existing fibrous web to form a composite fibrous web of bio-polyamide 6,10 and cellulose filaments. Finally, coagulate, regenerate and convert fibrous composite of bio-polyamide 6,10 and natural cellulose into nonwoven fabric with hygroscopic metastatic feature by hydro-entangled needle punching, drying, winding-up processes.
Abstract:
The present invention provides a processing method of natural cellulose fiber intrinsically with enhanced antiseptic, deodorant and negative-ion features from bamboo. The process uses mixture of wasted coffee residue and bamboo pulp as raw material. The process uses N-methylmorpholine N-oxide (NMMO) as primary solvent and 1, 3-phenylene-bis 2-oxazoline (BOX) as additive stabilizer. A cellulose solution is firstly formed by the wasted coffee residue, bamboo pulp, NMMO and BOX aforesaid. Secondly, via grinding, blending, dissolving and thermal dehydrating, the cellulose solution is converted into spinning dope. Thirdly, spin the dope obtained previously by dry-jet wet spinning method and coagulate and regenerate in a coagulation bath to form into threads. Finally, rinse, desiccate and lubricate the regenerated threads obtained previously as well as wind it up to produce reeled natural bamboo cellulose fiber with enhanced antiseptic, deodorant and negative-ion features.