Abstract:
Embodiments of glass articles exhibiting a grey or a green tint are described. In one or more embodiments, the glass article comprises a glass composition including SiO2, Al2O3 B2O3 or MgO, a non-zero amount of alkali metal oxides (R2O), R2O—Al2O3 in the range from about −0.5 to about 1.5; and up to 1 mol % Fe2O3. In one or more embodiments, the glass composition includes a ratio of R2O to Al2O3 equal to or greater than about 1, Na2O, from 0-13 mol % MgO, at least one of K2O, SnO2 and TiO2. Laminates including such glass articles and methods of making the glass articles are also described.
Abstract:
According to one embodiment, a glass article may include SiO2, Al2O3, Li2O and Na2O. The glass article may have a softening point less than or equal to about 810° C. The glass article may also have a high temperature CTE less than or equal to about 27×10−6/° C. The glass article may also be ion exchangeable such that the glass has a compressive stress greater than or equal to about 600 MPa and a depth of layer greater than or equal to about 25 μm after ion exchange in a salt bath comprising KNO3 at a temperature in a range from about 390° C. to about 450° C. for less than or equal to approximately 15 hours.
Abstract:
Glass compositions and glass articles comprising the glass compositions are disclosed. In one embodiment, a glass composition includes from about 65 mol. % to about 70 mol. % SiO2; from about 9 mol. % to about 14 mol. % Al2O3; and from about 0 mol. % to about 11 mol. % B2O3 as glass network formers. The glass composition also includes from about 5 mol. % to less than 10 mol. % alkali oxide R2O, wherein R is at least one of Li, Na, and K. The glass composition also includes from about 3 mol. % to about 11 mol. % of divalent oxide MO, wherein M is at least one of Mg, Ca, Ba, SrO and Zn. The glass composition has a coefficient of thermal expansion which is less than or equal to 55×10-7/° C. and is amenable to strengthening by ion-exchange. The glass composition is well suited for use as the glass cladding layers of a laminated glass article.
Abstract:
An ion exchangeable glass that is free of lithium and comprising 0.1-10 mol % P2O5 and at least 5 mol % Al2O3. The presence of P2O5 enables the glass to be ion exchanged more quickly and to a greater depth than comparable glasses that do not contain P2O5.
Abstract:
Disclosed herein are glass-ceramics having crystalline phases including β-spodumene ss and either (i) pseudobrookite or (ii) vanadium or vanadium containing compounds so as to be colored and opaque glass-ceramics having coordinates, determined from total reflectance—specular included—measurements, in the CIELAB color space of the following ranges: L*=from about 20 to about 45; a*=from about −2 to about +2; and b*=from about −12 to about +1. Such CIELAB color space coordinates can be substantially uniform throughout the glass-ceramics. In each of the proceeding, β-quartz ss can be substantially absent from the crystalline phases. If present, β-quartz ss can be less than about 20 wt % or, alternatively, less than about 15 wt % of the crystalline phases. Also Further crystalline phases might include spinel ss (e.g., hercynite and/or gahnite-hercynite ss), rutile, magnesium zinc phosphate, or spinel ss (e.g., hercynite and/or gahnite-hercynite ss) and rutile.
Abstract:
According to one embodiment, a glass article may include SiO2, Al2O3, Li2O and Na2O. The glass article may have a softening point less than or equal to about 810° C. The glass article may also have a high temperature CTE less than or equal to about 27×10−6/° C. The glass article may also be ion exchangeable such that the glass has a compressive stress greater than or equal to about 600 MPa and a depth of layer greater than or equal to about 25 μm after ion exchange in a salt bath comprising KNO3 at a temperature in a range from about 390° C. to about 450° C. for less than or equal to approximately 15 hours.
Abstract:
A fining agent for reducing the concentration of seeds or bubbles in a silicate glass. The fining agent includes at least one inorganic compound, such as a hydrate or a hydroxide that acts as a source of water. In one embodiment, the fining agent further includes at least one multivalent metal oxide and, optionally, an oxidizer. A fusion formable and ion exchangeable silicate glass having a seed concentration of less than about 1 seed/cm3 is also provided. Methods of reducing the seed concentration of a silicate glass, and a method of making a silicate glass having a seed concentration of less than about 1 seed/cm3 are also described.
Abstract:
A glass and an enclosure, including windows, cover plates, and substrates for mobile electronic devices comprising the glass. The glass has a crack initiation threshold that is sufficient to withstand direct impact, has a retained strength following abrasion that is greater than soda lime and alkali aluminosilicate glasses, and is resistant to damage when scratched. The enclosure includes cover plates, windows, screens, and casings for mobile electronic devices and information terminal devices.
Abstract:
According to one embodiment, a glass article may include SiO2, Al2O3, Li2O and Na2O. The glass article may have a softening point less than or equal to about 810° C. The glass article may also have a high temperature CTE less than or equal to about 27×10−6/° C. The glass article may also be ion exchangeable such that the glass has a compressive stress greater than or equal to about 600 MPa and a depth of layer greater than or equal to about 25 μm after ion exchange in a salt bath comprising KNO3 at a temperature in a range from about 390° C. to about 450° C. for less than or equal to approximately 15 hours.