Abstract:
A method for increasing working time/setting time of monolithic tetracalcium phosphate (TTCP) cement paste formed by mixing a TTCP powder with an aqueous solution, which includes heating the TTCP powder, prior to the mixing, so that the TTCP powder is maintained at a temperature of 50-350° C. for a period of time which is greater than one minute, and that a TTCP cement paste formed by mixing the resulting heated TTCP powder with the aqueous solution has a prolonged working time in comparison with that formed by mixing TTCP powder that has not been subjected to such heating with the aqueous solution.
Abstract:
A tetracalcium phosphate (TTCP) particle for use in preparing a fast-setting, bioresorbable calcium phosphate cement is disclosed. The TTCP particle has a basic calcium phosphate whiskers on a surface thereof; the basic calcium phosphate whiskers having a Ca/P molar ratio greater than 1.33, and having a length up to about 5000 nm and a width up to about 500 nm. The basic calcium phosphate whiskers are substantially free of a hydroxyapatite phase and mainly composed of TTCP phase.
Abstract:
A fast-setting, bioresorbable calcium phosphate cement is prepared by a process which can be carried out with a heat treatment up to 1000° C. on a mixture of a wetting solution and a calcium phosphate powder having a Ca to P molar ratio of 0.5-2.5. The wetting solution suitable for use in the process of the present invention includes water, an organic solvent, an acidic and basic solution. A setting solution for mixing with the heated powder to form the fast-setting, bioresorbable calcium phosphate cement may be water, an acidic or basic solution according to the process of the present invention.
Abstract:
A calcium phosphate cement suitable for use in dental and bone prosthesis is disclosed, which include calcium phosphate particles having a diameter of 0.05 to 100 microns, wherein said calcium phosphate particles on their surfaces have whiskers or fine crystals having a width ranging from 1 to 100 nm and a length ranging from 1 to 1000 nm.
Abstract:
A calcium phosphate cement suitable for use in dental and bone prosthesis is disclosed, which include calcium phosphate particles having a diameter of 0.05 to 100 microns, wherein said calcium phosphate particles on their surfaces have whiskers or fine crystals having a width ranging from 1 to 100 nm and a length ranging from 1 to 1000 nm.
Abstract:
A tetracalcium phosphate (TTCP) particle for use in preparing a fast-setting, bioresorbable calcium phosphate cement is disclosed. The TTCP particle has a basic calcium phosphate whiskers or fine crystals on a surface thereof; the basic calcium phosphate whiskers or fine crystals having a Ca/P molar ratio greater than 1.33, and having a length up to about 5000 nm and a width up to about 500 nm.
Abstract:
The present disclosure uses different kinds of surface treatment processes on titanium-made dental implants. The growth and attachment conditions of bone cells (MC3T3-E), fibroblasts (NIH 3T3) and epidermal cells (XB-2) on the metal surface of titanium slices with different surface treatments are observed. Tetra-calcium phosphate is used to perform secondary sand-blasting process to clean up the metal surface and provide calcium ions for osteoblastoma physiology. Thus, by adjusting the cells adhesive and proliferative abilities, the success rate of the clinical applications in dental implant is improved.
Abstract:
The present disclosure uses different kinds of surface treatment processes on titanium-made dental implants. The growth and attachment conditions of bone cells (MC3T3-E), fibroblasts(NIH 3T3) and epidermal cells (XB-2) on the metal surface of titanium slices with different surface treatments are observed. Tetra-calcium phosphate is used to perform secondary sand-blasting process to clean up the metal surface and provide calcium ions for osteoblastoma physiology. Thus, by adjusting the cells adhesive and proliferative abilities, the success rate of the clinical applications in dental implant is improved.