Abstract:
A block copolymer composition with a good balance of physical properties suitable for various types of packaging such as food product containers, beverage containers, industrial containers and blister packs, having excellent transparency, gloss, strength, rigidity and formability, having excellent anti-blocking properties and anti-sticking properties, and excelling in the aforementioned properties even when used in mixture with vinyl aromatic hydrocarbon-type polymers is offered. A block copolymer composition of a vinyl aromatic hydrocarbon and a conjugated diene, wherein a block copolymer component (I) having a molecular weight peak in the range of molecular weight 150,000 to 300,000 and comprising tapered blocks has a conjugated diene content of 10 to 20 mass %; a block copolymer component (II) having a molecular weight peak in the range of molecular weight 50,000 to 140,000 and comprising tapered blocks has a conjugated diene content of 30 to 50 mass %; and a ratio (I)/(II) between molecular weight peak areas occupied by block copolymer component (I) and block copolymer component (II) in the block copolymer composition is 20/80 to 80/20.
Abstract:
A scratch resistant article comprising a blend which comprises from 50 to 95 percent by weight polycarbonate; and from 5 to 50 percent by weight modified methyl methacrylate polymer, wherein the modified methyl methacrylate polymer is selected from the group consisting of modified methyl methacrylate homopolymer, modified methyl methacrylate copolymers, and combinations thereof; wherein the modified methyl methacrylate polymer has one or more end groups provided by reaction with one or more chain transfer agents selected from the group consisting of mercapto esters, cycloalkyl and substituted cycloalkyl thiols, hydroxyl thiols, aryl and substituted aryl thiols, and aminoalkyl thiols, wherein the modified methyl methacrylate polymer has a Mw from 5,000 to 100,000 g/mole; and wherein the blend exhibits a pencil hardness equal to or greater than F measured according to ASTM D3363-05 is provided. A method for making a scratch resistant article is also provided.
Abstract:
A transparent ABS resin composition of the present invention comprises: an acrylonitrile-butadiene-styrene graft (g-ABS) copolymer which is copolymerized by mixture of acrylate based monomer, styrene based monomer, and acrylonitrile based monomer (a2) on butadiene based rubber polymer (a1); and (B) a styrene-acrylonitrile based copolymer, satisfies a relation denoted by Equation 1 and Equation 2 below, and has excellent impact resistance, scratch resistance, and transparency: 0≦|X−Y|≦0.005 (Equation 1) 0≦|X−Z|≦0.005 (Equation 2) In the Equations, X is refractive index of the acrylonitrile-butadiene-styrene graft (g-ABS) copolymer, Y is refractive index of the butadiene based rubber polymer (a1), and Z is refractive index of the styrene-acrylonitrile based copolymer (B).
Abstract:
The present invention relates to a photochromic lens, which comprises a photochromic layer comprising a photochromic dye and a resin component, and an organic hardcoat layer in this order, wherein the resin component is an acrylic resin, and the photochromic layer further comprises a piperidine ring-containing compound having a molecular weight of equal to or greater than 1,000.
Abstract:
An acrylic thermoplastic resin composition includes a first acrylic resin having a first structural unit represented by the following formula (1) and a second structural unit represented by the following formula (2), and a second acrylic resin having the first structural unit represented by the following formula (1) and a third structural unit represented by the following formula (3), in which a total content of the first unit is 50 to 95 mass % and a total content of the second structural unit and the third structural unit is 5 to 50 mass % based on a total amount of the first acrylic resin and the second acrylic resin:
Abstract:
A method for manufacturing a polycarbonate composition having improved transparency can comprise reacting an aromatic dihydroxy compound and a diaryl carbonate under melt polymerization conditions to provide a polycarbonate; and contacting the polycarbonate with a polydiorgano siloxane having a kinematic viscosity of less than 20 mm2/sec at 25° C. as determined in accordance with ASTM D445, and an optional additive thereby making the polycarbonate composition. The polycarbonate composition has haze less than 1% as determined in accordance with ASTM D1003-07, and can be used for optical applications such as automotive headlamps.
Abstract:
A transparent article includes a continuous polyester matrix having at least one incompatible filler dispersed therein. The incompatible filler provides domains in the polyester matrix, each domain having a particular dimension, thus providing a range of dimensions for the domains in the article. To create haze, the dimensions are within the range of from about 380 nm to about 720 nm. Once the range of dimensions is determined, a light absorbent composition can be found which absorbs light at a range of wavelengths that at least substantially covers the range of dimensions of the domains. In doing so, it has been found that the haze of the article can be substantially masked. Method for producing the article and for masking the haze are also provided.
Abstract:
A polycarbonate containing composition comprising a peak melt viscosity of at least 8,000 poise when measured using a parallel plate melt rheology test at a heating rate of 10° C./min at a temperature of between about 350° C. to about 450° C., and wherein a molded article of the composition has a UL 94 VO rating at a thickness of 1.0 mm, 1.5 mm, 2.0 mm, or between 1.0 mm and 2.0 mm is disclosed.
Abstract:
A transparent article includes a continuous polyester matrix having at least one incompatible filler dispersed therein. The incompatible filler provides domains in the polyester matrix, each domain having a particular dimension, thus providing a range of dimensions for the domains in the article. To create haze, the dimensions are within the range of from about 380 nm to about 720 nm. Once the range of dimensions is determined, a light absorbent composition can be found which absorbs light at a range of wavelengths that at least substantially covers the range of dimensions of the domains. In doing so, it has been found that the haze of the article can be substantially masked. Method for producing the article and for masking the haze are also provided.
Abstract:
A transparent article includes a continuous polyester matrix having at least one incompatible filler dispersed therein. The incompatible filler provides domains in the polyester matrix, each domain having a particular dimension, thus providing a range of dimensions for the domains in the article. To create haze, the dimensions are within the range of from about 380 nm to about 720 nm. Once the range of dimensions is determined, a light absorbent composition can be found which absorbs light at a range of wavelengths that at least substantially covers the range of dimensions of the domains. In doing so, it has been found that the haze of the article can be substantially masked. Method for producing the article and for masking the haze are also provided.