Process for separating aniline derivatives
    27.
    发明授权
    Process for separating aniline derivatives 失效
    苯胺衍生物分离方法

    公开(公告)号:US4918232A

    公开(公告)日:1990-04-17

    申请号:US213069

    申请日:1988-06-29

    CPC classification number: C07C209/86

    Abstract: A process for separating from each other aniline and aniline derivatives having different numbers of C atoms bound to the N atoms is disclosed herein, this process being characterized in that a mixture of the substances mentioned is treated in liquid phase with zeolites of the faujasite type at a temperature from 0.degree. C. to 190.degree. C.

    Abstract translation: 本文公开了一种彼此分离的苯胺和与N原子结合的C原子数不同的苯胺衍生物的方法,该方法的特征在于所述物质的混合物用八面沸石沸石沸石处理 温度为0℃至190℃

    Vinylsilicone pastes for dental impression
    29.
    发明授权
    Vinylsilicone pastes for dental impression 失效
    乙烯基硅胶用于牙科印象

    公开(公告)号:US4359565A

    公开(公告)日:1982-11-16

    申请号:US288076

    申请日:1981-07-29

    CPC classification number: A61K6/10 G02B6/4492

    Abstract: In a polysiloxane-based dental composition which crosslinks by an addition reaction and hardens at room temperature, the composition comprising(a) an organopolysiloxane with at least two vinyl groups in the molecule,(b) an organohydridopolysiloxane,(c) a catalyst to accelerate the addition reaction, and(d) a hydrophobic filler, the improvement which comprises including therein(e) an aluminosilicate containing finely divided palladium. This removes any by-product hydrogen and results in a smoother surface on any plaster of Paris moldings made from the hardened composition.

    Abstract translation: 在通过加成反应交联并在室温下硬化的基于聚硅氧烷的牙科用组合物中,所述组合物包含(a)分子中具有至少两个乙烯基的有机聚硅氧烷,(b)有机氢聚硅氧烷,(c)加速催化剂 加成反应,和(d)疏水性填料,其改进包括(e)含有细碎钯的硅铝酸盐。 这可以除去任何副产物氢,并在由硬化组合物制成的任何石膏巴黎模塑制品上形成更平滑的表面。

    Process for the preparation of zeolite A from kaolin
    30.
    发明授权
    Process for the preparation of zeolite A from kaolin 失效
    从高岭土制备沸石A的方法

    公开(公告)号:US4271130A

    公开(公告)日:1981-06-02

    申请号:US095750

    申请日:1979-11-19

    CPC classification number: C04B33/10 C01B33/283 C01B39/02 C11D3/128 Y10S423/24

    Abstract: The invention provides a process for the production of zeolite A from kaolin by conversion of the kaolin into meta-kaolin followed by reaction of the meta-kaolin in an aqueous alkaline medium, wherein the conversion of the kaolin into the meta-kaolin is conducted at temperatures of between 700.degree. and 950.degree. C. in the presence of alkaline earth compounds and optionally in the presence of uncolored halides and/or halogens, wherein the process may be conducted under reducing conditions and in the presence of alkali metal compounds.

    Abstract translation: 本发明提供了一种从高岭土生产沸石A的方法,该方法是通过将高岭土转化为高高岭土,随后在含水碱性介质中使高岭土反应,其中高岭土转化为偏高岭土是在 在碱土金属化合物的存在下,任选地在未着色的卤化物和/或卤素的存在下,温度在700-950℃之间,其中该方法可以在还原条件下和在碱金属化合物的存在下进行。