Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 0.5 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 30.0 to 40.0 wt-%, a comonomer content in the range of more than 7.5 to 12.0 wt.-%, wherein further the comonomer content of xylene cold soluble (XCS) fraction of the propylene copolymer is in the range of 16.0 to 28.0 wt.-%.
Abstract:
The present invention is directed to a layer of an electrical device a photovoltaic module comprising at least one photovoltaic element and at least one layer comprising a polypropylene composition and to the use of a polypropylene composition for producing at least one layer of an element of a photovoltaic module.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 1.0 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 7.5 to 12.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 16.0 to 28.0 wt.-% and an intrinsic viscosity (IV) in the range of more than 1.2 to below 2.5 dl/g.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 0.8 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 4.5 to 10.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 12.0 to 22.0 wt.-% and the xylene cold insoluble (XCI) fraction of the propylene copolymer has a Mw/Mn of more than 4.9 to 10.0.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 1.0 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 7.5 to 12.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 16.0 to 28.0 wt.-% and an intrinsic viscosity (IV) in the range of more than 1.2 to below 2.5 dl/g.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 0.8 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 4.5 to 10.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 12.0 to 22.0 wt.-% and the xylene cold insoluble (XCI) fraction of the propylene copolymer has a Mw/Mn of more than 4.9 to 10.0.
Abstract:
A process for the preparation of a polypropylene in a sequential polymerization process including at least two polymerization reactors connected in series. The polymerization takes place in the presence of a Ziegler-Natta catalyst, and said Ziegler-Natta catalyst includes (a) a pro-catalyst that has a compound of a transition metal, a compound of a metal which metal is selected from one of the groups 1 to 3 of the periodic table (IUPAC), and an internal electron donor, (b) a co-catalyst, and (c) an external donor. The ratio of catalyst feed rate to propylene feed rate in the first polymerization reactor is 1.0 to 4.5 q/t.
Abstract:
Polyolefin composition comprising a heterophasic propylene copolymer and glass material, wherein said heterophasic propylene copolymer has • a xylene cold soluble fraction in the range of 25 to 50 wt.-%, and • a comonomer content in the range of 10.0 to 15.0 wt.-%, wherein further the xylene cold soluble fraction of the heterophasic propylene copolymer has a comonomer content in the range of 20 to 30 wt.-% and the polyolefin composition has a melt flow rate MFR2 (230° C.) of 2.0 to 15.0 g/10 min.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of 2.5 to 12.0 g/10 min, a xylene cold soluble content (XCS) in the range of 20.0 to 45.0 wt.-%, a comonomer content in the range of more than 7.5 to 12.0 wt.-%, wherein further the comonomer content of xylene cold soluble (XCS) fraction of the propylene copolymer is in the range of 16.0 to 28.0 wt.-%.
Abstract:
The present invention is directed to a heterophasic propylene copolymer (HECO), a polyolefin composition (PO) comprising the heterophasic propylene copolymer (HECO), an automotive article comprising the heterophasic propylene copolymer (HECO) and/or the polyolefin composition (PO) and a process for the preparation of the polyolefin composition (PO) as well as the use of the heterophasic propylene copolymer (HECO) for improving the mechanical properties of a polyolefin composition (PO).