Abstract:
Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of layer DOL of about 130 μm up to about 175 μm or, alternatively, to a depth of compression (DOC) in a range from about 90 μm to about 120 μm within the article. The compressive layer has a stress profile that includes a first substantially linear portion extending from a relatively shallow depth to the DOL or DOC and a second portion extending from the surface to the shallow depth. The second portion is substantially linear at a depth from 0 μm to 5 μm and has a steeper slope than that of the first portion of the profile. Methods of achieving such stress profiles are also described.
Abstract:
Disclosed are alkali aluminosilicate glasses having unexpected resistance to indentation cracking. The glasses obtain this high resistance as a result of a high level of surface compression accompanied by a shallow depth of layer. The advantaged glasses show greater resistance to radial crack formation from Vickers indentation than glasses with the same compressive stress, but higher depths of layer.
Abstract:
Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of compression DOC of at least about 125 μm within the glass article. The compressive stress profile includes a single linear segment or portion extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile may include an additional portion extending from the surface to a relatively shallow depth and the linear portion extending from the shallow depth to the depth of compression.
Abstract:
Disclosed are device display screen protectors comprising a first strengthened substrate sized to cover a display screen of an electronic device, the first strengthened substrate having a central tension value in the range greater than 0 MPa and less than 20 MPa, a surface having a Knoop lateral cracking scratch threshold of at least 3 N.
Abstract:
Disclosed are device display screen protectors comprising a first strengthened substrate sized to cover a display screen of an electronic device, the first strengthened substrate having a central tension value in the range greater than 0 MPa and less than 20 MPa, a surface having a Knoop lateral cracking scratch threshold of at least 3 N.
Abstract:
Disclosed are device display screen protectors comprising a first strengthened substrate sized to cover a display screen of an electronic device, the first strengthened substrate having a central tension value in the range greater than 0 MPa and less than 20 MPa, a surface having a Knoop lateral cracking scratch threshold of at least 3 N.
Abstract:
Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and a peak load at failure of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.
Abstract:
The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball test and a peak load at failure of at least 10 kgf as determined by abraded ring-on-ring testing.
Abstract:
Disclosed are device display screen protectors comprising a first strengthened substrate sized to cover a display screen of an electronic device, the first strengthened substrate having a central tension value in the range greater than 0 MPa and less than 20 MPa, a surface having a Knoop lateral cracking scratch threshold of at least 3 N.
Abstract:
Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and an equibiaxial flexural strength of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.