ELECTRODE FOR ELECTROCHEMICAL DEVICE AND ELECTROCHEMICAL DEVICE

    公开(公告)号:US20240154088A1

    公开(公告)日:2024-05-09

    申请号:US18549588

    申请日:2022-03-30

    Abstract: Provided is an electrode for an electrochemical device that has excellent flexibility, suppressed warping, and reduced interfacial resistance between an electrode mixed material layer and a current collector and that can cause an electrochemical device to display excellent high-temperature storage characteristics. The electrode includes a current collector and an electrode mixed material layer formed on the current collector. The current collector is formed of either or both of aluminum and an aluminum alloy, has a thickness of not less than 5 μm and less than 15 μm, and has a breaking elongation of 10% to 40%. The electrode mixed material layer contains electrode active material particles, a conductive material including a fibrous carbon material, and a binder and has a mass per unit area of 21 mg/cm2 to 30 mg/cm2, a storage modulus of 0.1 GPa to 2.2 GPa, and a loss modulus of 0.01 GPa to 0.04 GPa.

    LAMINATE FOR NON-AQUEOUS SECONDARY BATTERY, NON-AQUEOUS SECONDARY BATTERY, AND NON-AQUEOUS SECONDARY BATTERY PRODUCTION METHOD

    公开(公告)号:US20200176778A1

    公开(公告)日:2020-06-04

    申请号:US16629563

    申请日:2018-07-05

    Abstract: Provided is a laminate for a non-aqueous secondary battery including a substrate and a functional layer that is well adhered thereto. The laminate includes a substrate and a functional layer at one or both sides of the substrate. The functional layer contains non-conductive particles and a binder including a polymer A that includes a fluorine-containing monomer unit. The amount of polymer A in a region up to 20% of thickness of the functional layer from a substrate-side surface thereof is more than 20% and not more than 40% of the total amount of polymer A in the functional layer, and the amount of polymer A in a region up to 20% of thickness of the functional layer from an opposite surface thereof relative to the substrate-side surface is more than 20% and not more than 40% of the total amount of polymer A in the functional layer.

Patent Agency Ranking