公开(公告)号:US20180022636A1
公开(公告)日:2018-01-25
申请号:US15692433
申请日:2017-08-31
Applicant: Corning Incorporated
Inventor: Jonathan David Pesansky , Chandan Kumar Saha , Trevor E. Wilantewicz
CPC classification number: C03C3/097 , C03C3/083 , C03C3/085 , C03C3/087 , C03C3/091 , C03C3/093 , C03C21/002 , Y10T29/49863 , Y10T428/315
Abstract: Disclosed are alkali aluminosilicate glasses having unexpected resistance to indentation cracking. The glasses obtain this high resistance as a result of a high level of surface compression accompanied by a shallow depth of layer. The advantaged glasses show greater resistance to radial crack formation from Vickers indentation than glasses with the same compressive stress, but higher depths of layer.
-
公开(公告)号:US09783452B2
公开(公告)日:2017-10-10
申请号:US14547456
申请日:2014-11-19
Applicant: Corning Incorporated
Inventor: Jonathan David Pesansky , Chandan Kumar Saha , Trevor E Wilantewicz
CPC classification number: C03C3/097 , C03C3/083 , C03C3/085 , C03C3/087 , C03C3/091 , C03C3/093 , C03C21/002 , Y10T29/49863 , Y10T428/315
Abstract: Disclosed are alkali aluminosilicate glasses having unexpected resistance to indentation cracking. The glasses obtain this high resistance as a result of a high level of surface compression accompanied by a shallow depth of layer. The advantaged glasses show greater resistance to radial crack formation from Vickers indentation than glasses with the same compressive stress, but higher depths of layer.
-
公开(公告)号:US20170036952A1
公开(公告)日:2017-02-09
申请号:US15332504
申请日:2016-10-24
Applicant: CORNING INCORPORATED
Inventor: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
CPC classification number: C03C21/002 , C03C3/04 , C03C3/085 , C03C3/087 , C03C3/091 , C03C3/093 , C03C3/095 , C03C3/097 , C03C4/18 , C03C21/00 , C03C2204/00 , G06F1/1637 , G06F2200/1634 , H04B1/3827 , Y10T428/315
Abstract: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and an equibiaxial flexural strength of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.
Abstract translation: 提供了具有从制品表面延伸到制品内至少约45μm深度的至少一个深度压缩层的化学强化的玻璃制品。 在一个实施例中,压缩应力分布包括从表面延伸到压缩DOC深度的单个线性段。 或者,压缩应力分布包括两个线性部分:第一部分从表面延伸到相对较浅的深度并且具有陡峭的斜率; 以及从浅深度延伸到压缩深度的第二部分。 加强玻璃在倒置球滴试验中从80厘米的高度下降至60厘米的存活率,并且通过磨损的环上环试验确定的至少10kgf的等轴弯曲强度。 还描述了实现这种应力分布的方法。
-
公开(公告)号:US09487434B2
公开(公告)日:2016-11-08
申请号:US15158167
申请日:2016-05-18
Applicant: CORNING INCORPORATED
Inventor: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
CPC classification number: C03C21/002 , C03C3/04 , C03C3/085 , C03C3/087 , C03C3/091 , C03C3/093 , C03C3/095 , C03C3/097 , C03C4/18 , C03C21/00 , C03C2204/00 , G06F1/1637 , G06F2200/1634 , H04B1/3827 , Y10T428/315
Abstract: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and an equibiaxial flexural strength of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.
-
公开(公告)号:US20150368153A1
公开(公告)日:2015-12-24
申请号:US14740896
申请日:2015-06-16
Applicant: Corning Incorporated
CPC classification number: C03C21/002 , C03C3/091 , C03C3/093 , C03C3/097 , Y10T428/315
Abstract: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. Methods of achieving such stress profiles are also described.
Abstract translation: 提供了具有从制品表面延伸到制品内至少约45μm深度的至少一个深度压缩层的化学强化的玻璃制品。 在一个实施例中,压缩应力分布包括从表面延伸到压缩DOC深度的单个线性段。 或者,压缩应力分布包括两个线性部分:第一部分从表面延伸到相对较浅的深度并且具有陡峭的斜率; 以及从浅深度延伸到压缩深度的第二部分。 还描述了实现这种应力分布的方法。
-
公开(公告)号:US20150239776A1
公开(公告)日:2015-08-27
申请号:US14530155
申请日:2014-10-31
Applicant: Corning Incorporated
Inventor: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
CPC classification number: C03C21/002 , C03C3/04 , C03C3/085 , C03C3/087 , C03C3/091 , C03C3/093 , C03C3/095 , C03C3/097 , C03C4/18 , C03C21/00 , C03C2204/00 , G06F1/1637 , G06F2200/1634 , H04B1/3827 , Y10T428/315
Abstract: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and an equibiaxial flexural strength of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.
-
-
-
-
-