Upgrading of bauxites, bauxitic clays, and aluminum mineral bearing clays
    41.
    发明授权
    Upgrading of bauxites, bauxitic clays, and aluminum mineral bearing clays 失效
    铝土矿,铝土矿粘土和铝矿物轴承粘土的升级

    公开(公告)号:US4303204A

    公开(公告)日:1981-12-01

    申请号:US201279

    申请日:1980-10-27

    Applicant: David Weston

    Inventor: David Weston

    Abstract: A process for the upgrading of aluminum mineral bearing raw materials by using at least three beneficiation treatment stages consisting of dispersion of a pulp of the material in specific pH ranges, screening in specific mesh sizes, and using at least one stage of high intensity magnetic separation.

    Abstract translation: 一种通过使用至少三个选矿处理阶段来升级含铝矿物轴承原料的方法,所述选矿处理阶段包括在特定pH范围内分散材料的纸浆,以特定筛目尺寸筛选,并使用至少一个高强度磁选分离 。

    Composition comprising a pulverized purified substance, water and a
dispersing agent, and a method for preparing the composition
    43.
    发明授权
    Composition comprising a pulverized purified substance, water and a dispersing agent, and a method for preparing the composition 失效
    包含粉碎的纯化物质,水和分散剂的组合物及其制备方法

    公开(公告)号:US4217109A

    公开(公告)日:1980-08-12

    申请号:US908497

    申请日:1978-05-23

    Abstract: A composition consisting of carbon powder, water and a dispersing agent. The particle size of the carbon powder is less than 100 .mu.m, preferably less than 40 .mu.m. The composition is obtained by preparing a mixture of about 1-20% by weight, preferably about 10% by weight, of carbonaceous powder, water and 0.02-4% by weight of dispersing agent. The dispersing agent is selected preferably from polyelectrolytes, such as alkali metal and ammonium salts of polycarboxylic acids, and polyphosphates. These substances possess the property of charging the powder particles of carbon and the impurity particles in a different degree. This different charging is utilized to separate impurity particles from carbon particles, whereupon the purified composition is suitably dehydrated to attain an increased carbon powder concentration of, for instance, 50-80% by weight.

    Abstract translation: 由碳粉,水和分散剂组成的组合物。 碳粉末的粒径小于100微米,优选小于40微米。 该组合物通过制备约1-20重量%,优选约10重量%的碳质粉末,水和0.02-4重量%的分散剂的混合物而获得。 分散剂优选选自聚电解质,例如多元羧酸的碱金属盐和铵盐,以及聚磷酸盐。 这些物质具有以不同的程度对碳和杂质颗粒的粉末颗粒充电的性质。 使用这种不同的装料将杂质颗粒与碳颗粒分离,由此将纯化的组合物适当地脱水以获得例如50-80重量%的增加的碳粉浓度。

    Concentration of spodumene using flotation
    44.
    发明授权
    Concentration of spodumene using flotation 失效
    使用浮游生物的浓度

    公开(公告)号:US3710934A

    公开(公告)日:1973-01-16

    申请号:US3710934D

    申请日:1970-06-29

    Inventor: WYMAN R

    Abstract: A method of concentrating and recovering spodumene from an aqueous pulp or slurry by conditioning the pulp with an aliphatic primary beta-amine having from seven to 15 carbon atoms (preferably as a soluble acid salt), subjecting to flotation at a pH of about 8-10 to float off the impurities, and recovering the spodumene concentrate as residue.

    Abstract translation: 通过用具有7至15个碳原子的脂肪族伯胺(优选作为可溶性酸盐)调节纸浆,从水性纸浆或浆料中浓缩和回收锂辉石的方法,在pH约为8- 10漂浮杂质,并回收锂辉石浓缩物作为残留物。