Abstract:
There is provided a polycarbonate resin composition containing aluminum oxide nanoparticles and being capable of showing good moldability and retention heat stability and combining high transparency and dimensional stability with excellent mechanical properties. The polycarbonate resin composition is characterized by containing an organic acid and aluminum oxide and in that: the resin composition has a melt mass flow rate of 11 g/10 min or higher as measured according to JIS K 7210 under the conditions of a temperature of 280° C., a nominal load of 2.16 Kg and a nozzle dimension L/D of 8/2; and a No. 2 dumbbell-shaped specimen according to JIS K 7113 formed by heat-press molding the resin composition into a film of 0.2 mm in thickness and cutting the film has a breaking stress of 8 MPa or higher as measured under the conditions of a temperature of 23° C., a humidity of 50% RH and a tensile rate of 50 mm/min. The organic acid is preferably an organic sulfonic acid having a carbon number of 8 or greater, more preferably the one containing an aromatic ring in the molecule.
Abstract translation:提供含有氧化铝纳米颗粒的聚碳酸酯树脂组合物,并且能够显示出良好的成型性和保持热稳定性,并且结合高透明度和尺寸稳定性以及优异的机械性能。 聚碳酸酯树脂组合物的特征在于含有有机酸和氧化铝,其中:树脂组合物在温度为280℃的条件下,根据JIS K 7210测定的熔体质量流量为11g / 10min以上 公称负荷2.16千克,喷嘴尺寸L / D为8/2; 和根据JIS K 7113的2号哑铃形样品通过将树脂组合物热压成型为0.2mm厚的膜而形成,并且切割该膜的断裂应力为8MPa以上, 温度为23℃,湿度为50%RH,拉伸速度为50mm / min。 有机酸优选为碳数为8以上的有机磺酸,更优选分子中含有芳香环的有机磺酸。
Abstract:
The present invention provides a method for producing a liquid crystal polyester composition, the method comprising feeding a liquid crystal polyester and a polyhydric alcohol fatty acid ester into an extruder having a vent portion, followed by melt-kneading in a state where the degree of decompression of the vent portion is −0.06 MPa or less in terms of a gauge pressure. The composition obtained by the method can provide a molded article having a thin wall portion and complicated shape.
Abstract:
The present invention relates to a method for producing a conductive masterbatch containing a polyamide resin and a carbonaceous filler. The present invention provides a method for producing a conductive masterbatch which can suppress an increase in resin temperature during extrusion, formation of die drips, and strand breakage and can also significantly increase the output of extruding. The method is achieved by the steps of feeding the carbonaceous filler to a molten first polyamide to melt-knead them together and then feeding a second polyamide to the resulting melt-kneaded product to further melt-knead the second polyamide, the carbonaceous filler, and the first polyamide.
Abstract:
The present invention provides a method of preparing a transparent polymer material, the method comprising steps i) and ii) in any order, the steps consisting in: i) mixing: mineral nanoparticles having a form factor strictly greater than 1.0; and a polymer matrix comprising a quantity of at least 80% by weight of a polycarbonate (PC) first thermoplastic polymer and of a second transparent thermoplastic polymer other than the first thermoplastic polymer, in order to obtain a mixture; and ii) heating the polymer matrix to the molten state, on its own or in the mixture; to obtain the transparent, polymer material, the mixture of step i) comprising a quantity of mineral nanoparticles having a form factor strictly greater than 1.0 that is strictly less than 5% by weight.
Abstract:
A method for manufacturing black plastic article capable of transmitting infrared ray, which includes mixing a black colorant, produced by mixing several transparent colorants of different color, into a transparent resin used as support, and processing the resulting mixture to manufacture a black plastic article. Said black plastic article is capable of absorbing visible light and transmitting infrared ray, and may be used in combination with an infrared region-sensitive CCD camera. The infrared region-sensitive CCD camera can take photos of the subject in a long distance through the black plastic article, if sufficient infrared ray from a subject may penetrate the black plastic article.
Abstract:
Compartmentalized chips of at least two chemically similar crystallizable thermoplastic polymers each having a different intrinsic viscosity placed in separate zones are disclosed. These compartmentalized chips exhibit thermal characteristics that are different from the traditional technique of homogeneously combining the two materials into the chip. These compartmentalized chips in their amorphous, crystalline and solid phase polymerized forms exhibit a longer crystallization half time than the homogeneous mixture, thus permitting faster injection cycle times.
Abstract:
There is provided a method for producing resinous particles, containing: melting a mixture containing a binder resin and at least one additive having a melting point lower than T1/2 of the binder resin so as to prepare a molten material; atomizing resinous particles from the molten material in an atmosphere having a temperature higher than Tg of the binder resin and lower than 3 times of T1/2 of the binder resin; retaining the resinous particles in an atmosphere having a temperature higher than Tg of the binder resin, and lower than 1.5 times of T1/2 of the binder resin for 1 s to 15 s; and cooling and solidifying the resinous particles. There is also provided a method for producing resinous particles containing: melting the mixture so as to prepare a molten material; increasing a specific surface of the molten material in an atmosphere having a temperature higher than Tg of the binder resin, and lower than 3 times of T1/2 of the binder resin, so as to form a precursor; retaining the precursor in an atmosphere having a temperature higher than Tg of the binder resin, and lower than 1.5 times of T1/2 of the binder resin for 1 ms to 10 ms; cooling and solidifying the precursor; and atomizing resinous particles from the precursor.
Abstract:
A pulverized thermoplastic resin product such as a pulverized thermoplastic product containing a black pigment, a mixture of a pulverized thermoplastic product containing a colored pigment and a pulverized thermoplastic product containing a colored pigment, or a pulverized thermoplastic product containing two or more different colored pigments can be converted into colored reclaimed resin particles by a method comprising the steps of mixing the pulverized resin product with a white pigment and a black pigment, melting the resulting mixture, and converting the molten mixture into solid particles. The colored reclaimed resin products can be utilized in various field.
Abstract:
A method for producing thermoplastic plastic capable of grasping information concerning the production process even after distribution. In a plurality of production processes including fusion of thermoplastic plastic 90, an information presenting substance 91 is added to the thermoplastic plastic sequentially and dispersed therein in each of the production process, wherein the information presenting substance is associated with information concerning each of the production process and radiates fluorescence upon an irradiation of an electromagnetic wave in a specified wavelength region.
Abstract:
There is provided a method for producing a resin composition which is good in dispersability of a biodegradable resin. This method has a first kneading step of kneading (A) a biodegradable resin and (B) a compound that is reactive with the biodegradable resin (A) to produce a resin composition precursor, and a second kneading step of kneading the resin composition precursor and a polyolefin resin (C).