Abstract:
A method of polymerizing an olefin using a combination of a Ziegler-Natta catalyst and an unsupported molecular catalyst in a same reactor at the same time to give a polyolefin product, and the polyolefin product made by the method. Also, methods of preparing the combination of (pro)catalysts.
Abstract:
The invention provides an ethylene-based polymer comprising the following properties: a) a ZSVR value from 1.2 to 2.6, b) a MWD from 1.5 to 2.8, and c) a tan delta (0.1 rad/s; 190 C) from 5.0 to 50.
Abstract:
Disclosed herein is a cast film comprising a polyethylene composition comprising the reaction product of ethylene and optionally one or more alpha-olefin comonomers, wherein said polyethylene composition is characterized by the following properties: a melt index, I2, measured according to ASTM D1238 (2.16 kg, 190° C.), of from 1 to 20 g/10 min; a density (measured according to ASTM D792) of from 0.935 to 0.970 g/cm3; a melt flow ratio, I10/I2, wherein I10 is measured according to ASTM D1238 (10 kg, 190° C.) of from 5.5 to 7.0; a molecular weight distribution (Mw/Mn) of from 2.2 to 3.5; and a vinyl unsaturation of greater than 0.12 vinyls per one thousand carbon atoms present in the backbone of the composition.
Abstract:
The invention provides a composition comprising at least the following: a) a first composition comprising at least one first ethylene-based polymer, formed by high pressure, free-radical polymerization, and wherein the first composition comprises the following properties: a melt index (I2) from 1.0 to 15.0 g/10 min, and density from 0.910 to 0.940 g/cc; b) a second composition comprising at least one second ethylene-based polymer, and wherein the second composition comprises the following properties; a melt index (I2) from 1.0 to 1000 g/10 min, a density greater than 0.940 g/cc; wherein the composition comprises the following properties: melt index (I2) from 2.0 to 20.0 g/10 min, and a density from 0.915 to 0.940 g/cc; and wherein the first composition is present in an amount from 65 to 95 wt %, based on the weight of the composition.
Abstract:
An ethylene/α-olefin copolymer comprising units derived from ethylene; and units derived from at least one α-olefin; wherein the ethylene/α-olefin copolymer has a density in the range of from 0.90 to 0.94 g/cc; a melt index (I2) in the range of from 0.05 to 50 dg/min; an Mw/Mn of from 3 to 5; and from 300 to 500 vinyl unsaturations per 1,000,000 carbon atoms in the ethylene/α-olefin copolymer is provided. Also provided is a process for producing an ethylene/α-olefin copolymer comprising: (1) polymerizing ethylene and one or more α-olefins in a polymerization reactor; (2) thereby producing an enhanced melt strength ethylene/α-olefin copolymer having from 300 to 500 vinyl unsaturation units per 1,000,000 carbon atoms, a density in the range of from 0.90 to 0.94 g/cc; a melt index (I2) in the range of from 0.05 to 50 dg/min; and a Mw/Mn of from 3 to 5.
Abstract:
The instant invention provides a polymerization process for producing ethylene based polymers.In one embodiment, the instant invention provides a polymerization process for producing ethylene based polymers comprising: polymerizing ethylene with optionally one or more α-olefins in the presence of one or more first catalyst systems and optionally one or more second catalyst systems in in a dual reator system or a multiple reactor system, wherein first catalyst system comprises; (a) one ore more procatalysts comprising a metal-ligand complex of formula (I):
Abstract:
A polyethylene composition comprising the reaction product of ethylene and optionally one or more alpha-olefin comonomers in the presence of a catalyst composition comprising a multi-metallic procatalyst via solution polymerization; wherein said polyethylene composition is characterized by one or more of the following properties: a melt index, I2, measured according to ASTM D 1238 (2.16 kg @190° C.), of from 0.9 to 5 g/10 min; density (measured according to ASTM D792) from 0.910 to 0.935 g/cc; a melt flow ratio, I10/I2, wherein I10 is measured according to ASTM D1238 (10 kg @ 190° C.), of from 6 to 7.4; and molecular weight distribution (Mw/Mn) of from 2.5 to 3.5 is provided.
Abstract:
An ethylene/α-olefin copolymer comprising units derived from ethylene; and units derived from at least one α-olefin; wherein the ethylene/α-olefin copolymer has a density in the range of from 0.90 to 0.94 g/cc; a melt index (I2) in the range of from 0.05 to 50 dg/min; an Mw/Mn of from 3 to 5; and from 300 to 500 vinyl unsaturations per 1,000,000 carbon atoms in the ethylene/α-olefin copolymer is provided. Also provided is a process for producing an ethylene/α-olefin copolymer comprising: (1) polymerizing ethylene and one or more α-olefins in a polymerization reactor; (2) thereby producing an enhanced melt strength ethylene/α-olefin copolymer having from 300 to 500 vinyl unsaturation units per 1,000,000 carbon atoms, a density in the range of from 0.90 to 0.94 g/cc; a melt index (I2) in the range of from 0.05 to 50 dg/min; and a Mw/Mn of from 3 to 5.
Abstract:
The instant invention provides procatalysts and catalyst systems for olefin polymerization, olefin based polymers polymerized therewith, and process for producing the same. In one embodiment, the instant invention provides a procatalyst comprising a metal-ligand complex of formula (I).
Abstract:
The instant invention provides a polyethylene blend-composition suitable for blown films, and films made therefrom. The polyethylene blend-composition suitable for blown films comprises the melt blending product of: (a) from 0.5 to 4 percent by weight of a low density polyethylene having a density in the range of from 0.915 to 0.935 g/cm3, and a melt index (I2) in the range of from greater than 0.8 to less than or equal to 5 g/10 minutes, and a molecular weight distribution (Mw/Mn) in the range of from 6 to 10; (b) 90 percent or greater by weight of an ethylene/α-olefin interpolymer composition, wherein ethylene/α-olefin interpolymer composition has a Comonomer Distribution Constant (CDC) in the range of from 75 to 200, a vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of the ethylene/α-olefin interpolymer composition; a zero shear viscosity ratio (ZSVR) in the range from 2 to 20; a density in the range of from 0.903 to 0.950 g/cm3, a melt index (12) in a range of from 0.1 to 5 g/10 minutes, a molecular weight distribution (Mw/Mn) in the range of from 1.8 to 3.5; (c) optionally a hydrotalcite based neutralizing agent; (d) optionally one or more nucleating agents; (e) and optionally one or more antioxidants.