公开(公告)号:US12084385B2
公开(公告)日:2024-09-10
申请号:US17915412
申请日:2021-04-15
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Monica Galvan , Claudio Cavalieri , Gisella Biondini , Vincent Baudier
IPC: C04B26/26 , C04B24/26 , D06N5/00 , C04B111/00
CPC classification number: C04B26/26 , C04B24/2611 , C04B24/2688 , D06N5/003 , C04B2111/00586
Abstract: A mixture made from or containing
T1) from 99 wt % to 75 wt % of bitumen, and
T2) from 1 wt % to 25 wt % of a polymer composition made from or containing
A) 5-35% by weight of a propylene homopolymer;
B) 20-50% by weight of an ethylene homopolymer; and
C) 30-60% by weight of a terpolymer of ethylene, propylene, and 1-butene.-
公开(公告)号:US12012527B2
公开(公告)日:2024-06-18
申请号:US17261100
申请日:2019-07-15
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Roberta Marchini , Silvia Guerra , Stefano Pasquali , Ankur Rastogi , Stefano Spataro
IPC: C09J123/20 , C08L23/20 , C09J123/08 , C08L23/08
CPC classification number: C09J123/20 , C08L23/0815 , C08L23/20 , C09J123/0815
Abstract: A polyolefin-based hot melt adhesive composition made from or containing
(A) 25-75 wt. % of a copolymer of butene-1 with a Melt Flow Rate, measured according to ISO 1133 (190° C., 2.16 kg), higher than 1500; and
(B) 75-25 wt. % of at least one additional component selected from the group consisting of waxes, resins, plasticizers, additional polymers and mixtures thereof,
wherein the amounts of A) and B) are referred to the total weight of A)+B).-
公开(公告)号:US20240182388A1
公开(公告)日:2024-06-06
申请号:US18526332
申请日:2023-12-01
Applicant: Basell Poliolefine Italia S.r.l.
Inventor: Sandor Nagy , David S. Mannel , Natalia Nagy , Amy D. Rose , George R. Horvat , Larry W. Arndt , David W. Leyshon , Xueyong Yang , Barbara Kimmich
IPC: C07C29/17
CPC classification number: C07C29/172 , C07C2527/051
Abstract: Processes for conversion of propylene polyol feed into useful petrochemical products, including olefin monomers, are described. Such processes comprise: adding a feed stream comprising one or more propylene polyols to a dehydration cleavage reaction zone in the presence of a dehydration cleavage catalyst and reacting at a pressure and temperature sufficient to form a product stream comprising propionaldehyde, a dioxolane component, and a dioxane component; and adding the product stream and hydrogen to a dehydration reaction zone in the presence of a hydrogenation catalyst to form and reacting at a pressure and temperature sufficient to form a second product stream comprising a propanol component. The second product can be added to a dehydration reaction zone in the presence of a dehydration catalyst and reacted at a pressure and temperature sufficient to form a third product stream comprising propylene.
-
公开(公告)号:US11873365B2
公开(公告)日:2024-01-16
申请号:US17620968
申请日:2020-06-24
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Alessandro Mignogna , Dario Liguori , Giampiero Morini
CPC classification number: C08F4/6421 , C08F10/06
Abstract: A solid catalyst component for the polymerization of olefins made from or containing Mg, Ti and an electron donor of formula (I)
where the R1 and R5 groups, equal to or different from each other, are selected from C1-C15 hydrocarbon groups, R2 group is selected from C2-C10 hydrocarbon groups, R3 to R4 groups, independently, are selected from hydrogen or C1-C20 hydrocarbon groups, optionally fused together to form one or more cycles, with the proviso that at least one of R3 to R4 groups is a C1-C20 alkyl group.-
公开(公告)号:US11872545B2
公开(公告)日:2024-01-16
申请号:US17541474
申请日:2021-12-03
Applicant: Basell Poliolefine Italia S.r.l.
Inventor: Sandor Nagy , Daniel F. White , Christopher D. Smith , David L. Ramage , Diego Brita , Noel C. Hallinan
CPC classification number: B01J29/7007 , B01J27/16 , B01J29/084 , B01J29/40 , C08J11/16 , C08J2323/06 , C08J2323/12
Abstract: Catalytic compositions for depolymerizing polyolefin-based waste material into useful petrochemical products and methods of use are described. The compositions are a composite of at least one zeolite catalyst with one or more co-catalyst(s) that is a solid inorganic material. These composite catalysts, along with heat, are used to both increase the depolymerization reaction rate of the feed streams and suppress poisoning effects of non-polyolefin polymers that may be present. This results in a shorter residence time in the depolymerization unit and more efficient process.
-
公开(公告)号:US11840775B2
公开(公告)日:2023-12-12
申请号:US17617325
申请日:2020-05-26
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Roberto De Palo , Davide Tartari , Monica Galvan , Claudio Cavalieri , Isabella Maria Vittoria Camurati
IPC: D01F6/30 , C08F210/06 , D01F8/06
CPC classification number: D01F6/30 , C08F210/06 , D01F8/06 , C08F2800/20
Abstract: A fiber of a propylene ethylene copolymer having:
i) xylene soluble fraction at 25° C. ranging from 14 wt % to 27 wt %;
ii) intrinsic viscosity of the fraction soluble in xylene at 25° C. ranging from 1.0 to 2.4 dl/g;
iii) melt flow rate, MFR, ranging from 12 g/10 min to 60 g/10 min;
iv) an ethylene derived units content ranging from 5.0 wt % to 12.0 wt %;
v) the ethylene derived units content of the fraction insoluble in xylene at 25° C. ranging from 2.5 wt % to 6.0 wt %;
vi) the ethylene derived units content of the fraction soluble in xylene at 25° C. ranging from 15.2. wt % to 30.2 wt %
vii) C13 NMR sequences PEP measured on the fraction insoluble in xylene at 25° C. ranging from 3.5 mol % to 5.5 mol %; and
viii) the C13 NMR sequences PEP measured on the fraction soluble in xylene at 25° C. ranging from 11.0 mol % to 14.2 mol %.-
公开(公告)号:US11834534B2
公开(公告)日:2023-12-05
申请号:US17268653
申请日:2019-08-12
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Gianpiero Ferraro , Gianni Vitale , Fabrizio Piemontesi , Benedetta Gaddi , Gianni Collina , Giampiero Morini , Caroline Cathelin , Marco Ciarafoni , Claudio Cavalieri
IPC: C08F210/16 , C08F210/06
CPC classification number: C08F210/06 , C08F210/16
Abstract: A propylene ethylene copolymer having the following features:
an ethylene content of between 1.0 and 4.0% by weight;
a molecular weight distribution (MWD), expressed in terms of Mw/Mn, of greater than 4.0;
a content of xylene soluble fraction (XS) and ethylene content (C2) that fulfills the following relationship:
(C2×1.1)+1.25-
公开(公告)号:US20230383103A1
公开(公告)日:2023-11-30
申请号:US18032778
申请日:2021-10-11
Applicant: Basell Poliolefine Italia S.r.l.
Inventor: Gianluca Musacchi , Roberta Marchini , Fabio Di Pietro
IPC: C08L23/04
CPC classification number: C08L23/04 , C08L2201/52 , C08L2207/066 , C08L2205/02
Abstract: A polyolefin composition made from or containing:
A) from 88% to 99% by weight of an ethylene polymer having MIP of equal to or higher than 5 g/10 min, where MIP is the melt flow index at 190° C. with a load of 5 kg, determined according to 1133-2:2011; and
B) from 1% to 12% by weight of a butene-1 polymer having MIE of equal to or higher than 800 g/10 min., where MIE is the melt flow index at 190° C. with a load of 2.16 kg, determined according to 1133-2:2011;
wherein the amounts of A) and B) are referred to the total weight of A)+B).-
公开(公告)号:US11814759B2
公开(公告)日:2023-11-14
申请号:US17617427
申请日:2020-05-26
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Roberto De Palo , Renaud Lemaire , Jaume Marti Porqueres
IPC: D04H1/4382
CPC classification number: D04H1/43828 , D10B2321/021 , D10B2321/022
Abstract: A skin-core fiber having
a skin of a propylene ethylene copolymer having:
i) xylene soluble fraction from 14 wt % to 27 wt %;
ii) intrinsic viscosity of the fraction soluble in xylene at 25° C. from 1.0 to 2.4 dl/g;
iii) melt flow rate, MFR, from 12 g/10 min to 60 g/10 min;
iv) an ethylene derived units content from 5.0 wt % to 12.0 wt %;
v) the ethylene derived units content of the fraction insoluble in xylene from 2.5 wt % to 6.0 wt %;
vi) the ethylene derived units content of the fraction soluble in xylene ranging from 15.2. wt % to 30.2 wt %;
vii) C13 NMR sequences PEP on the fraction insoluble in xylene from 3.5 mol % to 5.5 mol %; and
viii) C13 NMR sequences PEP on the fraction soluble in xylene from 11.0 mol % to 14.2 mol %; and
a core of a polyethylene having a density between 0.940 g/cm3 to 0.975 g/cm3.-
公开(公告)号:US20230279209A1
公开(公告)日:2023-09-07
申请号:US18019907
申请日:2021-07-01
Applicant: Basell Poliolefine Italia S.r.l.
Inventor: Michele Grazzi , Claudio Cavalieri
IPC: C08L23/14 , B29C48/00 , D03D15/283 , D04H1/4291
CPC classification number: C08L23/142 , B29C48/022 , D03D15/283 , D04H1/4291 , B29K2023/14
Abstract: A polyolefin composition made from or containing:
(A) 10-40% by weight of a copolymer of propylene with hexene-1, is made from or containing 1.0-6.0% by weight, based on the weight of (A), of units deriving from hexene-1 and has a melt flow rate (MFRA) measured according to ISO 1133, 230° C., 2.16 kg ranging from 20 to 60 g/10 min.; and
(B) 60-90% by weight of a copolymer of propylene with an alpha-olefin of formula CH2═CHR, and optionally a diene, wherein R is H or a linear or branched C2-C8 alkyl and wherein the copolymer is made from or containing 20-35% by weight, based on the total weight of (B), of alpha-olefin,
wherein
the polyolefin composition has an amount of fraction soluble in xylene (XS(tot)) at 25° C. equal to or higher than 65% by weight, and
the amounts of (A), (B), and XS(tot) being based on the total weight of (A)+(B).
-
-
-
-
-
-
-
-
-