公开(公告)号:US20180170799A1
公开(公告)日:2018-06-21
申请号:US15898313
申请日:2018-02-16
Applicant: Dyrup A/S
Inventor: Soren Hillebrandt Poulsen , Sverrir Grimur Gunnarsson , Per Moller
IPC: C03C11/00 , C09D5/16 , C09D7/40 , C09C3/06 , C09C1/30 , C09D7/62 , C03C12/02 , C03C17/25 , C08K9/02 , B01J21/08 , B01J37/02 , B01J35/08 , C08K7/28 , B01J35/00
CPC classification number: C03C11/002 , B01J21/08 , B01J35/004 , B01J35/08 , B01J37/0209 , B01J37/0215 , B01J37/0219 , B01J37/0221 , C01P2002/72 , C01P2004/03 , C01P2004/32 , C01P2004/34 , C03C12/02 , C03C17/256 , C03C2217/212 , C03C2217/71 , C03C2218/111 , C03C2218/113 , C08K7/28 , C08K9/02 , C09C1/30 , C09C3/063 , C09D5/16 , C09D5/1606 , C09D5/1687 , C09D7/62 , C09D7/68 , C09D7/69
Abstract: The present invention relates to compositions with self-cleaning properties. More particularly, the invention concerns coatings or paints comprising particles coated with a catalytically active composition. In particular, a self-cleaning coating composition (paint) is provided, comprising micro-sized particles coated with a functional layer, wherein the micro-sized particles are hollow or solid beads, or any combination/ratio of hollow and solid beads, wherein the beads comprise one or more material(s) selected from ceramic material(s); polymeric material(s); cermet material(s); metallic material(s); pigmented material(s); light-absorbing and/or light reflecting material(s); including any combination thereof, wherein said layer is covalently bound to said particles, wherein the photocatalytic layer comprises TiO2 in the crystal form of anatase; and wherein the coating composition (paint) comprises less than 0.1 anatase particles derived/released from the micro-sized beads, determined as weight/weight of released anatase/total amount of anatase. The invention provides paint essentially without presence of unbound anatase crystals which is highly undesired, as it is believed that their presence has a negative influence on essential components of the paint, such as binder, pigment and/or additives and furthermore, anatase may cause eye, skin, and respiratory tract irritation.
-
公开(公告)号:US09932492B2
公开(公告)日:2018-04-03
申请号:US14369155
申请日:2012-12-20
Applicant: Perstorp AB , Dyrup A/S
Inventor: Kent Sorensen , David Lof
IPC: C09D167/08 , C08K3/10 , C08K3/36
CPC classification number: C09D167/08 , C08K3/10 , C08K3/36 , C08K2201/011 , C08K9/06
Abstract: Disclosed is an oxidatively drying alkyd resin composition and a method for preparing said composition. Said composition is obtained by admixing an aqueous silica sol into a substantially 100% alkyd resin being in a liquid state either at ambient temperature or at an elevated temperature. Said silica sol is added in an amount of 0.1-10% by weight calculated as 100% silica on 100% alkyd resin. The use of a said composition is in a further aspect disclosed.
-
公开(公告)号:US20170369734A1
公开(公告)日:2017-12-28
申请号:US15699338
申请日:2017-09-08
Applicant: PERSTORP AB , DYRUP A/S
Inventor: Kent Sörensen , David Löf
IPC: C09D167/08 , C08K3/36 , C08K3/10
CPC classification number: C09D167/08 , C08K3/10 , C08K3/36 , C08K2201/011 , C08K9/06
Abstract: Disclosed is an oxidatively drying alkyd resin composition and a method for preparing said composition. Said composition is obtained by admixing an aqueous silica sol into a substantially 100% alkyd resin being in a liquid state either at ambient temperature or at an elevated temperature. Said silica sol is added in an amount of 0.1-10% by weight calculated as 100% silica on 100% alkyd resin. The use of a said composition is in a further aspect disclosed.
-
公开(公告)号:US20140360408A1
公开(公告)日:2014-12-11
申请号:US14369155
申请日:2012-12-20
Applicant: Perstorp AB , Dyrup A/S
Inventor: Kent Sörensen , David Löf
IPC: C09D167/08
CPC classification number: C09D167/08 , C08K3/10 , C08K3/36 , C08K2201/011 , C08K9/06
Abstract: Disclosed is an oxidatively drying alkyd resin composition and a method for preparing said composition. Said composition is obtained by admixing an aqueous silica sol into a substantially 100% alkyd resin being in a liquid state either at ambient temperature or at an elevated temperature. Said silica sol is added in an amount of 0.1-10% by weight calculated as 100% silica on 100% alkyd resin. The use of a said composition is in a further aspect disclosed.
Abstract translation: 公开了一种氧化干燥的醇酸树脂组合物及其制备方法。 所述组合物通过将水性二氧化硅溶胶混合到在环境温度或升高的温度下处于液态的基本上100%的醇酸树脂中而获得。 所述二氧化硅溶胶的添加量为按100%二氧化硅计算的0.1-10重量%的100%醇酸树脂。 所述组合物的使用在公开的另一方面。
-
-
-