Abstract:
Polymer of formula (1) bearing an alkoxysilane end group: in which: is a double or single bond; each of R1, R2, R3, R4, R5 and R6 is H, a halo, an alkoxycarbonyl or an alkyl, m and p are each from 0 to 5, each of R and R′ is an alkyl, Z is an alkylene, optionally interrupted with COO, q is 0 or 1, r is 0, 1 or 2, and n is such that the number-average molar mass of the polymer (1) is from 400 to 50 000 g/mol, and the polydispersity index of the polymer (1) is from 1.0 to 2.0. Preparation by ring-opening metathesis polymerization.Use as an adhesion promoter or a reactive plasticizer.
Abstract:
1) Hydrocarbon polymer having two azlactone end groups F1 is formula (IIa) and F2 is formula (IIb): g and d are 0, 1, 2 or 3; R14 and R15 are C1-C4 or a cyclohexyl radical; R1 to R12 represents hydrogen or alkyl with 1 to 22 carbon atoms; x and y are integers, x+y is 0 to 2; R13 is oxygen or sulphur or divalent —CH2— n1, n2, m, p1 and p2 are an integer or equal to 0 and such that the molecular weight Mn of the polymer of formula (I) is between 400 and 100 000 g/mol; a process for preparation of the polymer; and use as adhesive in mixture with an amino compound with at least two amine groups.
Abstract:
1) Hydrocarbon-based copolymer comprising two end groups preceded by an ester function and chosen from a 2-oxo-1,3-dioxolan-4-yl (or cyclocarbonate), a dithiocyclocarbonate, an exo-vinylene cyclocarbonate and a 2-oxo-1,3-dioxolen-4-yl, the main chain of which comprises units (I) and (II) in which R0 is notably a methyl radical; and the number-average molecular mass Mn of which is between 400 and 100 000 g/mol. 2) Process for preparing said copolymer, comprising: (i) a step of heating a statistical bipolymer A chosen from a poly(butadiene-isoprene), a poly(butadiene-myrcene) and a poly(butadiene-farnesene); and then (ii) a step of heating the product formed, in the presence of a chain-transfer agent. 3) Use as adhesive, as a mixture with an amine compound comprising at least two amine groups.
Abstract:
1) Hydrocarbon-based copolymer comprising two end groups preceded by an ether function and chosen from a 2-oxo-1,3-dioxolan-4-yl (or cyclocarbonate), a dithiocyclocarbonate, and a 2-oxo-1,3-dioxolen-4-yl, the main chain of which comprises units (I) and (II) in which R0 is notably a methyl radical; and the number-average molecular mass Mn of which is between 400 and 100 000 g/mol. 2) Process for preparing said copolymer, comprising: (i) a step of heating a statistical bipolymer A chosen from a poly(butadiene-isoprene), a poly(butadiene-myrcene) and a poly(butadiene-farnesene); and then (ii) a step of heating the product formed, in the presence of a chain-transfer agent. 3) Use as adhesive, as a mixture with an amine compound comprising at least two amine groups.
Abstract:
1) Hydrocarbon-based polymer of formula (I): in which F1 and F2 have the respective formulae (IIa) and (IIb) or (II′a) and (II′b): a process for its preparation, and use as an adhesive.
Abstract:
Hydrocarbon-based polymer of formula (1) bearing alkoxysilane end groups: in which: is a double or single bond; each of R2, R3, R4 and R5 is H, a halo, an alkoxycarbonyl or an alkyl, m and p are each from 0 to 5, each of R and R′ is an alkyl, Z is an alkylene, optionally interrupted with COO, q is 0 or 1, r is 0, 1 or 2, and n is an integer such that the number-average molar mass Mn of the polymer is from 400 to 50 000 g/mol, and its polydispersity index (PDI) is from 1.0 to 2.0. Preparation by ring-opening metathesis polymerization for 2 hours to 24 hours. Adhesive composition comprising polymer (1) and crosslinking catalyst. Bonding by assembly of two substrates using this adhesive composition.
Abstract:
A polymer of formula (I): in which P is a divalent polymeric radical other than a polyoxypropylene radical; m is a number from 1 to 6; B is a monovalent, divalent, trivalent, tetravalent, pentavalent or hexavalent radical, having from 1 to 44 carbon atoms per molecule; the divalent polymeric radical P being such that the number-average molar mass Mn of the polymer of formula (I) is in a range from 400 to 8000 g/mol and such that the polydispersity (Pd) of the polymer of formula (I) is within a range from 1.0 to 4.0.Process for preparing the polymer of formula (I).Process for preparing polyurethanes, by reaction of a polymer of formula (I) with a compound, having an amine group, and also polyurethanes that may be thus obtained.