INDEX MATCHING AND TOUCH PANEL IMPROVEMENTS IN DISPLAY DEVICES
    1.
    发明申请
    INDEX MATCHING AND TOUCH PANEL IMPROVEMENTS IN DISPLAY DEVICES 审中-公开
    指示匹配和触控面板在显示设备中的改进

    公开(公告)号:US20150123911A1

    公开(公告)日:2015-05-07

    申请号:US14072952

    申请日:2013-11-06

    CPC classification number: G06F3/041 G06F2203/04103 Y10T29/49124

    Abstract: Provided are multilayered touch panel stacks and methods for forming thereof. The stacks include refractive index matching layers to minimize light losses. Specifically, the stacks may comprise a substrate, one, two, three, or four refractive index matching layers deposited on the substrate, and one or two transparent conductive layers such as indium tin oxide electrode layers. The stack may be attached to a light emitting element or be a part of an LCD or OLED displays. The refractive index matching interlayers may be based on a polymer solution having about 0.1%-30% by weight of specific rigid rod-like polymer molecules. The molecules may include various cores, spacers, and side groups to ensure their solubility, viscosity, and cross-linking ability. The refractive index matching interlayer may have a refractive index in between of about 1.60-1.80.

    Abstract translation: 提供多层触摸面板叠层及其形成方法。 堆叠包括折射率匹配层以最小化光损失。 具体地,堆叠可以包括沉积在衬底上的衬底,一个,两个,三个或四个折射率匹配层,以及一个或两个透明导电层,例如氧化铟锡电极层。 堆叠可以附接到发光元件或者是LCD或OLED显示器的一部分。 折射率匹配夹层可以基于具有约0.1%-30%重量的特定刚性棒状聚合物分子的聚合物溶液。 分子可以包括各种芯,间隔物和侧基,以确保其溶解性,粘度和交联能力。 折射率匹配中间层的折射率可以在约1.60-1.80之间。

    ORGANIC POLYMER COMPOUNDS SUITABLE FOR FORMING POSITIVE A-TYPE RETARDERS AND METHODS OF PRODUCTION THEREOF
    2.
    发明申请
    ORGANIC POLYMER COMPOUNDS SUITABLE FOR FORMING POSITIVE A-TYPE RETARDERS AND METHODS OF PRODUCTION THEREOF 审中-公开
    适用于形成A型阻滞剂的有机聚合物化合物及其生产方法

    公开(公告)号:US20150086799A1

    公开(公告)日:2015-03-26

    申请号:US14033415

    申请日:2013-09-20

    Abstract: An organic polymer solution may include about 0.1%-30% by weight of a specific polymer having rigid rod-like molecules. These molecules may include various cores, spacers, and sides groups to ensure their solubility, viscosity, and cross-linking ability. The rigid rod-like molecules are selected in such a way that they form self-assembling structures in the polymer solution, which makes it a lyotropic liquid crystal. The organic polymer solution, when properly deposited on a substrate and dried to remove solvents, forms a solid optical retardation layer of positive A-type substantially transparent to electromagnetic radiation in the visible spectral range.

    Abstract translation: 有机聚合物溶液可以包含约0.1%-30%重量的具有刚性棒状分子的特定聚合物。 这些分子可以包括各种芯,间隔物和侧基,以确保其溶解性,粘度和交联能力。 选择刚性棒状分子,使得它们在聚合物溶液中形成自组装结构,这使其成为溶致液晶。 当适当地沉积在基底上并干燥以除去溶剂时,有机聚合物溶液形成对可见光谱范围内的电磁辐射基本上透明的正A型的固体光学延迟层。

    LCD BACKLIGHT COMPONENT COATINGS FOR REDUCING LIGHT LOSSES AND IMPROVING IN-STACK LIGHT COLLIMATION
    3.
    发明申请
    LCD BACKLIGHT COMPONENT COATINGS FOR REDUCING LIGHT LOSSES AND IMPROVING IN-STACK LIGHT COLLIMATION 审中-公开
    LCD背光组件涂料,用于减轻光线损失并改善堆叠光线集合

    公开(公告)号:US20140133177A1

    公开(公告)日:2014-05-15

    申请号:US14159704

    申请日:2014-01-21

    CPC classification number: G02B6/005 G02B6/0065 Y10T29/49885

    Abstract: Provided are multilayer stacks for backlight units in LCD panels and methods for forming thereof. The stacks include refractive index matching layers and pressure sensitive adhesives to minimize light losses. More particularly, the stacks comprise a reflector, a light guide, a course diffuser, one or more brightness enhancing films, and a fine diffuser. A refractive index matching layer is deposited onto at least one surface of the backlight components. A pressure sensitive adhesive is deposited onto the refractive index matching layers. Alternatively, the stacks comprise two or more refractive index matching layers on each surface of the backlight components and retain an air gap between the backlight components. The refractive index matching interlayers are based on a polymer solution having about 0.1%-30% by weight of specific rigid rod-like polymer molecules. The molecules may include various cores, spacers, and sides groups to ensure their solubility, viscosity, and cross-linking ability.

    Abstract translation: 提供了用于LCD面板中背光单元的多层叠层及其形成方法。 堆叠包括折射率匹配层和压敏粘合剂以最小化光损失。 更具体地,堆叠包括反射器,光导,过程扩散器,一个或多个亮度增强膜和精细扩散器。 折射率匹配层沉积在背光组件的至少一个表面上。 压敏粘合剂沉积在折射率匹配层上。 或者,堆叠在背光组件的每个表面上包括两个或更多个折射率匹配层并且保持背光组件之间的气隙。 折射率匹配中间层基于具有约0.1重量%-30重量%的特定刚性棒状聚合物分子的聚合物溶液。 分子可以包括各种芯,间隔物和侧基,以确保其溶解性,粘度和交联能力。

    Depositing polymer solutions to form optical devices
    4.
    发明授权
    Depositing polymer solutions to form optical devices 有权
    沉积聚合物溶液以形成光学器件

    公开(公告)号:US09360596B2

    公开(公告)日:2016-06-07

    申请号:US13869041

    申请日:2013-04-24

    Abstract: Provided are methods of depositing polymer solutions on substrates to form various optical elements. A polymer solution may include about 0.1%-30% by weight of a specific polymer having rigid rod-like molecules. The molecules may include various cores, spacers, and sides groups to ensure their solubility, viscosity, and cross-linking ability. The deposition techniques may include slot die, spray, molding, roll coating, and so forth. Pre-deposition techniques may be used to improve wettability and adhesion of substrates. Post-deposition techniques may include ultraviolet cross-linking, specific drying techniques, evaporation of solvent, treating with salt solutions, and shaping. The disclosed polymers and deposition processes may yield optical elements with high refractive index values, such as greater than 1.6. These optical elements may be used as +A plates, −C plates, or biaxial polymers and used as retarders in LCD active panels or as light collimators and light guides.

    Abstract translation: 提供了在基底上沉积聚合物溶液以形成各种光学元件的方法。 聚合物溶液可以包含约0.1%-30%重量的具有刚性棒状分子的特定聚合物。 分子可以包括各种芯,间隔物和侧基,以确保其溶解性,粘度和交联能力。 沉积技术可以包括槽模,喷涂,模塑,辊涂等。 可以使用预沉积技术来改善基底的润湿性和粘附性。 后沉积技术可以包括紫外线交联,特定的干燥技术,溶剂蒸发,用盐溶液处理和成型。 所公开的聚合物和沉积方法可以产生具有高折射率值的光学元件,例如大于1.6。 这些光学元件可以用作+ A板,-C板或双轴聚合物,并用作LCD有源面板中的延迟器或者作为光准直器和光导。

    DEPOSITING POLYMER SOLUTIONS TO FORM OPTICAL DEVICES
    5.
    发明申请
    DEPOSITING POLYMER SOLUTIONS TO FORM OPTICAL DEVICES 有权
    沉积聚合物解决方案来形成光学器件

    公开(公告)号:US20140322452A1

    公开(公告)日:2014-10-30

    申请号:US13869041

    申请日:2013-04-24

    Abstract: Provided are methods of depositing polymer solutions on substrates to form various optical elements. A polymer solution may include about 0.1%-0% by weight of a specific polymer having rigid rod-like molecules. The molecules may include various cores, spacers, and sides groups to ensure their solubility, viscosity, and cross-linking ability. The deposition techniques may include slot die, spray, molding, roll coating, and so forth. Pre-deposition techniques may be used to improve wettability and adhesion of substrates. Post-deposition techniques may include ultraviolet cross-linking, specific drying techniques, evaporation of solvent, treating with salt solutions, and shaping. The disclosed polymers and deposition processes may yield optical elements with high refractive index values, such as greater than 1.6. These optical elements may be used as +A plates, −C plates, or biaxial polymers and used as retarders in LCD active panels or as light collimators and light guides.

    Abstract translation: 提供了在基底上沉积聚合物溶液以形成各种光学元件的方法。 聚合物溶液可以包含约0.1%-0%重量的具有刚性棒状分子的特定聚合物。 分子可以包括各种芯,间隔物和侧基,以确保其溶解性,粘度和交联能力。 沉积技术可以包括槽模,喷涂,模塑,辊涂等。 可以使用预沉积技术来改善基底的润湿性和粘附性。 后沉积技术可以包括紫外线交联,特定的干燥技术,溶剂蒸发,用盐溶液处理和成型。 所公开的聚合物和沉积方法可以产生具有高折射率值的光学元件,例如大于1.6。 这些光学元件可以用作+ A板,-C板或双轴聚合物,并用作LCD有源面板中的延迟器或者作为光准直器和光导。

Patent Agency Ranking