Abstract:
A polypeptide solution of the present invention is a polypeptide solution in which a polypeptide derived from natural spider silk proteins is dissolved in a solvent. The solvent contains at least one selected from the following (i)-(iii): (i) DMSO; (ii) DMSO with an inorganic salt; and (iii) DMF with an inorganic salt. Further, in the present invention, an artificial polypeptide fiber is obtained by: using the polypeptide solution as a dope solution; and extruding the dope solution from a spinneret into a desolvation bath so as to eliminate the solvent from the dope solution and form a fiber to produce an undrawn yarn. Moreover, in the present invention, a polypeptide is purified by subjecting the polypeptide solution to heat treatment and thereafter removing an undissolved substance therefrom. Thus, the present invention provides the polypeptide solution whose solute has high solubility and solvent itself is low cost, and that allows dissolution at high temperatures and has high safety: a method for producing an artificial polypeptide fiber: and a method for purifying a polypeptide.
Abstract:
A polypeptide solution of the present invention is a polypeptide solution in which a polypeptide derived from natural spider silk proteins is dissolved in a solvent. The solvent contains at least one selected from the following (i)-(iii): (i) DMSO; (ii) DMSO with an inorganic salt; and (iii) DMF with an inorganic salt. Further, in the present invention, an artificial polypeptide fiber is obtained by: using the polypeptide solution as a dope solution; and extruding the dope solution from a spinneret into a desolvation bath so as to eliminate the solvent from the dope solution and form a fiber to produce an undrawn yarn. Moreover, in the present invention, a polypeptide is purified by subjecting the polypeptide solution to heat treatment and thereafter removing an undissolved substance therefrom. Thus, the present invention provides the polypeptide solution whose solute has high solubility and solvent itself is low cost, and that allows dissolution at high temperatures and has high safety: a method for producing an artificial polypeptide fiber: and a method for purifying a polypeptide.
Abstract:
An information processing method performed by a processor, the method comprises garment selecting of receiving a selection of a garment from a user, price calculating of calculating a price of the garment on the basis of a type of the selected garment and parameters relating to a design and materials set for the garment, display controlling of causing a display part to display the calculated price, and parameter changing of changing the parameters in conjunction with an input from the user. The display controlling includes causing the display part to display the price that reflects the changed parameters in response to the change of the parameters.
Abstract:
A polypeptide solution of the present invention is a polypeptide solution in which a polypeptide derived from natural spider silk proteins is dissolved in a solvent. The solvent contains at least one selected from the following (i)-(iii): (i) DMSO; (ii) DMSO with an inorganic salt; and (iii) DMF with an inorganic salt. Further, in the present invention, an artificial polypeptide fiber is obtained by: using the polypeptide solution as a dope solution; and extruding the dope solution from a spinneret into a desolvation bath so as to eliminate the solvent from the dope solution and form a fiber to produce an undrawn yarn. Moreover, in the present invention, a polypeptide is purified by subjecting the polypeptide solution to heat treatment and thereafter removing an undissolved substance therefrom. Thus, the present invention provides the polypeptide solution whose solute has high solubility and solvent itself is low cost, and that allows dissolution at high temperatures and has high safety: a method for producing an artificial polypeptide fiber: and a method for purifying a polypeptide.
Abstract:
A polypeptide solution of the present invention is a polypeptide solution in which a polypeptide derived from natural spider silk proteins is dissolved in a solvent. The solvent contains at least one selected from the following (i)-(iii): (i) DMSO; (ii) DMSO with an inorganic salt; and (iii) DMF with an inorganic salt. Further, in the present invention, an artificial polypeptide fiber is obtained by: using the polypeptide solution as a dope solution; and extruding the dope solution from a spinneret into a desolvation bath so as to eliminate the solvent from the dope solution and form a fiber to produce an undrawn yarn. Moreover, in the present invention, a polypeptide is purified by subjecting the polypeptide solution to heat treatment and thereafter removing an undissolved substance therefrom. Thus, the present invention provides the polypeptide solution whose solute has high solubility and solvent itself is low cost, and that allows dissolution at high temperatures and has high safety: a method for producing an artificial polypeptide fiber: and a method for purifying a polypeptide.
Abstract:
The present invention relates to a method for recovering protein, which recovers a target protein from a mixture containing the target protein and a material different from the target protein, the method including a dissolution step of dissolving either the target protein or the material by applying pressure while heating to a solution for dissolution containing the mixture and a polar solvent, and a separation step of separating an obtained solution.
Abstract:
A polar solvent solution of the present invention is a polar solvent solution in which a solute containing a polyamine acid is dissolved in a polar solvent. An inorganic salt is added to the solution, and a mole ratio of moisture to the inorganic salt in the solution is 2.5×m×n or less, where m represents the number of cations forming the inorganic salt and n represents a charge number of the cation. A production method of the present invention is a method for producing the above solution, including: changing at, least one of a moisture content and a content of the inorganic salt in the solution to adjust a viscosity of the solution. Thus, the present invention provides a polar solvent solution whose viscosity can be easily adjusted to a desired value and thus enables stable spinning and casting when used as dopes for spinning, film, etc., and methods for producing the same.
Abstract:
An information processing method performed by a processor, the method comprises garment selecting of receiving a selection of a garment from a user, price calculating of calculating a price of the garment on the basis of a type of the selected garment and parameters relating to a design and materials set for the garment, display controlling of causing a display part to display the calculated price, and parameter changing of changing the parameters in conjunction with an input from the user. The display controlling includes causing the display part to display the price that reflects the changed parameters in response to the change of the parameters.
Abstract:
A solution-dyed protein fiber of the present invention includes 0-100 mass % of silk fibroin and 100-0 mass % of a polypeptide derived from spider silk proteins when the protein fiber is assumed to be 100 mass %, wherein the solution-dyed protein fiber contains a solution-dyeing colorant. The fiber is obtained by: dissolving or dispersing a solution-dyeing colorant in a solvent used for a spinning solution or in dimethyl sulfoxide, thereby preparing a coloring liquid; adding a solvent to the coloring liquid in an amount necessary for a spinning solution; adding and dissolving protein powder into the solvent, thereby preparing a spinning solution; and subjecting the spinning solution to wet spinning or dry-wet spinning. Thereby, the present invention provides a low-cost solution-dyed protein fiber in which a solution-dyeing colorant is dispersed uniformly and that can exhibit bright color tone, and a method for producing the same.
Abstract:
A polar solvent solution of the present invention is a polar solvent solution in which a solute containing a polyamine acid is dissolved in a polar solvent. The solution has a moisture content of less than 5 mass % based on 100 mass % of the solution. A method for producing a polar solvent solution of the present invention includes changing a moisture content of the solution to adjust the viscosity of the solution. Further, another method for producing a polar solvent solution includes reducing a moisture content of the solution to increase the viscosity of the solution. Thus, the present invention provides a polar solvent solution that enables stable spinning and casting without lowering its viscosity when used as dopes for spinning, film, etc., and methods for producing the same.