公开(公告)号:US09771626B2
公开(公告)日:2017-09-26
申请号:US14416378
申请日:2013-07-18
Applicant: TECHNOLOGICAL RESOURCES PTY. LIMITED
Inventor: Carolyn McCarthy , Rodney James Dry
IPC: C21B11/08 , C21B13/10 , C21B13/14 , C21C5/46 , C21C5/56 , F27B3/04 , F27B3/24 , F27B3/28 , C21B13/00 , F27B3/02 , F27B3/22 , C21C5/04 , C22B5/10 , C21C5/30 , C21C5/52 , F27D3/16 , F27D3/18
CPC classification number: C21B11/08 , C21B13/0006 , C21B13/0013 , C21B13/10 , C21B13/14 , C21B2100/66 , C21C5/04 , C21C5/305 , C21C5/4646 , C21C5/567 , C21C2005/5288 , C21C2100/02 , C21C2200/00 , C22B5/10 , F27B3/02 , F27B3/045 , F27B3/22 , F27B3/24 , F27B3/28 , F27D2003/168 , F27D2003/185 , Y02P10/136 , Y02P10/216 , Y02P10/265 , Y02P10/283
Abstract: A method of starting a molten bath-based process for smelting a metalliferous material is disclosed. The method includes using the heat flux of water-cooled elements in lower parts of a smelting vessel to provide an indication of molten bath temperature during at least an early part of the start-up method and adjusting injection rates of oxygen-containing gas and/or carbonaceous material into the smelting vessel to control the molten bath temperature during start-up without exceeding critical heat flux levels and tripping the start-up method.
-
公开(公告)号:US20150259758A1
公开(公告)日:2015-09-17
申请号:US14416378
申请日:2013-07-18
Applicant: TECHNOLOGICAL RESOURCES PTY. LIMITED
Inventor: Carolyn McCarthy , Rodney James Dry
CPC classification number: C21B11/08 , C21B13/0006 , C21B13/0013 , C21B13/10 , C21B13/14 , C21B2100/66 , C21C5/04 , C21C5/305 , C21C5/4646 , C21C5/567 , C21C2005/5288 , C21C2100/02 , C21C2200/00 , C22B5/10 , F27B3/02 , F27B3/045 , F27B3/22 , F27B3/24 , F27B3/28 , F27D2003/168 , F27D2003/185 , Y02P10/136 , Y02P10/216 , Y02P10/265 , Y02P10/283
Abstract: A method of starting a molten bath-based process for smelting a metalliferous material is disclosed. The method includes using the heat flux of water-cooled elements in lower parts of a smelting vessel to provide an indication of molten bath temperature during at least an early part of the start-up method and adjusting injection rates of oxygen-containing gas and/or carbonaceous material into the smelting vessel to control the molten bath temperature during start-up without exceeding critical heat flux levels and tripping the start-up method.
Abstract translation: 公开了一种开始熔融金属材料熔融浴工艺的方法。 该方法包括在熔化容器的下部使用水冷元件的热通量,以在启动方法的至少早期阶段提供熔融浴温度的指示,并且调节含氧气体和/ 或碳质材料进入熔炼炉,以控制启动期间的熔池温度,而不超过临界热通量水平并跳闸启动方法。
-