FLUOROPOLYETHER GROUP-CONTAINING POLYMER-MODIFIED ORGANIC SILICON COMPOUND, SURFACE TREATMENT AGENT, AND ARTICLE

    公开(公告)号:US20210171799A1

    公开(公告)日:2021-06-10

    申请号:US16616320

    申请日:2018-04-19

    Abstract: This surface treatment agent using a compound represented by formula (1) or (2) can, even without having a hydrolyzable group, form a water repellent and oil repellent layer having excellent abrasion resistance under mild conditions such as at room temperature. [Rf represents a monovalent or divalent fluorooxyalkylene group-containing polymer residue, Y1 and Y2 each represent a single bond or a divalent hydrocarbon group, Q represents a group that has a Si-containing structure having a valence of 2-4, Si, or C, X represents an epoxy-containing group, k represents 0-2, m represents 1-5, n represents 1-3, Z represents H, —SiR3 (R represents an alkyl group or a phenyl group), or -W1-Q′-W2-X′ (X′ represents X or —SiR3, W1 and W2 each represent a single bond or a divalent hydrocarbon group, Q′ represents a divalent group having a Si-containing structure), and a represents 1 or 2].

    Powder coating material, method for producing substrate provided with coating film and coated article

    公开(公告)号:US10723825B2

    公开(公告)日:2020-07-28

    申请号:US16040040

    申请日:2018-07-19

    Applicant: AGC Inc.

    Abstract: A powder coating material capable of forming a coating film that is excellent in weather resistance, processability and impact resistance and that improves corrosion resistance of a substrate (in particular, a substrate made of aluminum or of an aluminum alloy), wherein the powder coating material contains a powder of a resin composition, wherein the resin composition contains a fluorinated polymer (A) having a number average molecular weight of from 10,000 to 50,000 and a fluorine content of at least 10 mass %, a resin (B) having a fluorine content of less than 10 mass % or containing no fluorine atom, a curing agent, a plasticizer having a melting point of from 50 to 150° C. and core-shell particles, and wherein the absolute value of the difference between the melting point of the plasticizer and the glass transition temperature of a polymer of a shell portion in the core-shell particles is within 30° C. and the content of the plasticizer is from 5 to 25 parts by mass based on 100 parts by mass of the fluorinated polymer (A).

    Fluorinated resin composition and laminate

    公开(公告)号:US10400079B2

    公开(公告)日:2019-09-03

    申请号:US15277403

    申请日:2016-09-27

    Applicant: AGC Inc.

    Inventor: Hiroshi Aruga

    Abstract: To provide a fluorinated resin composition which is capable of forming a resin film excellent in moist heat resistance and solar reflectance. The fluorinated resin composition comprises composite particles, a fluorinated polymer and a liquid medium, wherein the composite particles are a composite having a part or whole of the surface of aluminum particles coated with at least one member selected from the group consisting of an acrylic resin and silica; the total coating amount of the acrylic resin and silica is from 6 to 25 parts by mass per 100 parts by mass of the aluminum particles; and the water surface diffusion area is from 14,000 to 27,000 cm2/g.

    METHOD OF MAKING A FUSER MEMBER
    9.
    发明申请
    METHOD OF MAKING A FUSER MEMBER 审中-公开
    制造熔炉成员的方法

    公开(公告)号:US20160312068A1

    公开(公告)日:2016-10-27

    申请号:US14693625

    申请日:2015-04-22

    Abstract: Described herein is a method of manufacturing a fuser member. The method includes mixing a high load fluoropolymer/carbon nanotube composition in a high shear mixer. The method includes mixing the high load fluoropolymer/carbon nanotube composition in the high shear mixer for 3 or more times. A fluoropolymer is added to the high load fluoropolymer/carbon nanotube composition to form a low load fluoropolymer/carbon nanotube composition. The low load fluoropolymer/carbon nanotube composition is mixed in a rubber compounding mixer for 3 or more times. The low load fluoropolymer/carbon nanotube composition is coated on a fuser substrate, cured and polished.

    Abstract translation: 这里描述的是制造定影器构件的方法。 该方法包括在高剪切混合器中混合高负荷含氟聚合物/碳纳米管组合物。 该方法包括将高负荷含氟聚合物/碳纳米管组合物在高剪切混合器中混合3次或更多次。 向高负荷含氟聚合物/碳纳米管组合物中加入含氟聚合物以形成低负荷含氟聚合物/碳纳米管组合物。 将低负荷含氟聚合物/碳纳米管组合物在橡胶配混混合机中混合3次以上。 将低负荷含氟聚合物/碳纳米管组合物涂布在定影基板上,进行固化和抛光。