Invention Grant
US08623453B2 Method for restoring antimicrobial hydrophilic coatings 有权
恢复抗微生物亲水涂层的方法

Method for restoring antimicrobial hydrophilic coatings
Abstract:
A method for restoring a silver oxide-containing hydrophilic coating includes heating the coating to a temperature between about 260° C. and about 540° C. and maintaining the coating at a temperature between about 260° C. and about 540° C. in an environment containing oxygen and ozone for less than 24 hours.