CZTSS 나노입자 전구체 및 제조방법과 상기 전구체를 이용한 고품질 CZTSS 나노입자 및 제조방법
    1.
    发明公开
    CZTSS 나노입자 전구체 및 제조방법과 상기 전구체를 이용한 고품질 CZTSS 나노입자 및 제조방법 有权
    CU2ZNSN(S,SE)4纳米颗粒(CZTSS NANO-PARTICLE)前体,用于生产前体的方法,使用前体的CZTSS纳米颗粒和生产CZTSS纳米颗粒的方法

    公开(公告)号:KR1020120017719A

    公开(公告)日:2012-02-29

    申请号:KR1020100080491

    申请日:2010-08-19

    Abstract: PURPOSE: A copper-zinc-tin-sulfur-selenium(CZTSS)-based nano-particle precursor, a method for manufacturing the same, the CZTSS-based nano-particles using the same, and a method for manufacturing the nano-particles are provided to synthesize the CZTSS-based nano-particle precursor by hardly using toxic materials. CONSTITUTION: A CZTSS-based nano-particle precursor is synthesized by irradiating microwave to a reacting solution containing copper, zinc, tin, and sulfur. The composition ratio of the copper, the zinc, the tin, the sulfur is adjusted according to the pH value of the reacting solution. The microwave irradiation is implemented for 5 minutes to 1 hours under 100-700W. A method for manufacturing the CZTSS-based nano-particle precursor includes the following: the reacting solution is prepared; the pH value of the reacting solution is adjusted; the microwave is irradiated to the reacting solution. The CZTSS nano-particle precursor is separated.

    Abstract translation: 目的:一种基于铜 - 锌 - 锡 - 硫 - 硒(CZTSS)的纳米颗粒前体及其制备方法,使用该纳米颗粒的CZTSS基纳米颗粒及其制备方法 提供用于通过几乎不使用有毒材料合成基于CZTSS的纳米颗粒前体。 构成:通过将微波照射到含有铜,锌,锡和硫的反应溶液中来合成基于CZTSS的纳米颗粒前体。 根据反应溶液的pH值调节铜,锌,锡,硫的组成比。 微波照射在100-700W下实施5分钟至1小时。 制造基于CZTSS的纳米颗粒前体的方法包括:制备反应溶液; 调整反应溶液的pH值; 将微波照射到反应溶液。 分离CZTSS纳米颗粒前体。

Patent Agency Ranking