초극세 탄소섬유 및 그 제조방법
    2.
    发明授权
    초극세 탄소섬유 및 그 제조방법 有权
    超细碳纤维及其制造方法

    公开(公告)号:KR101726822B1

    公开(公告)日:2017-04-13

    申请号:KR1020150073060

    申请日:2015-05-26

    Abstract: 본발명은도성분이탄소섬유형성능수지의초극세연속섬유집합체로이루어진해도형복합섬유를전자선을이용하여가교시켜초극세탄소섬유전구체로사용함으로써고성능의초극세탄소섬유의생산비용을낮출수 있는제조방법및 그방법에의하여제조된초극세탄소섬유에관한것으로, 보다상세하게는도성분이탄소섬유형성능수지의초극세연속섬유집합체로이루어진해도형복합섬유제조단계; 상기해도형복합섬유로부터해성분을제거하는해성분제거단계; 해성분이제거된탄소섬유형성능수지의초극세연속섬유집합체의내열성향상을위한가교화가이루어질수 있도록전자선을조사하는초극세탄소섬유전구체제조단계; 상기초극세탄소섬유전구체를산화·안정화시키는산화·안정화단계; 및산화·안정화된초극세탄소섬유전구체를탄화시키는탄화단계;를포함하는초극세탄소섬유의제조방법및 이제조방법에따라제조되는초극세탄소섬유에대한것이다.

    Abstract translation: 本发明的生产过程中,也将组分通过使用电子束通过由通过使用超细碳纤维前体形成能力的树脂中的碳纤维的超细长纤维集合体的成形复合纤维交联,从而降低生产高性能的超细碳纤维的成本,并 本发明涉及通过该方法制造的超细碳纤维,并且更具体地涉及包含碳纤维形成树脂的超细连续纤维聚集体的超细复合纤维的生产方法; 从溶解性复合纤维中除去溶液成分的溶液除去工序; 制备用于照射电子束的超细碳纤维前体以便交联以改善去除海成分的碳纤维形成树脂的超细连续纤维聚集体的耐热性的步骤; 氧化和稳定超细碳纤维前体; 本发明还涉及一种根据本发明生产的微细碳纤维。本发明还涉及一种根据本发明生产的微细碳纤维。

    고투과유량 및 고여과효율을 갖는 초극세 섬유상 필터 및 그 제조방법
    3.
    发明授权
    고투과유량 및 고여과효율을 갖는 초극세 섬유상 필터 및 그 제조방법 有权
    具有超滤和超滤功能的超滤纤维过滤器及其制备方法

    公开(公告)号:KR101691636B1

    公开(公告)日:2017-01-02

    申请号:KR1020150063335

    申请日:2015-05-06

    Abstract: 초극세섬유상필터는 2.5 psi 압력에서물투과유량이 7,500 L/hr.m이상의고투과유량을가지며 200 nm 입자의여과효율이 98 % 이상이거나, 또는 2.5 psi 압력에서물투과유량이 1,000 L/hr.m이상의고투과유량을가지며 100 nm 입자의여과효율이 98 % 이상이다. 이러한초극세섬유상필터는, 기존박테리아를여과하는멤브레인필터에비하여월등히우수한물투과유량과입자제거능력을가지며, 더나아가뛰어난물투과유량을가지면서바이러스등 극미립자도흡착제거할수 있다.

    고투과유량 및 고여과효율을 갖는 초극세 섬유상 필터 및 그 제조방법
    4.
    发明公开
    고투과유량 및 고여과효율을 갖는 초극세 섬유상 필터 및 그 제조방법 有权
    具有超滤和超滤功能的超滤纤维过滤器及其制备方法

    公开(公告)号:KR1020160131301A

    公开(公告)日:2016-11-16

    申请号:KR1020150063335

    申请日:2015-05-06

    Abstract: 초극세섬유상필터는 2.5 psi 압력에서물투과유량이 7,500 L/hr.m이상의고투과유량을가지며 200 nm 입자의여과효율이 98 % 이상이거나, 또는 2.5 psi 압력에서물투과유량이 1,000 L/hr.m이상의고투과유량을가지며 100 nm 입자의여과효율이 98 % 이상이다. 이러한초극세섬유상필터는, 기존박테리아를여과하는멤브레인필터에비하여월등히우수한물투과유량과입자제거능력을가지며, 더나아가뛰어난물투과유량을가지면서바이러스등 극미립자도흡착제거할수 있다.

    마찰계수의 상대습도 의존성이 감소된 나노 스케일 파상형다이아몬드상 카본(DLC) 박막
    5.
    发明公开
    마찰계수의 상대습도 의존성이 감소된 나노 스케일 파상형다이아몬드상 카본(DLC) 박막 无效
    具有纳米结构表面的类金刚石碳膜,减少滑动摩擦的湿度依赖性

    公开(公告)号:KR1020090060846A

    公开(公告)日:2009-06-15

    申请号:KR1020070127795

    申请日:2007-12-10

    Abstract: A diamond-like carbon film with a nano-undulated surface is provided to reduce the humidity dependence of friction coefficient due to the characteristics of the nano-undulated surface suppressing tribo-chemical reaction in the transition layer. A diamond-like carbon film has a nano-undulated surface which is formed on a nano dot pattern of a substrate, with RMS surface roughness of 5nm to 50nm. The nano dot pattern is made of metal selected in the group consisting of nickel, cobalt, chrome, iron, zinc, copper, gold, silver, molybdenum, palladium and platinum, and its diameter is 20nm to 800nm. The diamond-like carbon film with the nano-undulated surface is formed by RF-PACVD(Radio Frequency-Plasma Assisted Chemical Vapor Deposition) using methane gas as reaction gas.

    Abstract translation: 提供具有纳米波纹表面的类金刚石碳膜,以降低由于纳米波纹表面的特性而导致的摩擦系数的湿度依赖性,从而抑制过渡层中的摩擦化学反应。 类金刚石碳膜具有形成在基板的纳米点图案上的纳米波状表面,RMS表面粗糙度为5nm至50nm。 纳米点图案由选自镍,钴,铬,铁,锌,铜,金,银,钼,钯和铂的金属制成,直径为20nm至800nm。 具有纳米波状表面的类金刚石碳膜通过使用甲烷气体作为反应气体的RF-PACVD(射频等离子体辅助化学气相沉积)形成。

    초극세 탄소섬유 및 그 제조방법
    7.
    发明公开
    초극세 탄소섬유 및 그 제조방법 有权
    超滤碳纤维及其制备方法

    公开(公告)号:KR1020160138776A

    公开(公告)日:2016-12-06

    申请号:KR1020150073060

    申请日:2015-05-26

    Abstract: 본발명은도성분이탄소섬유형성능수지의초극세연속섬유집합체로이루어진해도형복합섬유를전자선을이용하여가교시켜초극세탄소섬유전구체로사용함으로써고성능의초극세탄소섬유의생산비용을낮출수 있는제조방법및 그방법에의하여제조된초극세탄소섬유에관한것으로, 보다상세하게는도성분이탄소섬유형성능수지의초극세연속섬유집합체로이루어진해도형복합섬유제조단계; 상기해도형복합섬유로부터해성분을제거하는해성분제거단계; 해성분이제거된탄소섬유형성능수지의초극세연속섬유집합체의내열성향상을위한가교화가이루어질수 있도록전자선을조사하는초극세탄소섬유전구체제조단계; 상기초극세탄소섬유전구체를산화·안정화시키는산화·안정화단계; 및산화·안정화된초극세탄소섬유전구체를탄화시키는탄화단계;를포함하는초극세탄소섬유의제조방법및 이제조방법에따라제조되는초극세탄소섬유에대한것이다.

    탄소복합섬유 및 이의 제조 방법
    10.
    发明公开
    탄소복합섬유 및 이의 제조 방법 有权
    碳复合纤维及其制造方法

    公开(公告)号:KR1020160150456A

    公开(公告)日:2016-12-30

    申请号:KR1020150088474

    申请日:2015-06-22

    Abstract: 탄소섬유전구체및 금속산화물전구체를포함하는혼합용액을제조하는단계; 혼합용액을방사공정을통해방사하여탄소복합섬유의제1전구체를제조하는단계; 탄소복합섬유의제1전구체를안정화하는단계; 안정화된탄소복합섬유의제1전구체를탄화하여탄소복합섬유의제2전구체를제조하는단계; 및탄소복합섬유의제2전구체를활성화하여탄소복합섬유를형성하는단계를포함하는탄소복합섬유의제조방법이제공된다. 이에따라, 광촉매특성등 우수한특성을갖는탄수복합섬유가제공될수 있다.