公开(公告)号:US20190338065A1
公开(公告)日:2019-11-07
申请号:US16093491
申请日:2017-03-17
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: PAOLA MASSARI , MARCO CIARAFONI , NICOLETTA MARTINI , DAVIDE TARTARI , ROBERTO PANTALEONI
IPC: C08F297/08
Abstract: The present disclosure provides a propylene composition made from or containing A) from 60 wt % to 75 wt %, of a propylene homopolymer having a Polydispersity Index (P.I.) value from 4.3 to 4.9, a fraction insoluble in xylene at 25° C., higher than 95%, based upon the weight of the propylene homopolymer, and MFR (Melt Flow Rate according to ISO 1133, condition L, at 230° C. and 2.16 kg load) ranging from 20 to 75 g/10 min; B) from 25 wt % to 40 wt %, of a copolymer of propylene with from 46.0 wt % to 49.0 wt %; of ethylene derived units, based upon the weight of the propylene copolymer; wherein the propylene polymer composition having an intrinsic viscosity of the fraction soluble in xylene at 25° C. between 2.2 to 2.9 dl/g; and the relation: 10.7+1.3×MFRa−17.7×P.I.−29.3×IV+4.9×Xs (I) between about 40 to about 66; wherein MFRa is the melt flow rate of the component A); P.I. is the polydispersity index of component A); IV is the intrinsic viscosity of the fraction soluble in xylene at 25° C.; and Xs is the fraction soluble in xylene at 25° C.; and wherein the amount of A+B is equal to 100 wt %.
-
公开(公告)号:US20180066086A1
公开(公告)日:2018-03-08
申请号:US15559374
申请日:2016-03-14
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: ROBERTA MARZOLLA , PAOLA MASSARI , NICOLETTA MARTINI , MARCO CIARAFONI , TIZIANA CAPUTO
IPC: C08F210/06 , C08J5/18
CPC classification number: C08F210/06 , C08J5/18 , C08J2323/14 , C08F210/08 , C08F210/16 , C08F2500/12 , C08F2500/26 , C08F4/651 , C08F4/6545 , C08F4/6465 , C08F2/001
Abstract: A propylene, ethylene, 1-butene terpolymer made from or containing a) from about 1.8 wt % to about 5.9 wt % of ethylene derived units; and b) from about 2.0 wt % to about 4.5 wt % of 1 butene derived units; and having i) a ratio of C2 wt %/C4 wt % in the range from about 0.9 to about 1.3; wherein C2 wt % is the weight percent of ethylene derived units and C4 wt % is the weight percent of 1-butene derived units; ii) a Melt flow rate (determined according to ISO 1133 230° C., 2.16 kg) in the range from about 1.0 to about 30.0 g/10 min; and iii) a xylene soluble fraction at 25° C. between about 10 wt % and about 30 wt %. The weight percentages are based upon the total weight of the terpolymer.
-